Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.3 g/10 min | 2.3 g/10 min | Condition 230/2-8; ASTM D1238 |
Plaskolite Optix® CA-81 General Purpose Acrylic Resin Extrusion Grade Pellets. Highest Molecular weight. |
|||
Melt Flow | 2.3 g/10 min @Temperature 190 °C |
2.3 g/10 min @Temperature 374 °F |
|
North Wood Plastics HDPE with 40% Wood Fiber Data provided by North Wood Plastics, Inc. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® LA-0219-AM LDPE Foam Resin Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinFilm properties are typical of blo.. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® FG220-A Octene LLDPE Film Resin Features: Exceptional toughnessLow gel level Applications: Cast stretch wrapNettingCo-extrusion and laminationInformation provided by Nova Chemicals |
|||
Melt Flow | 2.3 g/10 min | 2.3 g/10 min | ExxonMobil Method |
ExxonMobil LD 503.LN Foams and Compounding Resin
(discontinued **) LD 503.LN is a low density homopolymer specially designed for maximum performance in foam applications.Information provided by ExxonMobil Chemical |
|||
Melt Flow | 2.3 g/10 min | 2.3 g/10 min | Exxon Method |
ExxonMobil Escorene® LD-411 LDPE Power Cable Insulation
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A crosslinkable polyethylene homopolymer designed as an electrical grade base resin especially suitable for Henschel blending.Applications: A base r.. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
M. Holland Company LD219AA LDPE
(discontinued **) Features: Good Processability, Ultra High ToughnessUses: Bottles, PackagingProcessing Method: Blow MoldingInformation provided by M. Holland. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Bynel® 3080 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Bynel® 3095 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Phillips 66 COPYLENE® CH023NX Polypropylene, Homopolymer, Thermoforming COPYLENE™ CH023NX has a high performance nucleation system designed to yield high clarity thermoformed articlesApplications: ThermoformingInformation provided by Phillips 66. |
|||
Melt Flow | 2.3 - 3.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 - 3.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
±10% |
Kazanorgsintez PE2NT76-17 High Density Polyethylene for Blow Molding Production Method: Gaseous-phase method. Application: Compositions are intended for goods produced by injection molding method.Information Provided by Kazanorgsintez |
|||
Melt Flow | 2.3 g/10 min | 2.3 g/10 min | ASTM D1238 |
Kolon DIAMAT® GP Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 250 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
LG Chemical LUPOS GP2300 ABS+GF30%, General Purpose Feature: Injection Molding, ABS+GF30%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-54-7, 9003-56-9 and 65997-17-3Information provided by LG Chemical |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) LL0220KJ Linear Low Density Polyethylene LL0220KJ are linear low density polyethylene copolymers containing butane-1 as the comonomer.Applications: shipping sacks, carrier and garbage bags, consumer packaging, high clarity film, agricultu.. |
|||
Melt Flow | 2.3 g/10 min @Load 10.0 kg, Temperature 220 °C |
2.3 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Techmer ES Plastiblend® ABS 8002 Availability: North AmericaForms: PelletsFeatures: High Heat ResistanceProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Total LDPE 1022 FH 24 Low Density Polyethylene - Blown Film LDPE 1022 FH 24 is a low density polyethylene made by a high pressure process.LDPE 1022 FH 24 is a slip and anti-block formulated grade.LDPE 1022 FH 24 is suited to many applications in the field of.. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow 621I Low Density Polyethylene (LDPE) Specialty resin designed for high melt strength applications Provides excellent bubble stability Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow |
|||
Melt Flow | 2.3 g/10 min | 2.3 g/10 min | ASTM D1238 |
Dow DOWLEX™ 2047G Linear Low Density Polyethylene For high performance stretch film applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow |
|||
Melt Flow | 2.3 g/10 min | 2.3 g/10 min | ASTM D1238 |
Dow DOWLEX™ 2247G Polyethylene Resin Next Generation DOWLEX™ 2247G Polyethylene Resin with Extra Stretch Performance (ESP) is an ethylene-octene-1 copolymer designated for cast stretch film applications, such as industrial pallet wrap.. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escorene™ 768.MJ Blown Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra UL 768.MJ is a low gel 26.2% vinyl acetate copolymer designed for film and compounding applications. This resin provides very low modulus films with high tensile .. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 235 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® AESN P20 TL Nylon 12, Flexible Grade (Conditioned) Designation ISO 1874-PA12-P,EHL,22-005Flexible grade for overmolding. Available colors: natural and white. Light and heat stabilized. No lubricant.Flexibility. Very good ability to overmold Pebax an.. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 235 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® AESN P20 TL Nylon 12, Flexible Grade (Dry) Designation ISO 1874-PA12-P,EHL,22-005Flexible grade for overmolding. Available colors: natural and white. Light and heat stabilized. No lubricant.Flexibility. Very good ability to overmold Pebax an.. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Braskem Green PE SLH218 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene Description: SLH218 is a LLDPE Hexene copolymer produced by Braskem. It shows a good balance between optical properties, mechanical properties (Mainly stretchability), sealability and processability.. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Braskem Green PE SLL218 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene Description: SLL218 is a Linear Low Density Polyethylene, copolymer of butene-1. Developed for cast film extrusion. Films obtained with this product show a good processing performance balanced with .. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
M. Holland Company LD220MM LDPE
(discontinued **) Additives: Medium Antiblock, SlipFeatures: Medium Antiblocking, Good Heat Seal, Medium SlipUses: Liners, PackagingProcessing Method: Blown FilmInformation provided by M. Holland. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Total LDPE 1022 FN 24 Low Density Polyethylene - Blown Film LDPE 1022 FN 24 is a low density polyethylene made by a high pressure process without antioxidant.LDPE 1022 FN 24 is suited to many applications in the field of consumer, industrial, food or hygiene.. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
M. Holland Company LL217AA LLDPE
(discontinued **) Features: High Clarity, Copolymer, Good ProcessabilityUses: Film, Cast FilmApprovals: FDA 21 CFR 177.1521Processing Method: Blown Film and Cast FilmInformation provided by M. Holland. |
|||
Melt Flow | 2.3 g/10 min | 2.3 g/10 min | ASTM D1238 |
M. Holland Company MAGMA® LM124-C LLDPE
(discontinued **) Features: Good Heat Seal, Good Processability, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |