Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 17.0 - 50.0 g/10 min | 17.0 - 50.0 g/10 min | Average value: 27.7 g/10 min Grade Count:10 |
Overview of materials for Polyetheretherketone, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Melt Flow | 17.0 - 22.0 g/10 min | 17.0 - 22.0 g/10 min | |
Shuman 502 Black Polypropylene Copolymer Good impact strength, excellent chemical resistance, excellent processability, good wear and abrasion resistance, good resistance to fatigue from flexing.Data provided by the manufacturer. |
|||
Melt Flow | 17.0 - 22.0 g/10 min | 17.0 - 22.0 g/10 min | |
Shuman 502C Black Polypropylene Copolymer Excellent impact strength, excellent chemical resistance, excellent processability, good wear and abrasion resistance, good resistance to fatigue from flexing.Data provided by the manufacturer. |
|||
Melt Flow | 17.0 - 22.0 g/10 min | 17.0 - 22.0 g/10 min | |
Shuman 510 Black Polypropylene Homopolymer Excellent chemical resistance, excellent processabilityData provided by the manufacturer. |
|||
Melt Flow | 17.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
17.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 1049 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 17.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
17.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 1527 Thermoplastic Elastomer Notes: Translucent Features: Good Flow; Tough; Good Melt StrengthInformation Provided by Teknor Apex |
|||
Melt Flow | 17.0 g/10 min @Load 21.6 kg, Temperature 190 °C |
17.0 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinvicomp SRF 9702/C Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: Medium Impact Resistance Uses: Electrical/Electronic Applications Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Melt Flow | 17.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
17.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® OBC 4955A Thermoplastic Elastomer Notes: Telcar OBC has superior mechanical strength and higher elongation which will provide a tougher more durable finished product. Telcar OBC can be used in less demanding sealing applications. T.. |
|||
Melt Flow | 17.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
17.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® OBC 4985A Thermoplastic Elastomer Notes: Telcar OBC has superior mechanical strength and higher elongation which will provide a tougher more durable finished product. Telcar OBC can be used in less demanding sealing applications. T.. |
|||
Melt Flow | 17.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
17.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-1431A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 17.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
17.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® OBC 4975A Thermoplastic Elastomer Notes: Telcar OBC has superior mechanical strength and higher elongation which will provide a tougher more durable finished product. Telcar OBC can be used in less demanding sealing applications. T.. |
|||
Melt Flow | 17.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
17.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-2270A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Flow | 17.0 g/10 min @Load 2.16 kg, Temperature 250 °C |
17.0 g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
BASF Ultradur B 4406 G4 PBT Description: Is a PBT, flame-retardant injection-molding grades, with 20% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh.. |
|||
Melt Flow | 17.0 - 52.0 g/10 min | 17.0 - 52.0 g/10 min | Average value: 28.5 g/10 min Grade Count:4 |
Overview of materials for Silicone Polyurethane, Polycarbonate Based This property data is a summary of similar materials in the MatWeb database for the category "Silicone Polyurethane, Polycarbonate Based". Each property range of values reported is minimum and maxim.. |