Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 6.0 - 12 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.0 - 12 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Polymer Resources AC-GP2 Acetal Copolymer, Medium Flow Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Melt Flow | 5.0 - 12 g/10 min @Load 2.16 kg, Temperature 265 °C |
5.0 - 12 g/10 min @Load 4.76 lb, Temperature 509 °F |
ASTM D1238 |
Polymer Resources PC/TP-FR2 Flame Retardant PC/Polyester Alloy Flame Retardant, High Impact, Excellent Chemical ResistanceFeatures: • Flame Retardant • Impact Modified • Self Extinguishing • Good Chemical ResistanceProcess: Injection MoldingNotes: All p.. |
|||
Melt Flow | 6.0 - 12 g/10 min @Load 2.16 kg, Temperature 265 °C |
6.0 - 12 g/10 min @Load 4.76 lb, Temperature 509 °F |
ASTM D1238 |
Polymer Resources PC/TP-GP3-IM PC/Polyester Alloy, Impact Modified Superior Chemical Resistance, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide.. |
|||
Melt Flow | 5.0 - 12 g/10 min @Load 1.20 kg, Temperature 300 °C |
5.0 - 12 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-G15 Polycarbonate, 15% Glass Reinforced Polycarbonate, 15% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polym.. |
|||
Melt Flow | 3.0 - 12 g/10 min @Load 1.20 kg, Temperature 300 °C |
3.0 - 12 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-G30-TFE15 Polycarbonate, 30% Glass Reinforced, 15% PTFE Polycarbonate, 30% Glass Reinforced, 15% PTFEProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide.. |
|||
Melt Flow | 5.0 - 12 g/10 min @Load 1.20 kg, Temperature 300 °C |
5.0 - 12 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-HM-FR1-[color]-3 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Melt Flow | 8.0 - 12 g/10 min | 8.0 - 12 g/10 min | ASTM D1238 |
Kolon KOCETAL® LW301 Wear Modified Acetal Resin Special polymer added, improved wear property. Applications: Products for low noise and precision gear. Information provided by API-Kolon. |
|||
Melt Flow | 8.1 - 12 g/10 min | 8.1 - 12 g/10 min | B |
Shandong Dongyue Shenzhou New Material Co DS600 Perfluorinated Ethylene-Propylene Copolymer Conformable with: Q/DYS 003-2007Fluorinated Ethylene Propylene resin is the copolymer of the TFE and HFP, with good thermal stability, outstanding chemical inertness, good electrical insulation, and.. |
|||
Melt Flow | 8.0 - 12 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.0 - 12 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
A. Schulman PP 984 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 984 is a medium impact polypropylene used primarily for automotive parts subjected to impact.Information provided by A. Schulman. |
|||
Melt Flow | 8.0 - 12 g/10 min | 8.0 - 12 g/10 min | 230/2.16; May be specified; ASTM D1238 |
Plastics Group Polifil® C-30 30% Calcium Carbonate-Reinforced Polypropylene Polifil® C series compounds are homopolymer polypropylene resins reinforced with fine particle size calcium carbonate. They combine high impact with stiffness, heat aging, good colorability, resist.. |
|||
Melt Flow | 8.0 - 12 g/10 min | 8.0 - 12 g/10 min | 230/2.16; May be specified; ASTM D1238 |
Plastics Group Polifil® C-40 40% Calcium Carbonate-Reinforced Polypropylene Polifil® C series compounds are homopolymer polypropylene resins reinforced with fine particle size calcium carbonate. They combine high impact with stiffness, heat aging, good colorability, resist.. |
|||
Melt Flow | 8.0 - 12 g/10 min | 8.0 - 12 g/10 min | 230/2.16; May be specified; ASTM D1238 |
Plastics Group Polifil® M-40 40% Mica-Reinforced Polypropylene Polifil® M series compounds are homopolymer polypropylene resins reinforced with mica. They combine an improved range of high-stiffness values with low mold shrinkage. These compounds are used in l.. |
|||
Melt Flow | 8.0 - 12 g/10 min | 8.0 - 12 g/10 min | 230/2.16; May be specified; ASTM D1238 |
Plastics Group Polifil® RMC-30 30% Calcium Carbonate-Reinforced Polypropylene, High Impact Polifil® RMC series compounds are high impact polypropylenes reinforced with fine particle size calcium carbonate. In addition to the highest impact possible, they possess good stiffness, heat agin.. |
|||
Melt Flow | 8.0 - 12 g/10 min | 8.0 - 12 g/10 min | 230/2.16; May be specified; ASTM D1238 |
