Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.28 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.28 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition G; ASTM D1238 |
Global D-2022 Low Density Polyethylene, Film Extrusion Grade
(discontinued **) Description-transparency, high toughness, flexibility, high impact strength, good chemical resistanceApplications-bagsMeets FDA requirements as listed in food additives regulation 21 CFR 117.1520 fo.. |
|||
Melt Flow | 0.28 g/10 min | 0.28 g/10 min | Condition 190/2.16; ASTM D1238 |
Chevron Phillips Marlex® HHM TR-140 Polyethylene, Film Grade; HDPE
(discontinued **) FDA approved.Data provided by the manufacturer |
|||
Melt Flow | 0.28 g/10 min @Load 2.16 kg |
0.28 g/10 min @Load 4.76 lb |
ASTM D 1238 |
Total Finathene® DF 210 HDPE resin
(discontinued **) Applications: Irrigation tape and tubingInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines. |
|||
Melt Flow | 0.28 g/10 min @Load 2.16 kg |
0.28 g/10 min @Load 4.76 lb |
ASTM D1238 |
Reliance Industries Relene E41003 Polyethylene Relene E41003 is a High Density Polyethylene grade with broad molecular weight distribution and good melt strength , suitable for making pipes for water supply, irrigation, sewage and industrial eff.. |
|||
Melt Flow | 0.28 g/10 min @Load 2.16 kg |
0.28 g/10 min @Load 4.76 lb |
ASTM D1238 |
Reliance Industries Relene L41003 Polyethylene The UV stabilized version of Relene E41003Information provided by Reliance Industries |
|||
Melt Flow | 0.28 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.28 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
SCG Chemicals EL-Leneâ„¢ H1000PBL High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stability, good resistance to weathering, good balance of MRS and SCGRecommended Applications: Water pressure pipes and stripe lines for PE100 pi.. |
|||
Melt Flow | 0.28 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.28 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
SCG Chemicals EL-Leneâ„¢ H1000PYL High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stability, good resistance to weatheringRecommended Applications: Stripe lines for PE100 pipe, non pressure pipesCertification: Certified by LNE.. |
|||
Melt Flow | 0.28 g/10 min @Load 2.16 kg |
0.28 g/10 min @Load 4.76 lb |
ASTM D 1238 |
Total CD 4300 HDPE extrusion Applications: General profile extrusion, irradiation-crosslinked productsInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product.. |
|||
Melt Flow | 0.28 g/10 min @Load 2.16 kg |
0.28 g/10 min @Load 4.76 lb |
ASTM D 1238 |
Total HL 428 HDPE film resin Applications: multi-wall liner, poultry multi-layer gas flush bags, mailing envelopes, heavy-duty shipping sacks, fresh cut produce packaging, coextrusionInformation provided provided by Total Petro.. |
|||
Melt Flow | 0.28 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.28 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Total HL 428 HDPE Film Grade Medium molecular weight grade. Excellent processability, excellent compatibility with LDPE and LLDPE, good tear and impact strength, good stiffness, excellent drawdown, and good moisture barrier pro.. |
|||
Melt Flow | 0.28 g/10 min | 0.28 g/10 min | ASTM D1238 |
ExxonMobil LDPE LD 358BW Low Density Polyethylene Resin (European Grade) Product Description: LD 358BW is an EVA LDPE which offers a combination of excellent sealability and toughness even at low temperatures.Availability: Europe Additive: Antiblock: NoSlip: No Thermal .. |
|||
Melt Flow | 0.28 g/10 min @Load 2.16 kg |
0.28 g/10 min @Load 4.76 lb |
ASTM D 1238 |
Total Finathene® HL 328 HDPE resin
(discontinued **) Applications: Specialty merchandise bags, millinery/notion bags, mailing envelopes, heavy-duty shipping sacks, shrink films, fresh cut produce packaging, coextrusionInformation provided provided by .. |
|||
Melt Flow | 0.28 g/10 min @Load 2.16 kg |
0.28 g/10 min @Load 4.76 lb |
ASTM D 1238 |
Total CD 471 HDPE conduit Applications: Wire and cable conduit, fiber optic innerductInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines. |
|||
Melt Flow | 0.28 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.28 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 59D HDPE Blow Molding Resin
(discontinued **) Features: High impact resistance, good stiffness, moderate ESCR.Applications: Food packaging, small parts (HIC), oil bottles.Data provided by the manufacturer. |
|||
Melt Flow | 0.28 g/10 min @Load 2.16 kg |
0.28 g/10 min @Load 4.76 lb |
ASTM D1238 |
Reliance Industries Relene B31101 Polyethylene Steel pipe coating base High Density Polyethylene resin. Characteristics:broad molecular weight distribution, good melting strength, excellent toughness/ESCR, and good cut through/abrasion resistanc.. |