Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 18.2 g/10 min @Load 1.20 kg, Temperature 300 °C |
18.2 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® FXD121R PC Transparent/translucent PC for light diffusion special effects. MFR of 18.2. Color package may affect performance. |
|||
Melt Flow | 18.2 g/10 min @Load 1.20 kg, Temperature 300 °C |
18.2 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® FXD121R PC (Asia Pacific) Transparent/translucent PC for light diffusion special effects. MFR of 18.2. Color package may affect performance. |
|||
Melt Flow | 18.2 g/10 min @Load 1.20 kg, Temperature 300 °C |
18.2 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® FXE121R PC Transparent PC. ILLUMINATE special effects (fluorescent/edge glow colors). MFR 18.2. Internal mold release. |
|||
Melt Flow | 18.2 g/10 min @Load 1.20 kg, Temperature 300 °C |
18.2 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® FXG121R PC PC in special effects colors. ""Diamond Sparkle"" appearance additives. Color package may affect performance. |
|||
Melt Flow | 18.2 g/10 min @Load 1.20 kg, Temperature 300 °C |
18.2 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® FXM121R PC PC in special effects colors. Metallic and pearlescent additives. Color package may affect performance. |
|||
Melt Flow | 18.2 g/10 min @Load 1.20 kg, Temperature 300 °C |
18.2 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR2210 PC LNP* Lubricomp* Lexan_WR2210 compound is an alternative polymeric wear additive technology. No silicones, superior processability/part appearance. Flow similar to LEXAN 121. |
|||
Melt Flow | 18.2 g/10 min @Load 1.20 kg, Temperature 300 °C |
18.2 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR2210 PC (Asia Pacific) Alternative polymeric wear additive technology. No silicones, superior processability/part appearance. Flow similar to LEXAN 121. |