Plastics Group Polifil® RMT-30 30% Talc-Reinforced Polypropylene, High Impact Polifil® RMT series compounds are high impact polypropylenes reinforced with asbestos-free talc. In addition to high impact strength, they possess a high flex modulus and high heat deflection resis.. |
|||
Melt Flow | 8.0 - 12 g/10 min | 8.0 - 12 g/10 min | 230/2.16; May be specified; ASTM D1238 |
Plastics Group Polifil® T-40 40% Talc-Reinforced Polypropylene Polifil® T series compounds are homopolymer polypropylene resins reinforced with asbestos-free talc. They possess high flex modulus, high deflection temperature, good chemical resistance and colora.. |
|||
Melt Flow | 8.0 - 12 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.0 - 12 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
A. Schulman PP 984 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 984 is a medium impact polypropylene used primarily for automotive parts subjected to impact.Information provided by A. Schulman. |
|||
Melt Flow | 6.0 - 12 g/10 min @Temperature 230 °C |
6.0 - 12 g/10 min @Temperature 446 °F |
Condition L; ASTM D1238 |
A. Schulman PP 1349 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1349 is a medium impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 8.0 - 12 g/10 min | 8.0 - 12 g/10 min | 230/2.16; May be specified; ASTM D1238 |
Plastics Group Polifil® GFPP-30 30% Glass-Reinforced Polypropylene Polifil® GFPP series compounds are homopolymer polypropylene resins reinforced with glass fibers. They provide high impact with increased strength, stiffness, surface hardness, and higher continuou.. |
|||
Melt Flow | 8.0 - 12 g/10 min | 8.0 - 12 g/10 min | ASTM D1238 |
Buckeye Polymers BP FLEX D4107 C BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Melt Flow | 8.0 - 12 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.0 - 12 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
AKG Polymers Vision PP PPC BL1008 Polypropylene Copolymer Compound Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin.. |
|||
Melt Flow | 9.0 - 12 g/10 min | 9.0 - 12 g/10 min | Cond. O, for C1175 |
Ashley Polymers Ashlene® C1174,C1175 Polycarbonate These are also available with UV, designated by -3. For release, add R. These are all flame retardant grades developed for various applications such as electrical, electronic, lighting, computer, .. |
|||
Melt Flow | 8.0 - 12 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.0 - 12 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Aaron Industries AAROPRENE® TFIPP 2020 High Impact Talc Filled Polypropylene AAROPRENE® TFIPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Melt Flow | 8.0 - 12 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.0 - 12 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Aaron Industries AVPP C 200-2 Virgin Polypropylene Melt flow index may be specified. |
|||
Melt Flow | 4.0 - 12 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.0 - 12 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Aaron Industries AVPS H 100-3 Virgin Polystyrene Melt flow index may be specified. |
|||
Melt Flow | 8.0 - 12 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.0 - 12 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Aaron Industries AAROPRENE® GFIPP 2010 High Impact Glass Filled Polypropylene AAROPRENE® GFIPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Melt Flow | 8.0 - 12 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.0 - 12 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Aaron Industries AAROPRENE® GFPP 2020 Glass Filled Polypropylene AAROPRENE® GFPP 2000 Series Glass Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Melt Flow | 4.0 - 12 g/10 min | 4.0 - 12 g/10 min | 200/5; May be specified; ASTM D1238 |
Plastics Group Polifil® RP-HIPS High Impact Polystyrene Polifil® RP-High Impact Polystyrene (HIPS) combines the good stiffness properties of polystyrene, with enhanced impact properties gained by the addition of impact modifiers, usually butadiene rubbe.. |
|||
Melt Flow | 4.0 - 12 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.0 - 12 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 - ISO 1133 |
DuPont Elvaloy® HP443 Ethylene/N-Butyl Acrylate/Carbon Monoxide Copolymer
(discontinued **) A low volatile version of Elvaloy® HP441Availability: GloballyInformation provided by DuPont. |