Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Multibase Nylex™ 4032 Polyamide + PP Forms: PelletsInformation provided by Multibase |
|||
Melt Flow | 1.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Clearflex® H&T FHH 508 Octene Copolymer Linear Medium Density Polyethylene Clearflex H&T FHH 508 is an octene copolymer linear medium density polyethylene (C8-LMDPE), with antioxidant, suitable for blown film extrusion.Films obtained from Clearflex H&T FHH 508 show good op.. |
|||
Melt Flow | 1.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
|
Polycasa Acryl® G 87 E Acrylic Grade for extruding semi-finished products such as twin-strapped panels, profile and tubes, as well as injection molding of watch glasses, dishes, bowls, water-tap hand grips and bathroom fittings, .. |
|||
Melt Flow | 1.5 g/10 min | 1.5 g/10 min | ExxonMobil Method |
ExxonMobil Exceed™ 1518EC Tough Premium Film Resin
(discontinued **) Exceed 1518EC resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1518EC resin have outstanding tensile, impact strength and puncture. These superi.. |
|||
Melt Flow | 1.5 g/10 min | 1.5 g/10 min | Cond. G; ASTM D1238 |
Global ABS-1805 General Purpose ABS
(discontinued **) Information provided by Global Polymers Corporation. |
|||
Melt Flow | 1.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Phillips 66 COPYLENE® CM015 Polypropylene Impact Copolymer COPYLENE™ CM015 is low melt flow impact copolymer with a barefoot additive package and is designed for excellent processing in injection molding and extrusion applications.Applications: Injection M.. |
|||
Melt Flow | 1.5 g/10 min | 1.5 g/10 min | Exxon Method |
ExxonMobil Iotek® 7020 Zinc Ionomer Molding/Extrusion Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A zinc ionomer with excellent flexibility, abrasion resistance, impact strength and tensile strength. This ionomer has outstanding adhesion to glas.. |
|||
Melt Flow | 1.5 - 2.5 g/10 min | 1.5 - 2.5 g/10 min | ±12% |
Kazanorgsintez 158-225 Film Grade Composition of High Density Polyethylene Production Method: Based on polyethylene grades 10803-20, 15803-20, 15813-020,17504-006. Application: Designed for packing manufacture for milk and milk products.Information Provided by Kazanorg.. |
|||
Melt Flow | 1.5 - 2.5 g/10 min | 1.5 - 2.5 g/10 min | ±12% |
Kazanorgsintez 158-76 Film Grade Composition of High Density Polyethylene Production Method: Based on polyethylene grades 10803-20, 15803-20, 15813-020,17504-006. Application: Designed for packing manufacture for milk and milk products.Information Provided by Kazanorg.. |
|||
Melt Flow | 1.5 - 2.5 g/10 min | 1.5 - 2.5 g/10 min | |
Kazanorgsintez 162-280 Low Density Polyethylene Composition with Improved Processibility Production Method: Compositions are produced from low density polyethylene with additives. Application: Intended for cable core lapping.Information Provided by Kazanorgsintez |
|||
Melt Flow | 1.5 g/10 min | 1.5 g/10 min | ASTM D1238 |
LyondellBasell Aquathene® AQ120000 Ethylene Vinylsilane Copolymer ApplicationsAQUATHENE AQ 120-000 is an ethylene vinylsilane copolymer designed for use in low voltage, power cable applications. This natural resin can be crosslinked, by exposure to moisture after.. |
|||
Melt Flow | 1.5 g/10 min | 1.5 g/10 min | ASTM D1238 |
KKPC Kuhmo GP 125H High Transparency GPPS Key features: High Transparency Common Uses: Humidifiers, optical instruments.GPPS has excellent transparence, colorability, electric property, water-resistance, harmlessness, molding processability.. |
|||
Melt Flow | 1.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Ineos Styrenics Polystyrene 168M (NAFTA) High heat, high molecular weight general purpose polystyrene with low crystal clarity. It offers high stiffness for extrusion/thermoforming applications, especially for the food packaging.Informati.. |
|||
Melt Flow | 1.5 - 2.1 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.5 - 2.1 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem PH 0141 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Melt Flow | 1.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
Condition G; ASTM D1238 |
Styrolution NAS® 90 High Performance Styrenic NAS® 90 has sparkling clarity, improved toughness, and good scratch resistance. This easily processed copolymer blends well with clear impact modifiers. It meets USP XXIII Spec. of Class VI Pla.. |
|||
