Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.300 - 45.0 g/10 min | 0.300 - 45.0 g/10 min | Average value: 15.9 g/10 min Grade Count:42 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m.. |
|||
Melt Flow | 1.00 - 45.0 g/10 min | 1.00 - 45.0 g/10 min | Average value: 25.3 g/10 min Grade Count:4 |
Overview of materials for Nylon 6, Glass Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu.. |
|||
Melt Flow | 2.00 - 45.0 g/10 min | 2.00 - 45.0 g/10 min | Average value: 17.3 g/10 min Grade Count:3 |
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl.. |
|||
Melt Flow | 15.0 - 45.0 g/10 min @Load 10.0 kg, Temperature 190 °C |
15.0 - 45.0 g/10 min @Load 22.0 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBB3462 Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (400000 ppm) Features: General Purpose Uses: Non-specific Food Applications Forms: Pellets Pro.. |
|||
Melt Flow | 20.0 - 45.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
20.0 - 45.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBW1994 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (500000 ppm) Forms: Pellets Features: General PurposeInformation Provided by Teknor .. |
|||
Melt Flow | 1.20 - 45.0 g/10 min | 1.20 - 45.0 g/10 min | Average value: 13.5 g/10 min Grade Count:24 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum.. |
|||
Melt Flow | 3.00 - 45.0 g/10 min | 3.00 - 45.0 g/10 min | Average value: 13.8 g/10 min Grade Count:6 |
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |