Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 17 g/10 min @Load 2.16 kg, Temperature 230 °C |
17 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products FT4650-583UV Thermoplastic Polyolefin, UV Stabilized, Exterior DX9 Black Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Melt Flow | 17 g/10 min @Load 2.16 kg, Temperature 230 °C |
17 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products FT4702-698UV Thermoplastic Polyolefin, UV Stabilized, RXF Jet Black Applications: Bumper trimExterior componentsDoor claddingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Melt Flow | 17 g/10 min @Load 2.16 kg, Temperature 230 °C |
17 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products FT4900-772UV Thermoplastic Polyolefin, UV Stabilized, RXF Jet Black Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Melt Flow | 17 g/10 min | 17 g/10 min | ISO 1133 |
Mytex Polymers AN18KW-01 FK Polypropylene, Rubber modified Description: Rubber modified polypropylene produced for automotive interior applications using Mytex® Technology. Specifically designed to achieve ductile performance at cold temperatures during a.. |
|||
Melt Flow | 17 g/10 min @Load 2.16 kg, Temperature 230 °C |
17 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products M15P101-01A 15% Mica Reinforced Polypropylene, Black Applications: Air ducts - distributionFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Melt Flow | 17 g/10 min @Load 2.16 kg, Temperature 230 °C |
17 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products T20P100-00 20% Talc Reinforced Polypropylene, Natural Applications: Electronic housingsConsolesIP componentsHVAC ducts - air distributionClose out panelDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.. |
|||
Melt Flow | 17 g/10 min @Load 2.16 kg, Temperature 230 °C |
17 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products T20P100-517UV 20% Talc Reinforced Polypropylene, UV Stabilized, Interior DX9 Black Applications: Center consolesIP componentsClose out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Melt Flow | 17 g/10 min @Load 1.20 kg, Temperature 300 °C |
17 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® EXL1132 PC Copolymer Lexan* EXL1132 polycarbonate (PC) siloxane copolymer resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high fl.. |
|||
Melt Flow | 17 g/10 min @Load 1.20 kg, Temperature 300 °C |
17 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
Melt Flow | 17 g/10 min @Load 2.16 kg, Temperature 230 °C |
17 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
PolyMirae Moplen HP652P Fiber (BCF/CF) Grade Polypropylene Moplen HP652P is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP652P is a homopolymer particularly suitable for heavy denier BCF .. |
|||
Melt Flow | 17 g/10 min @Load 5.00 kg, Temperature 260 °C |
17 g/10 min @Load 11.0 lb, Temperature 500 °F |
cm³/10 min |
Polimeri Europa KOBLEND PCA 839F PC+ABS
(discontinued **) Symbol according to ISO 1043/1: PC+ABSUnfilled. Suitable for Injection Molding. Supplied as pellets.ISO data. Information provided by EnichemPolimeri Europa now has Enichem's plastics businesses... |
|||
Melt Flow | 17 - 21 g/10 min @Load 5.00 kg, Temperature 230 °C |
17 - 21 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
FKuR Kunststoff Biograde® C 7500 Biodegradable Plastic Compound BIOGRADE® are easy to process blends based on cellulose. BIOGRADE® is composed mainly of natural resources. Based on cellulose, a product of the paper industry BIOGRADE® has been especial.. |
|||
Melt Flow | 17 - 27 g/10 min | 17 - 27 g/10 min | ASTM D1238 |
Lushan EV1050G1/RF EVA Film for Encapsulating Solar modules, Reinforced Friendly EVA film for encapsulating solar modules Lushan EV1050G1 is mainly used for PV module encapsulation. It’s based on an ethylene vinyle acetate (EVA) copolymer and supplemented by special Chemica.. |
|||
Melt Flow | 17 g/10 min @Load 1.20 kg, Temperature 300 °C |
17 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
MRC Polymers NAXELL™ PC117MH General Purpose Polycarbonate, Medium High MFR • Available in natural and custom colors• Can be UV Stabilized• Internal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Melt Flow | 17 g/10 min @Load 2.16 kg, Temperature 230 °C |
