Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
SABIC 318CN Linear Low Density Polyethylene for Wire & Cable Product Description: 318CN is a Linear Low Density Polyethylene natural resin for wire and cable applications. It contains a low level of antioxidants and does not contain any slip or antiblock a.. |
|||
Melt Flow | 2.8 g/10 min @Load 1.20 kg, Temperature 300 °C |
2.8 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® ML4249 PC Polycarbonate for aircraft applications requiring FAR 25.853a compliance. Transparent, transluscent and opaque colors. For blow molding. |
|||
Melt Flow | 2.8 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.8 g/10 min @Load 8.38 lb, Temperature 446 °F |
|
Arkema Group Oroglas® HFI-10 Acrylic, Impact Grade
(discontinued **) OROGLAS HFI-10 is an impact grade that in addition to its superior impact resistance provides an improvement in flow which contribute to improve molding behavior and reduce cycle time.Key features :.. |
|||
Melt Flow | 2.8 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.8 g/10 min @Load 8.38 lb, Temperature 446 °F |
|
Arkema Group Oroglas® MI-2T Acrylic
(discontinued **) OROGLAS MI-2T is an injection molding acrylic grade that offers excellent thermal resistance with slight improvement in impact performance.Key features improved deformation and toughness : up to 2.. |
|||
Melt Flow | 2.8 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.8 g/10 min @Load 8.38 lb, Temperature 446 °F |
|
Arkema Group Oroglas® MI-4T Acrylic, Heat Resistant
(discontinued **) OROGLAS MI-4T is an acrylic grade that associates improved impact resistance with high heat resistance.Key features improved impact resistance: up to 4 times more impact resistant than standard acr.. |
|||
Melt Flow | 2.8 - 4.6 g/10 min @Load 21.6 kg, Temperature 230 °C |
2.8 - 4.6 g/10 min @Load 47.6 lb, Temperature 446 °F |
ASTM D1238 |
Solvay Specialty Polymers Solef® 1015 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 1015 PVDF homopolymer has very high viscosity, suitable for membrane manufacturing. It is available exclusively as powder.Information provided by Solvay Specialty Polymers. |
|||
Melt Flow | 2.8 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.8 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Ineos H03G-03 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: ExtrusionFeatures: Ease of processingTypical applications: Oriented filmComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from inject.. |
|||
Melt Flow | 2.8 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.8 g/10 min @Load 11.0 lb, Temperature 392 °F |
Condition G; ASTM D1238 |
Global 121-PC-Blue Acrylonitrile Styrene, General Purpose Grade Description-transparent, blue, medium impact resistance, high hardness, good stiffness, high heat resistance, good chemical resistanceApplications-automotive, electrical parts, household goodsInform.. |
|||
Melt Flow | 2.8 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.8 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Ineos Styrenics Polystyrene 486N (NAFTA) High-impact grade of polystyrene with excellent ESCR.Information provided by BASF.Ineos Styrenics purchased this product line from BASF in 2005. |
|||
Melt Flow | 2.8 - 3.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.8 - 3.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem PH 0320 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Melt Flow | 2.8 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.8 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
IRPC Polimaxx Polene 120PC Styrene Acrylonitrile APPLICATIONS: INJECTION MOLDING, HOUSEHOLD PRODUCTS : SANITARY WARE, AUTOPART APPLICATION : LAMP ELECTRICAL APPLIANCES : ELECTRICAL FAN |
|||
Melt Flow | 2.8 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.8 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
IRPC Polimaxx Polene 320PC Styrene Acrylonitrile APPLICATIONS: INJECTION MOLDING, HOUSEHOLD PRODUCTS : SANITARY WARE, AUTOPART APPLICATION : LAMP ELECTRICAL APPLIANCES : ELECTRICAL FAN |
|||
Melt Flow | 2.8 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.8 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
LG Chemical 25SPE GPPS Heat resistance, Chemical resistance, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Superior extrusion pr.. |
|||
Melt Flow | 2.8 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.8 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Bormod™ HC905TF Polypropylene Homopolymer for Thermoforming Bormod HC905TF is a low melt flow rate polypropylene homopolymer intended for thermoformed packaging applications. This homopolymer is produced using the Borealis Controlled Crystallinity Polypropy.. |
|||
Melt Flow | 2.8 g/10 min | 2.8 g/10 min | |
UBE B (Low-Cis) HIPS (n-DM = 0.03 wt % and PH-3H = 0.03 wt %) Description: UBE high impact polystyrene (HIPS).Information provided by UBE. |
|||
Melt Flow | 2.8 g/10 min | 2.8 g/10 min | |
UBE C (Low-Cis) HIPS (n-DM = 0.03 wt % and PH-3H = 0.03 wt %) Description: UBE high impact polystyrene (HIPS).Information provided by UBE. |
|||
Melt Flow | 2.8 g/10 min | 2.8 g/10 min | |
UBE UBEPOL B -B HIPS (Low-cis) Description: UBE high impact polystyrene (HIPS).Information provided by UBE. |
|||
Melt Flow | 2.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Borealis SuperCOPO™ LH4201R Polyethylene Insulation Compound, Crosslinkable SuperCOPO™ LH4201R is a crosslinkable natural polyethylene compound, specially designed for insulation applications. Applications: SuperCOPO™ LH4201R is intended for insulation of XLPE power cabl.. |
|||
Melt Flow | 2.8 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.8 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
TPI Porene® AS 121 PC (Blue) General Purpose SAN Porene® is a registered trademark of Thai Petrochemical Industry Co. LTD. Information provided by Dayson Polymers. |
|||
Melt Flow | 2.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
condition E; ASTM D1238 |
DuPont™ Surlyn® 8940 Ionomer Resin, Sodium Surlyn® 8940 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Melt Flow | 2.8 g/10 min | 2.8 g/10 min | ASTM D1238 |
Aclo Accucomp ABS ABS810L Medium Impact Grade |
|||
Melt Flow | 2.8 g/10 min | 2.8 g/10 min | ISO 1133 D |
Asahi Kasei Tenac®-C 3510 Copolymer Acetal Resin High-impact, high elongation grade, with increased molecular weightInformation provided by Asahi Kasei Corporation. |
|||
Melt Flow | 2.8 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.8 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Americas Styrenics STYRON® 487R High Impact Polystyrene Product CharacteristicsToughnessHeat resistanceGood stiffnessFood Contact CompliantUL Classification 94HBTypical ApplicationsLidsAppliancesPackaging/disposablesHousewaresInformation provided by Amer.. |
|||
Melt Flow | 2.8 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.8 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Total PSI 975E Polystyrene Polystyrene 975E is a high impact polystyrene designed for extrusion/thermoforming applications. The food ESCR properties of 975E dictate its use for dairy applications that are subjected to high bu.. |
|||
Melt Flow | 2.8 g/10 min @Load 5.00 kg, Temperature 230 °C |
2.8 g/10 min @Load 11.0 lb, Temperature 446 °F |
|
Arkema Group Kynar® FLEX 2822 PVDF
(discontinued **) Designation ISO 12086-VDF/HFP-K, EDN, N. ?E5.C.H.B.C,, ? (4-8)Kynar FLEX PVDF are fluorinated thermoplastic copolymers.Outstanding characteristics of Kynar FLEX: chemical resistance, imperviousness .. |
|||
Melt Flow | 2.8 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.8 g/10 min @Load 8.38 lb, Temperature 446 °F |
|
Arkema Group Oroglas® V 825 T Acrylic
(discontinued **) OROGLAS V 825 T exhibits an excellent balance of properties including superior thermal resistance with an easy processing behavior.OROGLAS V 825 T is then the material of choice for automotive appli.. |
|||
Melt Flow | 2.8 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.8 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Bormod™ HC904CF Polypropylene Bormod™ BJ368MO is a polypropylene copolymer characterized by good flow, and optimum combination of high stiffness and high impact strength. The material is nucleated with Borstar® Nucleation Tech.. |
|||
Melt Flow | 2.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Bynel® 2174 Anhydride-Modified Ethylene Acrylate Adhesive Resin
(discontinued **) Bynel® Series 2100 resins are anhydride-modified ethylene acrylate resins. They contain a temperature stable ester that makes them functional in high temperature coextrusions. They are available in.. |