Melt Flow | 1.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis RB307MO Polypropylene Random Copolymer RB307MO is a random copolymer with good transparency and contact clarity, very good gloss and surface finish. This grade also features high heat distortion temperature. Applications: household and.. |
|||
Melt Flow | 1.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 1407L-01 Polypropylene High-Impact Copolymer Polypropylene DescriptionPolypropylene PP 1407L-01 is a super high-impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 1.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Total PPC 3666 Polypropylene, Heterophasic Copolymer, Extrusion Polypropylene PPC 3666 is a heterophasic copolymer with a Melt Flow index of 1.5 g/10 min. This resin offers an outstanding processability in combination with good melt strength and excellent mecha.. |
|||
Melt Flow | 1.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Borealis BorPURE™ MB6561 High Density Polyethylene for Injection Molding BorPure™ MB6561 is a bimodal, high-density polyethylene intended for injection and compression molding. This grade combines excellent organoleptic properties, environmental stress crack resistance .. |
|||
Melt Flow | 1.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis RB607MO Polypropylene Random Copolymer RB607MO is a random copolymer for blow molding, with good transparency and contact clarity, very good gloss and surface finish. Bottles up to 2 liters can be steam sterilized due to heat distortion .. |
|||
Melt Flow | 1.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Exceed™ 1518KC Metallocene Polyethylene Resin Product Description: Exceed 1518KC is a metallocene ethylene-hexene copolymer. Films made from Exceed 1518KC have outstanding tensile, impact strength and puncture. These superior strength propertie.. |
|||
Melt Flow | 1.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LDPE LD 368ON Low Density Polyethylene Resin Product Description: LD 368 series are high clarity EVA LDPE grades, offering good optical properties combined with toughness and impact resistance. Two additive combinations are available according.. |
|||
Melt Flow | 1.5 - 2.5 g/10 min @Load 5.00 kg, Temperature 372 °C |
1.5 - 2.5 g/10 min @Load 11.0 lb, Temperature 702 °F |
|
Daikin NEOFLON AP-231SH PFA Semiconductor Grade NEOFLON PFA semiconductor grade.Applications: Linings, tubing, etc.Information provided by Daikin Industries. |
|||
Melt Flow | 1.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Americas Styrenics STYRON® 685D High Heat Crystal Polystyrene Product CharacteristicsHigh heat resistanceHigh tensile strengthBlue tintFood Contact CompliantUL Classification 94HBUSP Class VITypical ApplicationsFoamOPSMedicalInformation provided by AmericasSty.. |
|||
Melt Flow | 1.5 - 2.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.5 - 2.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Arkema Group Orevac® 9314 Film EVA-MAH Terpolymer EVA Terpolymers based Main Application: Blown film coextrusionInformation provided by Arkema Group |
|||
Melt Flow | 1.5 g/10 min | 1.5 g/10 min | ASTM D1238 |
Huntsman PE1078 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with high clarity and excellent stiffness.Applications: Film extrusion: overwrap packaging.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (.. |
|||
Melt Flow | 1.5 g/10 min @Temperature 230 °C |
1.5 g/10 min @Temperature 446 °F |
Condition L; ASTM D1238 |
A. Schulman PP 2407 Polypropylene Impact Resistant Copolymer Polypropylene DescriptionPolypropylene PP 2407 is a low flow, impact resistant copolymer polypropylene. Information provided by A. Schulman. |
|||
Melt Flow | 1.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Bynel® 41E712 Adhesive Resin
(discontinued **) Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Melt Flow | 1.5 g/10 min | 1.5 g/10 min | |
DuPont Fusabond® MC250D Ethylene Vinyl Acetate (28% VA)
(discontinued **) Typical Use: Adhesion promoterCoupling agent for nonhalogen, flame retarded wire and cable compounds containing fillers such as aluminum trihydrate or magnesium hydroxideAvailability: North AmericaI.. |
|||
Melt Flow | 1.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
|
Arkema Group Oroglas® V 045 Acrylic, Extrusion Grade
(discontinued **) OROGLAS V 045 is a lubricated extrusion grade offering good combination of physical and optical properties.OROGLAS V 045 provides easy processing behavior.OROGLAS V 045 is recommended for extrusion.. |