17 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LyondellBasell Higlass PF062-4 Polypropylene Homopolymer, 40% Glass Fiber Key Features: high melt flow, high modulus, chemically coupled, glass fiber-reinforced polypropylene homopolymer, high rigidity, high strength, excellent processabilityApplications: appliance parts,.. |
|||
Melt Flow | 17 g/10 min @Load 2.16 kg, Temperature 250 °C |
17 g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
SABIC Innovative Plastics Valox® 420 PBT 30% GR, excellent strength, stiffness and dimensional stability. High heat resistance. Appliance handles, spotlights, electric motors, connectors. |
|||
Melt Flow | 17 g/10 min @Load 10.0 kg, Temperature 250 °C |
17 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® TH-1100 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 17 g/10 min @Load 1.20 kg, Temperature 270 °C |
17 g/10 min @Load 2.65 lb, Temperature 518 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics LNP Thermocomp RX06324 PA 66 (Asia Pacific) This material is Mineral filled Nylon grade with high dielectric constantThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 17 g/10 min @Load 2.16 kg, Temperature 260 °C |
17 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics LNP STAT-LOY SLDM2005 PC (Asia Pacific) Antistatic Polycarbonate, Non Halogen FR V-2 grade, mineral 5% filled |
|||
Melt Flow | 17 g/10 min @Load 2.16 kg, Temperature 190 °C |
17 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Yellow 2200 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 2200 is a yellow color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 2200 contai.. |
|||
Melt Flow | 17 - 23 g/10 min @Load 2.16 kg, Temperature 230 °C |
17 - 23 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 1329H-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1329H-01 is a natural high flow, medium impact polypropylene that is suitable for molding thin parts with long mold flow distances. It permits reduction of injection tem.. |
|||
Melt Flow | 17 - 23 g/10 min @Load 2.16 kg, Temperature 230 °C |
17 - 23 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 1467-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1467-01ApplicationPP 1467-01 meet FDA Regulation 21 CFR 177.1520, for all food contact applications.Information provided by A. Schulman. |
|||
Melt Flow | 17 g/10 min @Load 2.16 kg, Temperature 230 °C |
17 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ FPP 1697HU High Flow Fortified Polypropylene DescriptionPolyfort® FPP 1697HU is a high flow fortified polypropylene with high temperature dimensioned stability. It is stabilized for UV exposure and available in matched automotive color.Infor.. |
|||
Melt Flow | 17 - 23 g/10 min @Load 2.16 kg, Temperature 230 °C |
17 - 23 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 1329H-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1329H-01 is a natural high flow, medium impact polypropylene that is suitable for molding thin parts with long mold flow distances. It permits reduction of injection tem.. |
|||
Melt Flow | 17 g/10 min @Load 1.20 kg, Temperature 300 °C |
17 g/10 min @Load 2.65 lb, Temperature 572 °F |
estimated from MVR using room temperature density; ISO 1133 |
Covestro Makrolon® 2558 Polycarbonate ISO 7391-PC,MR,(,,)-18-9MVR (300 °C/1.2 kg) 14.5 cm3/10 minMedical devicessuitable for ETO and steam sterilization at 121 °CComplies with the requirements of FDA-modified ISO 10993-1 and USP Class.. |
|||
Melt Flow | 17 g/10 min @Load 2.16 kg, Temperature 190 °C |
17 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow ASPUN™ 6835A Linear Low-Density Polyethylene (LLDPE) ASPUN™ 6835A Fiber Grade Resin: Suggested Optimum Process: Staple CardableTypical Application: Yarn & Bonding FibersInformation provided by Dow |
|||
Melt Flow | 17 g/10 min @Load 1.20 kg, Temperature 300 °C |
17 g/10 min @Load 2.65 lb, Temperature 572 °F |
Melt Volume Rate (ml/10 min); ISO 1133 |
Chi Mei Wonderloy® PC-385 PC/ABS Alloy Ultra-high Heat, Ultra-high Impact |
|||
Melt Flow | 17 g/10 min | 17 g/10 min | ASTM D1238 |
Aclo Accutech Polypropylene Homopolymer HP0339M40L Mica Reinforced |