Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 20 - 30 g/10 min @Load 2.16 kg, Temperature 230 °C |
20 - 30 g/10 min @Load 4.76 lb, Temperature 446 °F |
STN EN ISO 1133 |
Plastcom PLASTALEN® PQ 81 N 003 Polypropylene with improved impact strength PP copolymer regranulate for injection molding, impact modified. General use in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Plastcom spol.. |
|||
Melt Flow | 25 - 30 g/10 min @Load 5.00 kg, Temperature 190 °C |
25 - 30 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Polyplastic Armoflen® PO MF 65-4 Polypropylene, 65% Calcium Carbonate Information provided by PolyPlastic Group. |
|||
Melt Flow | 10 - 30 g/10 min @Load 2.16 kg, Temperature 190 °C |
10 - 30 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NatureWorks® Ingeo™ 3001D Injection Grade PLA NatureWorks® PLA (polylactide) polymer 3001D is designed for injection molding applications. It is designed for clear applications with heat deflection temperatures lower than 130ºF (55ºC). Appli.. |
|||
Melt Flow | 15 - 30 g/10 min @Load 2.16 kg, Temperature 210 °C |
15 - 30 g/10 min @Load 4.76 lb, Temperature 410 °F |
ASTM D1238 |
NatureWorks® Ingeo™ 6201D Fiber Grade PLA NatureWorks® PLA polymer 6201D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6201D is designed for extrusion into mechanically .. |
|||
Melt Flow | 15 - 30 g/10 min @Load 2.16 kg, Temperature 210 °C |
15 - 30 g/10 min @Load 4.76 lb, Temperature 410 °F |
ASTM D1238 |
NatureWorks® Ingeo™ 6204D Fiber Grade PLA NatureWorks® PLA polymer 6204D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6204D is designed for extrusion into mechanically .. |
|||
Melt Flow | 18 - 30 g/10 min @Load 1.20 kg, Temperature 300 °C |
18 - 30 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-GP4-[color]-3 Polycarbonate, UV-stabilized, Easy Flow Polycarbonate, UV-stabilized, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Melt Flow | 18 - 30 g/10 min @Load 1.20 kg, Temperature 300 °C |
18 - 30 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-GP4-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Easy Flow Polycarbonate, FDA-compliant Feedstocks, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Melt Flow | 18 - 30 g/10 min @Load 1.20 kg, Temperature 300 °C |
18 - 30 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-GP4-[color]-6 Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samp.. |
|||
Melt Flow | 20 - 30 g/10 min @Load 1.20 kg, Temperature 300 °C |
20 - 30 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-IM4 Polycarbonate, Impact Modified, Easy Flow Polycarbonate, Impact Modified, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Melt Flow | 20 - 30 g/10 min | 20 - 30 g/10 min | ASTM D1238 |
Polymer Resources PPX-GP4 Modified PPO, General Purpose with HDT of 210 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Flow | 18 - 30 g/10 min @Load 1.20 kg, Temperature 300 °C |
18 - 30 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-FD4 Polycarbonate, FDA-compliant Feedstocks, Easy Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Easy Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Melt Flow | 18 - 30 g/10 min @Load 1.20 kg, Temperature 300 °C |
18 - 30 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-UV4-[color]-1 Polycarbonate, UV-stabilized, Easy Flow with Mold Release Polycarbonate, UV-stabilized, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Melt Flow | 20 - 30 g/10 min @Load 2.16 kg, Temperature 230 °C |
20 - 30 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238/L |
NIZHNEKAMSKNEFTEKHIM PP 1300R (Z30G) Propylene Homopolymer Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P.. |
|||
Melt Flow | 5.0 - 30 g/10 min | 5.0 - 30 g/10 min | ASTM D1238 |
Polymer Resources PEI-GP1 Polyetherimide, General Purpose, Unreinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Flow | 15 - 30 g/10 min @Load 5.00 kg, Temperature 200 °C |
15 - 30 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Kraton® D2109 DS-N (SBS) Compound Description: Kraton D2109 DS-N is an easy processing, general purpose 45 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Melt Flow | 15 - 30 g/10 min @Load 2.16 kg, Temperature 170 °C |
15 - 30 g/10 min @Load 4.76 lb, Temperature 338 °F |
ISO 1133 |
Lubrizol Advanced Materials PEARLBOND® 120 Linear Thermoplastic Polyurethane Pearlbond® 120 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines an extremely high crystallization rate with a very high thermoplasticity .. |
|||
Melt Flow | 10 - 30 g/10 min @Load 2.16 kg, Temperature 170 °C |
10 - 30 g/10 min @Load 4.76 lb, Temperature 338 °F |
ISO 1133 |
Lubrizol Advanced Materials Pearlbond® 180 Thermoplastic Polyurethane Pearlbond™ 180 is a linear, polyester-based polyurethane, supplied in form of small white granules, which combines a very high crystallization rate with a very high thermoplasticity level. It i.. |
|||
Melt Flow | 10 - 30 g/10 min @Load 2.16 kg, Temperature 170 °C |
10 - 30 g/10 min @Load 4.76 lb, Temperature 338 °F |
ISO 1133 |
Lubrizol Advanced Materials Pearlbond® 550 Thermoplastic Polyurethane Pearlbond™ 550 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a very high thermoplasticity level... |
|||
Melt Flow | 10 - 30 g/10 min @Load 2.16 kg, Temperature 170 °C |
10 - 30 g/10 min @Load 4.76 lb, Temperature 338 °F |
ISO 1133 |
Lubrizol Advanced Materials Pearlbond® 580 Thermoplastic Polyurethane Pearlbond™ 580 is a linear, Polyester-based TPU, supplied in form of white spherical granules with a very high crystallization rate and a very high thermoplasticity level.Application: Pearlbond.. |
|||
Melt Flow | 15 - 30 g/10 min | 15 - 30 g/10 min | Melt Volume Rate (cm³/10 min) |
Huntsman IROGRAN® A 92 P 4207 TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
Melt Flow | 22.1 - 30 g/10 min @Load 1.20 kg, Temperature 300 °C |
22.1 - 30 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Iran Petrochemical (PCC) PC 2230 Polycarbonate Suitable for injection moldingInformation provided by Iran Petrochemical Commercial Co. |
|||
Melt Flow | 20 - 30 g/10 min @Temperature 230 °C |
20 - 30 g/10 min @Temperature 446 °F |
Condition L; ASTM D1238 |
A. Schulman POLYFORT™ PP 2175HU Toyota High Flow Copolymer Polypropylene DescriptionPolyfort® PP 2175HU Toyota is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 20 - 30 g/10 min @Temperature 230 °C |
20 - 30 g/10 min @Temperature 446 °F |
Condition L; ASTM D1238 |
A. Schulman POLYFORT™ PP 2175HU-31 High Flow Copolymer Polypropylene DescriptionPolyfort® PP 2175HU-31 is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 20 - 30 g/10 min @Temperature 230 °C |
20 - 30 g/10 min @Temperature 446 °F |
Condition L; ASTM D1238 |
A. Schulman POLYFORT™ PP 2175HU Toyota High Flow Copolymer Polypropylene DescriptionPolyfort® PP 2175HU Toyota is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 20 - 30 g/10 min @Temperature 230 °C |
20 - 30 g/10 min @Temperature 446 °F |
Condition L; ASTM D1238 |
A. Schulman POLYFORT™ PP 2175HU-31 High Flow Copolymer Polypropylene DescriptionPolyfort® PP 2175HU-31 is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 20 - 30 g/10 min @Temperature 230 °C |
20 - 30 g/10 min @Temperature 446 °F |
Condition L; ASTM D1238 |
A. Schulman POLYFORT™ FPP 1007X Extra High Flow, Talc Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1007X is an extra high flow, 40% talc fortified homopolymer polypropylene. Information provided by A. Schulman. |
|||
Melt Flow | 20 - 30 g/10 min @Temperature 230 °C |
20 - 30 g/10 min @Temperature 446 °F |
Condition L; ASTM D1238 |
A. Schulman POLYFORT™ PP 2175HU Toyota High Flow Copolymer Polypropylene DescriptionPolyfort® PP 2175HU Toyota is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 20 - 30 g/10 min | 20 - 30 g/10 min | |
Daikin NEOFLON RP-5000 EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Melt Flow | 25 - 30 g/10 min @Load 1.20 kg, Temperature 190 °C |
25 - 30 g/10 min @Load 2.65 lb, Temperature 374 °F |
die 8/1; ISO 1133 |
Addcomp PRIEX® 20097 Maleic Anhydride Grafted PP homopolymer Fields of application: Functionalised polypropylene to be used as compatibiliser for polymer blends or coupling agent for glass fibre, wood flour, natural fibres, multilayer films, aluminium foils, .. |