Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.270 - 4.80 g/10 min | 0.270 - 4.80 g/10 min | Average value: 2.15 g/10 min Grade Count:17 |
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Film This property data is a summary of similar materials in the MatWeb database for the category "Linear Medium Density Polyethylene (LMDPE), Film". Each property range of values reported is minimum and.. |