Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.90 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.90 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Clearflex® H&T FGH 196 Hexene Copolymer Linear Low Density Polyethylene Clearflex H&T FGH 196 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films obtained from Clearflex H&T FGH .. |
|||
Melt Flow | 0.90 g/10 min | 0.90 g/10 min | Condition E; ASTM D 1238 |
Chevron Phillips 6109CL LLDPE Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene Copolymer, High Slip, Very High Antiblock Version of 6109Characteristics: Good Stiffness at Thin Gauges, Good Drawdown, Low COF, Can be used straight or blended with LDPE or HDPE... |
|||
Melt Flow | 0.90 g/10 min | 0.90 g/10 min | Condition E; ASTM D 1238 |
Chevron Phillips 7109DLT LLDPE Blown Film Resin, Hexene Copolymer
(discontinued **) Resin Type: Hexene Copolymer, Very High Antiblock, Processing Aid Version of 7109T, Cast/Blown Film ResinCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blende.. |
|||
Melt Flow | 0.90 g/10 min | 0.90 g/10 min | ASTM D1238 |
Chevron Phillips 7109BK Linear low density polyethylene blown film resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymer, blow film resin, medium slip, medium antiblock version of 7109Characteristics: good stiffness at thin gauges, good drawdown, low COF, c.. |
|||
Melt Flow | 0.90 g/10 min | 0.90 g/10 min | ASTM D1238 |
Formosa Plastics Formolene® L42108E2 Film (Butene Grade) LLDPE
(discontinued **) Butene Copolymer (High slip and antiblock)Applications: Thin gauge blown film with improved stiffnessThin gauge blown film with improved stiffnessInformation provided by Formosa Plastics Corporation.. |
|||
Melt Flow | 0.90 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.90 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® FORMAX® L71709H Film (Hexene Grade) LLDPE
(discontinued **) High Strength Linear Low Density Polyethylene for Film Extrusion Formolene FORMAX® L7 is a high strength linear low density hexene copolymer polyethylene made using a gas-phase process. Film mechan.. |
|||
Melt Flow | 0.90 g/10 min | 0.90 g/10 min | ASTM D1238 |
M. Holland Company LL102 LLDPE
(discontinued **) Additives: Medium Antiblock, Medium SlipFeatures: Medium Antiblocking, Butene Comonomer, Copolymer, Good Drawdown, Good Processability, Medium SlipUses: Film, LinersApprovals: FDA 21 CFR 177.1520(c).. |
|||
Melt Flow | 0.90 g/10 min @Load 2.16 kg |
0.90 g/10 min @Load 4.76 lb |
ASTM D1238 |
Reliance Industries Reclair F19010 Polyethylene Blow film Linear Low Density Polyethylene grade. Reclair F19010 is butene comonomer based, with optimum levels of antioxidants, antiblocking agents, slip additives, and polymer processing aids. Th.. |
|||
Melt Flow | 0.90 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.90 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Inno-Comp INNOPOL® CS 2-8960 60% Barium-Sulfate Filled Polypropylene Block-Copolymer INNOPOL® CS 2-8960 is a 60% Barium-sulfate filled compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-8960 is developed for.. |
|||
Melt Flow | 0.90 g/10 min | 0.90 g/10 min | |
JPJ Technologies 5000S HDPE Extrusion Information provided by JPJ Technologies |
|||
Melt Flow | 0.90 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.90 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) LL0209AA Linear Low Density Polyethylene LL 0209AA is a LLDPE copolymer with butene as comonomer which contains anti-oxidant. It is recommended for general purpose applications.Information provided by Iran Petrochemical Commercial Co. |
|||
Melt Flow | 0.90 g/10 min @Load 2.16 kg |
0.90 g/10 min @Load 4.76 lb |
ISO 1133 |
SIDPEC EGYPTENE® LL 0209 AA LLDPE Film Applications:Heavy duty sacksAgricultural films and linersProduce bags, stretch filmFilm properties were measured on 15 micron film extruded at a blow up ratio of 2:1.Information provided by Interch.. |
|||
Melt Flow | 0.90 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.90 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis BB108E Polypropylene compound for Steel Pipe Coating BB108E is a high molecular weight, low melt flow rate polypropylene block copolymer. Applications: BB108E is recommended for steel pipe coating.Information provided by Borealis AG |
|||
Melt Flow | 0.90 g/10 min @Temperature 230 °C |
0.90 g/10 min @Temperature 446 °F |
Condition L; ASTM D1238 |
A. Schulman POLYFORT™ FPP 1182E Talc Filled, Extrusion Grade Copolymer Polypropylene DescriptionPolyfort® FPP 1182E is a 20% talc-filled, extrusion grade copolymer polypropylene. It had a good balance of flexural modulus, low temperature impact, and appearance properties. Informat.. |
|||
Melt Flow | 0.90 g/10 min | 0.90 g/10 min | LE 4421; ASTM D1238 |
