Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 15 - 25 g/10 min @Load 11.6 kg, Temperature 250 °C |
15 - 25 g/10 min @Load 25.6 lb, Temperature 482 °F |
ASTM D1238 |
Polymer Resources PPX-FR5 Modified-PPO, V-0 Flame Retardant Modified-Polyphenylene Oxide, V-0 Flame Retardant, 225F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Melt Flow | 12 - 25 g/10 min @Load 2.16 kg, Temperature 250 °C |
12 - 25 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Polymer Resources TP-GP1 Polybutylene Terephthalate, General Purpose, Flow Modified Polybutylene Terephthalate, General Purpose, Flow ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Melt Flow | 12 - 25 g/10 min @Load 2.16 kg, Temperature 250 °C |
12 - 25 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Polymer Resources TP-GP1F Polybutylene Terephthalate, General Purpose, FDA-compliant Feedstocks Polybutylene Terephthalate, General Purpose, FDA-compliant FeedstocksProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Melt Flow | 15 - 25 g/10 min @Load 2.16 kg, Temperature 170 °C |
15 - 25 g/10 min @Load 4.76 lb, Temperature 338 °F |
DIN 53.735 |
Lubrizol Advanced Materials PEARLBOND® 110 Linear Thermoplastic Polyurethane
(discontinued **) PEARLBOND® 110 is a linear, aromatic polyurethane, supplied in form of white slightly yellowish pellets, which combines a high crystallization rate with a low thermoplasticity level.Applications: P.. |
|||
Melt Flow | 17 - 25 g/10 min | 17 - 25 g/10 min | ±15% |
Kazanorgsintez 294-73 High Density Polyethylene Composite Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: Composition of HD grad.. |
|||
Melt Flow | 15 - 25 g/10 min @Load 2.16 kg, Temperature 150 °C |
15 - 25 g/10 min @Load 4.76 lb, Temperature 302 °F |
|
Taiwan Sheen Soon Sheenthane® AH-580 TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for soft hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes.. |
|||
Melt Flow | 15 - 25 g/10 min @Load 2.16 kg, Temperature 150 °C |
15 - 25 g/10 min @Load 4.76 lb, Temperature 302 °F |
|
Taiwan Sheen Soon Sheenthane® AH-780 TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for hotmelt adhesiveNon-yellowing, aliphatic gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized... |
|||
Melt Flow | 15 - 25 g/10 min @Load 2.16 kg, Temperature 150 °C |
15 - 25 g/10 min @Load 4.76 lb, Temperature 302 °F |
|
Taiwan Sheen Soon Sheenthane® AH-781 TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for hotmelt adhesiveNon-yellowing, aliphatic gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized... |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
Shuman 910 Utility Black Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
Shuman 910-05V0 Utility Black Polycarbonate Glass Filled Easy processability, heat resistance, weatherability, color stability, self extinguishing5% glass fiber for foam moldingInformation provided by Shuman Plastics, Inc. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
Shuman 920 Black Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
Shuman 930 White Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
Shuman 930-05V0 White Polycarbonate Glass Filled Easy processability, heat resistance, weatherability, color stability, self extinguishing5% glass fiber for foam moldingInformation provided by Shuman Plastics, Inc. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
Shuman FR910V0 Utility Black Polycarbonate Flame Retardant Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
Shuman FR980V0 Grey Polycarbonate Flame Retardant Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
Shuman SP910 Utility Black Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self-extinguishing.Data provided by the manufacturer. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
Shuman SP920 Black Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self-extinguishing.Data provided by the manufacturer. |
|||
Melt Flow | 15 - 25 g/10 min @Load 2.16 kg, Temperature 150 °C |
15 - 25 g/10 min @Load 4.76 lb, Temperature 302 °F |
|
Taiwan Sheen Soon Sheenthane® AH-500 TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for soft hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes.. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ PP 3701 Information provided by A. Schulman. |
|||
Melt Flow | 20 - 25 g/10 min @Temperature 230 °C |
20 - 25 g/10 min @Temperature 446 °F |
Condition L; ASTM D1238 |
A. Schulman POLYFORT™ FPP 1902HU Talc Fortified Polypropylene DescriptionPolyfort® FPP 1902 HU is a 10% talc fortified polypropylene. It exhibits high flow and is stabilized for UV resistance. Information provided by A. Schulman. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ PP 3701 Information provided by A. Schulman. |
|||
Melt Flow | 20 - 25 g/10 min @Temperature 230 °C |
20 - 25 g/10 min @Temperature 446 °F |
Condition L; ASTM D1238 |
A. Schulman POLYFORT™ FPP 1902HU Talc Fortified Polypropylene DescriptionPolyfort® FPP 1902 HU is a 10% talc fortified polypropylene. It exhibits high flow and is stabilized for UV resistance. Information provided by A. Schulman. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ PP 3701 Information provided by A. Schulman. |
|||
Melt Flow | 17 - 25 g/10 min @Load 2.16 kg, Temperature 280 °C |
17 - 25 g/10 min @Load 4.76 lb, Temperature 536 °F |
Z-011A |
Zeon Chemicals Zeonex® 480R Cyclo-Olefin Polymer |
|||
Melt Flow | 10 - 25 g/10 min @Load 8.70 kg, Temperature 170 °C |
10 - 25 g/10 min @Load 19.2 lb, Temperature 338 °F |
|
Lubrizol ESTANE® GP65AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 65AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ISO 1133 |
CTC SunPro® SP 200 P 5000 Polypropylene Copolymer SunPro® SP 200 P 5000 is a general purpose, medium flow, polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Certifications: MS DB5.. |
|||
Melt Flow | 15 - 25 g/10 min @Load 5.00 kg, Temperature 230 °C |
15 - 25 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
E-Polymers EFLEX® M500 SEBS M-series: E-FLEX M series resins are a maleic anhydride grafted (MAH) polymer concentrate designed as synthetic rubber and polyolefin manufactured by E-Polymers. It offers excellent adhesion to nyl.. |
|||
Melt Flow | 6.0 - 25 g/10 min @Load 12.5 kg, Temperature 232 °C |
6.0 - 25 g/10 min @Load 27.6 lb, Temperature 450 °F |
ASTM D1238 |
Arkema Group KYNAR® 740 Black/Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purityAppli.. |
|||
Melt Flow | 6.0 - 25 g/10 min @Load 12.5 kg, Temperature 232 °C |
6.0 - 25 g/10 min @Load 27.6 lb, Temperature 450 °F |
ASTM D1238 |
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Melt Flow | 15 - 25 g/10 min | 15 - 25 g/10 min | ASTM D1238 |
Polymer Resources PPX-MF-FR1 Modified PPO, UL 94 V-0 with HDT of 190 F, Mineral Reinforced
(Unverified Da Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |