Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 10.8 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.8 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® FXM141R PC (Europe-Africa-Middle East) FXM141R is a Lexan PC grade in Metallic or Pearlescent effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color .. |
|||
Melt Flow | 10.8 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.8 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® ML4506 PC Transparent polycarbonate for aircraft applications requiring FAR 25.853a compliance. Injection moldable. |
|||
Melt Flow | 10.8 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.8 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® FXM141R PC (Asia Pacific) FXM141R is a Lexan PC grade in Metallic or Pearlescent effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color .. |
|||
Melt Flow | 10.8 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.8 g/10 min @Load 2.65 lb, Temperature 572 °F |
Calculated from Volume Flow Rate of 8 cm<sup>3</sup>/10min.; ISO 1133 |
Mitsubishi Xantar® G4F 22 R Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Melt Flow | 10.8 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.8 g/10 min @Load 2.65 lb, Temperature 572 °F |
Calculated from Volume Flow Rate of 8 cm<sup>3</sup>/10min.; ISO 1133 |
Mitsubishi Xantar® G4F 22 UR Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Melt Flow | 10.8 g/10 min @Load 2.16 kg, Temperature 230 °C |
10.8 g/10 min @Load 4.76 lb, Temperature 446 °F |
Calculated from Volume Flow Rate of 9 cm<sup>3</sup>/10 min; ISO 1133 |
DSM Arnitel® PM471 45 Shore D, Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melt Flow | 10.8 g/10 min @Load 2.16 kg, Temperature 230 °C |
10.8 g/10 min @Load 4.76 lb, Temperature 446 °F |
Calculated from Volume Flow Rate of 9 cm<sup>3</sup>/10min.; ISO 1133 |
DSM Arnitel® PM471 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |