Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 13.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
13.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite Optix® CA - 51 LL General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Melt Flow | 13.5 g/10 min @Load 5.00 kg, Temperature 260 °C |
13.5 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® CM5820 PC+ABS (Asia Pacific) Cycoloy CM5820 resin is a Mineral Filled Non-FR PC+ABS blend with high impact, high modulus, good chemical resistance & improved surface aesthetic, designed for hand help device chassis that require.. |
|||
Melt Flow | 13.5 g/10 min @Load 2.16 kg, Temperature 260 °C |
13.5 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® FXC630SK PC+ABS Color package may affect performance. PC+ABS, ECO-conforming flame retardant with diamond sparkle appearance. |
|||
Melt Flow | 13.5 g/10 min @Load 2.16 kg, Temperature 260 °C |
13.5 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® FXC630SK PC+ABS (Asia Pacific) PC+ABS, ECO-conforming flame retardant with diamond sparkle appearance. |
|||
Melt Flow | 13.5 g/10 min @Load 5.00 kg, Temperature 260 °C |
13.5 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® IP1000 PC+ABS Automotive applications: High impact and ductility to -22F for interior trim and instrument panel applications. |
|||
Melt Flow | 13.5 g/10 min @Load 5.00 kg, Temperature 260 °C |
13.5 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® IP1000 PC+ABS (Asia Pacific) IP1000 is a high impact PC/ABS blend developed for the automotive instrument panel business. |
|||
Melt Flow | 13.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
13.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite West Optix® CA - 51 LL General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Melt Flow | 13.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
13.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Ineos H13G-00 Polypropylene Homopolymer
(discontinued **) Formerly Amoco® 7444. Suggested fabrication methods: Injection moldingFeatures: General purposeTypical applications: Rigid packaging, Medical componentsComplies with FDA specification, Title 21, C.. |
|||
Melt Flow | 13.5 - 16.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
13.5 - 16.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
|
Kazanorgsintez PC-015 Polycarbonate Production Method: Obtained by means of polycondensation method. Application: Intended for product manufacture by method of die-casting.Information Provided by Kazanorgsintez |
|||
Melt Flow | 13.5 g/10 min | 13.5 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® NA206000 Low Density Polyethylene ApplicationsPETROTHENE NA 206-000 is an extrusion coating resin especially recommended for high-speed, light weight coating applications. The resin can be drawn to a 3 lb/ream coating weight at lin.. |
|||
Melt Flow | 13.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
13.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Ineos H13M-00 Polypropylene Homopolymer Grade H13M-00 is a general purpose polypropylene homopolymer for injection molding applications. It provides good long-term heat stability.Suggested fabrication methods: Injection moldingFeatures: .. |
|||
Melt Flow | 13.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
13.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
IRPC Polimaxx Polene 1196NN Polypropylene Compound CHARACTERISTICS: POLYPROPYLENE HOMOPOLYMER UNREINFORCED, CONTAIN FLAME RETARDANT, UL 94 V-2 APPROVAL, HIGH IMPACT STRENGTHAPPLICATIONS: INJECTION MOLDING FOR ELECTRICAL APPLIANCES |
|||
Melt Flow | 13.5 g/10 min @Load 6.60 kg, Temperature 337 °C |
13.5 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 2212R PEI 20% Milled glass filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Melt Flow | 13.5 g/10 min @Load 6.60 kg, Temperature 337 °C |
13.5 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 2212R PEI (Asia Pacific) 20% Milled glass filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Melt Flow | 13.5 g/10 min @Load 10.0 kg, Temperature 250 °C |
13.5 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® NH-8310 MPPE, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 13.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
13.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex ELEXAR® EL 8421 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Melt Flow | 13.5 g/10 min @Load 5.00 kg, Temperature 280 °C |
13.5 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS Noryl NH6020 resin is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 .. |
|||
Melt Flow | 13.5 g/10 min @Load 5.00 kg, Temperature 280 °C |
13.5 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS (Asia Pacific) Noryl NH6020 resin is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 .. |
|||
Melt Flow | 13.5 g/10 min @Load 5.00 kg, Temperature 280 °C |
13.5 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH6020 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 mm an.. |
|||
Melt Flow | 13.5 g/10 min @Load 10.0 kg, Temperature 250 °C |
13.5 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® NH-8310 MPPE, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 13.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
13.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Supreme Petrochem SP6432 9690 Medium Impact Polystyrene Characteristics High flow Good toughness Available in various colors Processing Injection moldingApplications Air conditioner and cooler grills Refrigerator parts Washing machine components Mate.. |
|||
Melt Flow | 13.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
13.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
cm<sup>3</sup>/10min Melt Volume-flow Rate; ISO 1133 |
DSM Arnitel® VT3104 TPC-ET Extrusion Grade |
|||
Melt Flow | 13.5 g/10 min @Load 2.16 kg, Temperature 250 °C |
13.5 g/10 min @Load 4.76 lb, Temperature 482 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Crastin® HR5315HFS BK591 Polybutylene Terephthalate (PBT)
(Unverified Data**) 15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene.. |
|||
Melt Flow | 13.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
13.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Dow DT702 TPO Dow Fascia TPO for Painted ApplicationsInformation provided by Dow |
|||
Melt Flow | 13.5 g/10 min | 13.5 g/10 min | ASTM D1238 |
Formosa Plastics Formolene® LH5214 Injection Molding HDPE
(discontinued **) High Density Polyethylene for Injection Molding Applications Formolene® LH5214 meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of .. |
|||
Melt Flow | 13.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
13.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Nucrel® 1214 Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating
(discontinued 12 wt% Methacrylic Acid.Nucrel® 1214 is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment des.. |
|||
Melt Flow | 13.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
13.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Ineos H13Z-00 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Packaging, Consumer productsComplies with FDA specification, Title 21, CFR 177.1520.Typical prope.. |