Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.24 - 0.36 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.24 - 0.36 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem GF 5250 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Melt Flow | 0.24 - 0.36 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.24 - 0.36 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem MB 0310 MDPE IPQ employs Spherilene technology from Basell in the production of MDPE. The raw materials, which are supplied by COPESUL, are pre-treated and fed into gas-phase reactors, where medium density polye.. |