Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 16 g/10 min @Load 2.16 kg, Temperature 230 °C |
16 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products FT5100-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: IP structural componentBody side moldingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Melt Flow | 16 g/10 min @Load 2.16 kg, Temperature 230 °C |
16 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products HP517-00 23% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trim moldingsSill platesTire coverInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Melt Flow | 16 g/10 min @Load 2.16 kg, Temperature 230 °C |
16 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products HP521-00UV 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Natural Applications: Interior trimIP structural componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Melt Flow | 16 g/10 min @Load 2.16 kg, Temperature 230 °C |
16 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products HP521-372 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 110D Medium Dark Pewter Applications: Interior trimIP structural componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Melt Flow | 16 g/10 min @Load 2.16 kg, Temperature 210 °C |
16 g/10 min @Load 4.76 lb, Temperature 410 °F |
|
Noltex Soarnol® H4815 Ethylene Vinyl Alcohol Copolymer Special designed the highest ethylene content grade. Ethylene content 48 mol%.Information provided by Soarus, LLC. In the United States SOARNOL is produced by Noltex, L.L.C., an affiliate of Nippo.. |
|||
Melt Flow | 16 g/10 min | 16 g/10 min | 230/2.16 (typical); ASTM D1238 |
Fiberfil® PP-60/TC/20/VO/ND Polypropylene Homopolymer, 20% Talc Filled, Flame Retardant Information provided by FIBERFIL Engineered Plastics |
|||
Melt Flow | 16 g/10 min @Load 3.80 kg, Temperature 230 °C |
16 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Global PC/ABS-1216 General Purpose Polycarbonate/ABS Alloy Information provided by Global Polymers Corporation. |
|||
Melt Flow | 16 g/10 min @Load 2.16 kg, Temperature 230 °C |
16 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LG Chemical SEETEC M1500 Polypropylene Impact Copolymer SEETEC M1500 is a heterophasic polypropylene copolymer for injection molding applications. SEETEC M1500 exhibits a high flowability and a good balance of stiffness and impact strength. SEETEC M1500 .. |
|||
Melt Flow | 16 g/10 min @Load 5.00 kg, Temperature 260 °C |
16 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
Lucent Polymers PC/ABS-1216LG Polycarbonate+ABS, Low Gloss, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Melt Flow | 16 g/10 min @Load 2.16 kg, Temperature 230 °C |
16 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Multibase Multi-Flex® A 6221 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Thermal Stability, GoodOzone ResistantGeneral PurposeForms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsAutomotive Under the HoodInfo.. |
|||
Melt Flow | 16 g/10 min @Load 2.16 kg, Temperature 260 °C |
16 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
Techmer ES Plastiblend® PC/ABS FR 2810 Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Melt Flow | 16 g/10 min @Load 5.00 kg, Temperature 265 °C |
16 g/10 min @Load 11.0 lb, Temperature 509 °F |
ASTM D1238 |
Techmer ES Plastiblend® PC/PBT IM 1799 BK Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Melt Flow | 16 g/10 min @Load 2.16 kg, Temperature 300 °C |
16 g/10 min @Load 4.76 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL GTX EXNX0080 PPE+PPS (Europe-Africa-Middle East) Noryl APS* EXNX0080 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can.. |
|||
Melt Flow | 16 g/10 min @Load 2.16 kg, Temperature 230 °C |
16 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Daplen™ EE108U Polypropylene TPO Compound Daplen™ EE108U is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, gives.. |
|||
Melt Flow | 16 - 20 g/10 min | 16 - 20 g/10 min | 230/2.16; May be specified; ASTM D1238 |
Plastics Group Polifil® RMC-20V 20% Calcium Carbonate-Reinforced Polypropylene, High Impact, UV Stabilized Polifil® RMC-V series compounds are high impact, UV stabilized polypropylenes reinforced with fine particle size calcium carbonate. In addition to the highest impact possible, these compounds retar.. |
|||
Melt Flow | 16 g/10 min @Load 2.16 kg, Temperature 190 °C |
16 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Red 5670 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 5670 is a red color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® 56.. |
|||
Melt Flow | 16 - 24 g/10 min @Temperature 230 °C |
16 - 24 g/10 min @Temperature 446 °F |
Condition L; ASTM D1238 |
A. Schulman POLYFORT™ PP 1498HU UV Stabilized, Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1498HU is a high flow UV stabilized medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. .. |
|||
Melt Flow | 16 g/10 min | 16 g/10 min | |
Zylog Hipolyene® 3080 HC RM Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Melt Flow | 16 - 24 g/10 min @Temperature 230 °C |
16 - 24 g/10 min @Temperature 446 °F |
Condition L; ASTM D1238 |
A. Schulman POLYFORT™ PP 1498HU UV Stabilized, Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1498HU is a high flow UV stabilized medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. .. |
|||
Melt Flow | 16 g/10 min @Load 2.16 kg, Temperature 190 °C |
16 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Blue 4020 Concentrate Based In Polyethylene DescriptionPOLYBATCH® Blue 4020 is a blue color concentrate based in polyethylene. This concentrate was designed to provide intense blue color in polyolefin film and molding applications. POLYBA.. |
|||
Melt Flow | 16 g/10 min @Load 2.16 kg, Temperature 190 °C |
16 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
ELASTO UK Dryflex® 8010-102 Flame Retardant TPE for Extrusion, Pebble Gray Vitaprene® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Vitaprene® compounds permit sophisticated component design and.. |
|||
Melt Flow | 16 g/10 min @Load 21.6 kg, Temperature 190 °C |
16 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil HDPE HTA 002 High Density Polyethylene Resin Product Description: HTA 002 is a general purpose medium molecular weight HDPE grade, characterized by easy processability, especially in coextrusion and blending with other polyolefins. HTA 002 can.. |
|||
Melt Flow | 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Diamond Polymers PC-1500F Clear, Natural Polycarbonate Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 16 g/10 min | 16 g/10 min | ASTM D1238 |
Aclo Accutech Polypropylene Copolymer CP0437T30L Talc Reinforced |
|||
Melt Flow | 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Covestro Makrolon® Rx1452 Polycarbonate ISO 7391-PC,M,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minMedical devicesLipid resistantsuitable for sterilization with high-energy radiationComplies with the requirements of FDA-modifie.. |
|||
Melt Flow | 16 - 40 g/10 min @Load 5.00 kg, Temperature 232 °C |
16 - 40 g/10 min @Load 11.0 lb, Temperature 450 °F |
ASTM D1238 |
Arkema Group KYNAR® 9000 HD Polyvinylidene Fluoride - Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Melt Flow | 16 g/10 min @Load 2.16 kg, Temperature 230 °C |
16 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Daplen™ EF103AE Polypropylene TPO Compound Daplen™ EF103AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, high melt flow rate an.. |