Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 26 - 36 g/10 min @Load 5.00 kg, Temperature 365 °C |
26 - 36 g/10 min @Load 11.0 lb, Temperature 689 °F |
ASTM D1238 |
Solvay Specialty Polymers Radel® R-5900 Polyphenylsulfone (PPSU) Radel® R-5900 polyphenylsulfone (PPSU) offers medium melt viscosities for long flow lengths and greater injection molding ease. It also provides exceptional hydrolytic stability and toughness tha.. |
|||
Melt Flow | 30 - 36 g/10 min @Temperature 230 °C |
30 - 36 g/10 min @Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ PP 1930UX Extra High Flow, UV Stabilized Copolymer Polypropylene DescriptionPolyfort® PP 1930UX is an extra high flow, heat resistant, UV stabilized copolymer polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 30 - 36 g/10 min @Temperature 230 °C |
30 - 36 g/10 min @Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ PP 1930UX Extra High Flow, UV Stabilized Copolymer Polypropylene DescriptionPolyfort® PP 1930UX is an extra high flow, heat resistant, UV stabilized copolymer polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 30 - 36 g/10 min @Temperature 230 °C |
30 - 36 g/10 min @Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ PP 1930UX Extra High Flow, UV Stabilized Copolymer Polypropylene DescriptionPolyfort® PP 1930UX is an extra high flow, heat resistant, UV stabilized copolymer polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 30 - 36 g/10 min @Temperature 230 °C |
30 - 36 g/10 min @Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ PP 1930UX Extra High Flow, UV Stabilized Copolymer Polypropylene DescriptionPolyfort® PP 1930UX is an extra high flow, heat resistant, UV stabilized copolymer polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 30 - 36 g/10 min @Temperature 230 °C |
30 - 36 g/10 min @Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ PP 1930UX Extra High Flow, UV Stabilized Copolymer Polypropylene DescriptionPolyfort® PP 1930UX is an extra high flow, heat resistant, UV stabilized copolymer polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 30 - 36 g/10 min @Temperature 230 °C |
30 - 36 g/10 min @Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ PP 1930UX Extra High Flow, UV Stabilized Copolymer Polypropylene DescriptionPolyfort® PP 1930UX is an extra high flow, heat resistant, UV stabilized copolymer polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 24 - 36 g/10 min | 24 - 36 g/10 min | |
Asahi Glass Fluon® P-62XP PFA Perfluoropolymer Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character.. |
|||
Melt Flow | 24 - 36 g/10 min | 24 - 36 g/10 min | |
Asahi Glass Fluon® P-830UP PFA Perfluoropolymer Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character.. |