Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 200 g/10 min @Load 2.16 kg, Temperature 190 °C |
200 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Riblene® MY 00 Low Density Polyethylene - Injection Molding Riblene MY 00 is a very high flowability low density polyethylene resin (LDPE).Main Applications: Riblene MY 00 is suitable for hot melts.Information provided by Polimeri Europa. |
|||
Melt Flow | 200 g/10 min @Load 2.16 kg, Temperature 190 °C |
200 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Eastman 812A Polyethylene
(discontinued **) Polyethylene 812A is a natural low density material with a 200 melt index. This high-flow formulation is used for specialty injection molding applications in the medical market.Unless otherwise not.. |
|||
Melt Flow | 200 g/10 min @Load 2.16 kg, Temperature 190 °C |
200 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Eastman 812P Polyethylene
(discontinued **) Polyethylene 812A is a natural low density material with a 200 melt index. Its high melt index exhibits excellent wettability. This makes it ideal as a carpet backing to bind fibers to the carpet... |
|||
Melt Flow | 200 g/10 min | 200 g/10 min | ISO 1133-1981E |
LyondellBasell Montell 0800 Polybutene Key Features: highly isotactic, semi-crystalline homopolymer, good creep resistance, good environmental crack resistance, miscible with polypropylenes, FDA acceptableApplications: concrete carrierMe.. |
|||
Melt Flow | 200 g/10 min @Load 2.16 kg, Temperature 190 °C |
200 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polyram Bondyram® 1010 Maleic Anhydride Modified Polypropylene Information provided by Polyram. |
|||
Melt Flow | 200 g/10 min @Load 2.16 kg, Temperature 190 °C |
200 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Westlake EC812AA Low Density Polyethylene WESTLAKE low-density polyethylene EC812 is a natural low-density material with a 200 melt index. Its high melt index exhibits excellent wettability. This makes it ideal as a backing to carpet to bin.. |
|||
Melt Flow | 200 g/10 min @Load 2.16 kg, Temperature 190 °C |
200 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Westlake EM812AA Low Density Polyethylene WESTLAKE low-density polyethylene EM812 is a low-density formulation used for injection molding. It is an outstanding material for molding lids and other container closures because it processes easi.. |