Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 12.1 - 18 g/10 min @Load 1.20 kg, Temperature 300 °C |
12.1 - 18 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Iran Petrochemical (PCC) PC 1218 Polycarbonate Suitable for molding, injection, and blow moldingInformation provided by Iran Petrochemical Commercial Co. |
|||
Melt Flow | 12.1 g/10 min @Load 10.0 kg, Temperature 230 °C |
12.1 g/10 min @Load 22.0 lb, Temperature 446 °F |
Calculated from Volume Flow Rate of 10.5 cm<sup>3</sup>/10 min; ISO 1133 |
DSM Arnitel® EB463 41 Shore D, Blow Molding Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melt Flow | 12.1 g/10 min @Load 10.0 kg, Temperature 230 °C |
12.1 g/10 min @Load 22.0 lb, Temperature 446 °F |
Calculated from Volume Flow Rate of 10.5 cm<sup>3</sup>/10min.; ISO 1133 |
DSM Arnitel® EB463 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melt Flow | 12.1 g/10 min @Load 10.0 kg, Temperature 230 °C |
12.1 g/10 min @Load 22.0 lb, Temperature 446 °F |
Calculated from Volume Flow Rate of 10.5 cm<sup>3</sup>/10 min; ISO 1133 |
DSM Arnitel® EB464 42 Shore D, Blow Molding Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melt Flow | 12.1 - 15.3 g/10 min | 12.1 - 15.3 g/10 min | Average value: 14.1 g/10 min Grade Count:3 |
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu.. |
|||
Melt Flow | 12.1 - 16 g/10 min | 12.1 - 16 g/10 min | D |
Shandong Dongyue Shenzhou New Material Co DS608 Fluorinated Ethylene-Propylene Copolymer For High-Speed Extrusion Conformable with: Q/DYS 003-2007Fluorinated Ethylene Propylene is the copolymer of TFE and HFP, with good thermal stability, outstanding chemical inertness, good electrical insulation, and low coeff.. |
|||
Melt Flow | 12.1 g/10 min @Load 10.0 kg, Temperature 250 °C |
12.1 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL PX2622 PPE+HIPS (Asia Pacific) PPE/HIPS for auto interior |