Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.6 g/10 min | 1.6 g/10 min | (Condition L) ASTM D-1238 |
Multibase Multi-Flex® TPE A 7606 NAT The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Melt Flow | 1.6 g/10 min | 1.6 g/10 min | ASTM D1238 |
Plaskolite Optix® CA-1000 IG Clear High Impact Acrylic Resin High impact acrylic resin, injection molding and extrusion gradeApplications: A premium impact acrylic resin particularly suited for medical and food uses. This resin offers the best impact resista.. |
|||
Melt Flow | 1.6 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.6 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite Optix® CP - 86 General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Melt Flow | 1.6 g/10 min @Temperature 190 °C |
1.6 g/10 min @Temperature 374 °F |
|
North Wood Plastics PS with 20% Wood Fiber Data provided by North Wood Plastics, Inc. |
|||
Melt Flow | 1.6 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.6 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite West Optix® CP - 86 UVA General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Melt Flow | 1.6 g/10 min | 1.6 g/10 min | |
DuPont Fusabond® MN493D Ethylene Octene Copolymer
(discontinued **) Typical Use: Nylon 6 toughenerNylon 6/6 toughenerComplies to FDA 21CFR 175.105Availability: North AmericaInformation provided by DuPont. |
|||
Melt Flow | 1.6 g/10 min | 1.6 g/10 min | Condition G |
Ineos Nova 1210 High Heat Crystal Polystyrene
(discontinued **) High heat resistance, High molecular weight, optimum performance in extruded foamApplications: Meat and poultry trays, Egg cartons, Food packagingExposure to gamma radiation in the 2.02-6.06 megarad.. |
|||
Melt Flow | 1.6 g/10 min | 1.6 g/10 min | Condition G |
Ineos Nova 1280 High Heat Crystal Polystyrene
(discontinued **) Good processing characteristics, Low residual monomer, Low oligomersApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radiation in the 2.02-6.06 megarad r.. |
|||
Melt Flow | 1.6 g/10 min | 1.6 g/10 min | ExxonMobil Method |
ExxonMobil LD 117.08 Blown Overwrap Film Resin
(discontinued **) LD 117 resins are homopolymer film resins with good clarity and excellent stiffness. Film from LD 117 resins can be used in overwrap applications and push-through type packaging equipment. Film ma.. |
|||
Melt Flow | 1.6 g/10 min | 1.6 g/10 min | Exxon Method |
ExxonMobil Escorene® LD-117 MDPE Blown Overwrap Film Resin, Tough
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity and excellent stiffness. Film made from LD-117 can be used in overwrap applications and in push-through .. |
|||
Melt Flow | 1.6 g/10 min | 1.6 g/10 min | Condition G |
Ineos Nova 1290 High Heat Crystal Polystyrene Good processing characteristics, Low residual monomer, Low oligomersApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radiation in the 2.02-6.06 megarad r.. |
|||
Melt Flow | 1.6 - 2.0 g/10 min @Load 2.61 kg, Temperature 190 °C |
1.6 - 2.0 g/10 min @Load 5.75 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical SEETEC BF415 LDPE Characteristics: Good Processability and Excellent Optical Properties Applications: Masking filmCAS No. 9002-88-4Information provided by LG Chemical |
|||
Melt Flow | 1.6 - 2.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.6 - 2.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem HE 7250 LS-L HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Melt Flow | 1.6 g/10 min | 1.6 g/10 min | ASTM D1238 |
Lucky CF-920 Acrylic May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and coloring capability. |
|||
Melt Flow | 1.6 g/10 min @Load 6.60 kg, Temperature 295 °C |
1.6 g/10 min @Load 14.6 lb, Temperature 563 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM LTX300B PEI (Asia Pacific) Standard flow Polyetherimide blend with low toxicity, smoke, and flame evolution. ECO Compliant, UL94 V0 listing. |
|||
Melt Flow | 1.6 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.6 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D 1238 |
Styrolution PS 1200/1201 GPPS Extrusion / thermoforming foam sheetHigh melt strengthHigh StiffnessUSP Class VI certifiedUL Classification 94 HBInformation provided by Styrolution |
|||
Melt Flow | 1.6 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.6 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® VE-0860 ABS, Unreinforced FR Flame-retardant ABS with high heat resistance that can be used in battery cases and adaptorsInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 1.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont Surlyn® 1650SB DuPont™ Surlyn® 1650SB is available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Slip and antiblock agents are added to .. |
|||
Melt Flow | 1.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont™ Fusabond® N493 Polymer Modifier DuPont™ Fusabond® N493 is an anhydride modified ethylene copolymer. DuPont™ Fusabond® N493 can only be used in the following applications: all polyamide blends and blends for golf balls and ble.. |
|||
Melt Flow | 1.6 g/10 min @Load 2.16 kg |
1.6 g/10 min @Load 4.76 lb |
Melt flow ratio I10/I2 is 10.2. |
Dow AFFINITY™ SE 1400 Polyolefin Plastomer AFFINITY® SE 1400 polyolefin plastomer is an ethylene octene resin that offers excellent performance for profile extrusion of thick tubes and good melt strength for low shear blow molding. It has e.. |
|||
Melt Flow | 1.6 g/10 min | 1.6 g/10 min | ASTM D1238 |
E-Polymers EFLEX® I2030 Ionomer I-series (Ionomer): E-FLEX Ionomer is a family of ethylene acrylic acid (E/AA) copolymers, in which part of the acrylic acid is neutralized with metal ions such as zinc (Zn) or sodium (Na) or magnes.. |
|||
Melt Flow | 1.6 g/10 min @Load 2.16 kg, Temperature 235 °C |
1.6 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® AESN Y T6L Nylon 12, MoS2 Filled (Dry) Designation ISO 1874-PA12,EHLS,22-010,MD05Grade with molybdenum filler for extrusion. Available color: steel gray. Reinforced light and heat stabilizing agents.Low friction coefficient. No need of l.. |
|||
Melt Flow | 1.6 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.6 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Braskem TI4015F Impact Copolymer Polypropylene Description: Superior balance of stiffness and impact strength. Applications: Suggested uses include extrusion applications requiring good impact strength. Process: Extrusion. This resin meets the .. |
|||
Melt Flow | 1.6 g/10 min | 1.6 g/10 min | |
Ashley Polymers Ashlene® ABS Resin F-216 General purpose high impact resin.Data provided by the manufacturer |
|||
Melt Flow | 1.6 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.6 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Braskem TI4015F2 Impact Copolymer Polypropylene Description: Superior balance of stiffness and impact strength. Applications: Suggested uses include extrusion applications requiring good impact strength. Process: Extrusion. This resin meets the r.. |
|||
Melt Flow | 1.6 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.6 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite Optix® CP - 86 UVA General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Melt Flow | 1.6 g/10 min | 1.6 g/10 min | Exxon Method |
ExxonMobil Iotek® 8020 Sodium Ionomer Molding/Extrusion Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A sodium ionomer with excellent abrasion resistance, impact strength, hardness and tensile strength. IOTEK ionomers provide superb low temperature .. |