Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 99 g/10 min @Load 5.00 kg, Temperature 260 °C |
99 g/10 min @Load 11.0 lb, Temperature 500 °F |
Calculated from MVR using melt density; ISO 1133 |
Lanxess Durethan® B 31 SK 000000 Nylon 6 PA 6, injection molding grade, non-reinforced, easy flow, easy-release, rapid solidification, crystallizes somewhat more finely and uniformly than B 30 S |