Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 105 g/10 min @Load 2.16 kg, Temperature 190 °C |
105 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 2318 LLDPE Injection Molding Resin
(discontinued **) Features: Low odor, low warpage, fast cycling, high surface gloss, permits light weight lid design.Applications: Thin walled container lids and closures.Data provided by the manufacturer. |
|||
Melt Flow | 105 - 160 g/10 min @Load 2.16 kg, Temperature 170 °C |
105 - 160 g/10 min @Load 4.76 lb, Temperature 338 °F |
ISO 1133 |
Lubrizol Advanced Materials PEARLBOND® 122 Linear Thermoplastic Polyurethane Pearlbond™ 122 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines an extremely high crystallization rate with a very high thermoplasticit.. |
|||
Melt Flow | 105 - 160 g/10 min @Load 2.16 kg, Temperature 170 °C |
105 - 160 g/10 min @Load 4.76 lb, Temperature 338 °F |
ISO 1133 |
Lubrizol Advanced Materials PEARLBOND® 522 Linear Thermoplastic Polyurethane Pearlbond™ 522 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a very high thermoplasticity level... |
|||
Melt Flow | 105 g/10 min | 105 g/10 min | ASTM D1238 |
Total PPC 4920WZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 4920WZ is a nucleated impact copolymer with a Melt Flow index of 105 g/10 min.TOTAL Polypropylene 4920WZ is characterized by excellent stiffness and impact resista.. |
|||
Melt Flow | 105 g/10 min @Load 2.16 kg, Temperature 210 °C |
105 g/10 min @Load 4.76 lb, Temperature 410 °F |
cm<sup>3</sup>/10 min; ISO 1133 |
EMS-Griltech Griltex® D 1502E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melt Flow | 105 g/10 min @Load 2.16 kg, Temperature 160 °C |
105 g/10 min @Load 4.76 lb, Temperature 320 °F |
cm<sup>3</sup>/10 min; ISO 1133 |
EMS-Griltech Griltex® D 1539E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melt Flow | 105 g/10 min @Load 2.16 kg |
105 g/10 min @Load 4.76 lb |
Melt flow ratio I10/I2 is 6.5. |
Dow DOWLEX™ 2503 Linear Low Density Polyethylene, Narrow MW Distribution DOWLEX® 2503 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer excellent environmental stress crack resistance and tear strength with excellent rigidity. It h.. |
|||
Melt Flow | 105 - 140 g/10 min @Load 2.16 kg, Temperature 235 °C |
105 - 140 g/10 min @Load 4.76 lb, Temperature 455 °F |
ASTM D1238 |
Gromax CCP PBT 1200-211E Product Description: PBT unreinforced middle viscosity injection molding grade.Characteristics:Excellent electrical propertyExcellent temperature resistance, high heat distortion temperature.Excelle.. |