Borealis Visico™ LE4421/LE4460/LE4432 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation Visico LE4421/LE4460/LE4432 is a black, halogen-based flame retardant, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The.. |
|||
Melt Flow | 0.90 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.90 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133/D |
Total Lumicene® mPE M 3509 Medium Density Polyethylene, Blow Molding Lumicene® mPE M 3509 is a metallocene-based medium density polyethylene combining the features of conventional blow molding polyethylene with differentiated optical propertied such as gloss and co.. |
|||
Melt Flow | 0.90 g/10 min @Temperature 230 °C |
0.90 g/10 min @Temperature 446 °F |
Condition L; ASTM D1238 |
A. Schulman POLYFORT™ FPP 1182E Talc Filled, Extrusion Grade Copolymer Polypropylene DescriptionPolyfort® FPP 1182E is a 20% talc-filled, extrusion grade copolymer polypropylene. It had a good balance of flexural modulus, low temperature impact, and appearance properties. Informat.. |
|||
Melt Flow | 0.90 g/10 min | 0.90 g/10 min | ASTM D1238E |
Chevron Phillips MarFlex® 7109 LLDPE Blown Film Resin Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Melt Flow | 0.90 g/10 min | 0.90 g/10 min | ASTM D1238E |
Chevron Phillips MarFlex® 7109DJ LLDPE Blown Film Resin Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Melt Flow | 0.90 g/10 min | 0.90 g/10 min | Condition 190/2.16; ASTM D1238 |
Chevron Phillips MarFlex® D139 m-LLDPE Linear Low Density Polyethylene Low Density PolyethyleneCustomer Benefits: Possesses the typical physical properties of metallocene polyethylenes with the added potential benefit of improved processability (bubble stability, down-.. |
|||
Melt Flow | 0.90 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.90 g/10 min @Load 4.76 lb, Temperature 374 °F |
condition E; ASTM D1238 |
DuPont™ Surlyn® 8920 Ionomer Resin, Sodium Surlyn® 8920 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Melt Flow | 0.90 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.90 g/10 min @Load 4.76 lb, Temperature 374 °F |
condition E; ASTM D1238 |
DuPont™ Surlyn® PC100 Ionomer Resin, Highest Clarity, Sodium Surlyn® PC100 luxury molding resin is a "select" grade of Surlyn® 8920, controlled to achieve the highest possible optical clarity in molded perfume jars and caps. It complies with the provisions .. |
|||
Melt Flow | 0.90 g/10 min | 0.90 g/10 min | ASTM D1238 |
ExxonMobil NTX™ NTX 104 Super Strength Film Resin NTX super strength hexene blown film resins are designed for applications requiring exceptional strength for maximum downgauging potential. Key property improvements are significantly superior impac.. |
|||
Melt Flow | 0.90 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.90 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers SAN 250 Styrene Acrylonitrile, Transparent Engineering Thermoplastic Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 0.90 g/10 min @Load 2.16 kg, Temperature 235 °C |
0.90 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Orgalloy® LE 60HM Flexible Nylon Alloy (Conditioned) LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents).higher in rigidity than LE 6000. For film, hollow vessel blow moldi.. |
|||
Melt Flow | 0.90 - 1.1 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.90 - 1.1 g/10 min @Load 4.76 lb, Temperature 374 °F |
B.P. 112 |
Iran Petrochemical (PCC) Tabriz 0410AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Melt Flow | 0.90 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.90 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Paxon™ EA60-007 Blow Molding Resin
(discontinued **) EA60-007 is an unstabilized blow molding grade high density polyethylene copolymer. The base resin can be compounded to incorporate such things as stabilizers, fillers, and colorants before process.. |
|||
Melt Flow | 0.90 g/10 min | 0.90 g/10 min | Condition E; ASTM D 1238 |
Chevron Phillips 6109L LLDPE Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene Copolymer, Very High Antiblock Version of 6109Characteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPEApplications:Industr.. |
|||
Melt Flow | 0.90 g/10 min | 0.90 g/10 min | Condition E; ASTM D 1238 |
Chevron Phillips 7109DJT LLDPE Blown Film Resin, Hexene Copolymer
(discontinued **) Resin Type: Hexene Copolymer, Medium Antiblock, Processing Aid Version of 7109T, Cast/Blown Film ResinCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended w.. |
|||
Melt Flow | 0.90 g/10 min | 0.90 g/10 min | Condition E; ASTM D 1238 |
Chevron Phillips 6109M LLDPE Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene Copolymer, High Slip, Very High Antiblock Version of 6109Characteristics: Good Stiffness at Thin Gauges, Good Drawdown, Low COF, Can be used straight or blended with LDPE or HDPE... |