Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.112 - 40.0 g/10 min | 0.112 - 40.0 g/10 min | Average value: 8.51 g/10 min Grade Count:239 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |