Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 9.5 g/10 min | 9.5 g/10 min | ASTM D1238 |
Multibase Multi-Pro® 2008 X Polypropylene Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Melt Flow | 9.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
9.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers F7000 Polystyrene Description: Ignition RetardantInformation provided by Network Polymers Inc. |
|||
Melt Flow | 9.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
9.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
PolyMirae Moplen EP648N Injection Molding Grade Polypropylene Moplen EP648N is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP648N is a high gloss block copolymer particularly suitable fo.. |
|||
Melt Flow | 9.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Bynel® 3120 Acid-/Acrylate-Modified EVA Adhesive Resin
(discontinued **) Bynel® Series 3100 resins are acid/acrylate-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to proce.. |
|||
Melt Flow | 9.5 g/10 min | 9.5 g/10 min | ASTM D1238 |
LyondellBasell Microthene® F FE53200 Ethylene Vinyl Acetate Copolymer General DescriptionMicrothene F polyolefin powders are ultra-fine, spherically shaped particles with narrow size distribution suitable for use in a broad range of specialty applications. Microthene.. |
|||
Melt Flow | 9.5 g/10 min @Load 5.00 kg, Temperature 280 °C |
9.5 g/10 min @Load 11.0 lb, Temperature 536 °F |
|
LG Chemical LUMILOY GP2200 Injection Molding Grade, General Purpose 20% Glass Reinforced PPE NSF Certified for KA02 and E2035. Noted for High Flow, High Impact Strength, and Hydrolytic Stability. Uses include electric/electronic parts and water pump Housing or impellers and other parts wi.. |
|||
Melt Flow | 9.5 g/10 min @Load 5.00 kg, Temperature 280 °C |
9.5 g/10 min @Load 11.0 lb, Temperature 536 °F |
|
LG Chemical LUMILOY GP2300 Injection Molding Grade, General Purpose 30% Glass Reinforced PPE NSF Certified for KA02 and E2035. Noted for High Impact Strength, and Hydrolytic Stability. Uses include electric/electronic parts and water pump Housing or impellers and other parts with water co.. |
|||
Melt Flow | 9.5 g/10 min @Load 2.16 kg, Temperature 250 °C |
9.5 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
LG Chemical LUPOY GN5001RFM PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, General PurposeApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Melt Flow | 9.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
|
Mitsubishi Iupilon® S2000R 9.5 MFI Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Melt Flow | 9.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
|
Mitsubishi Iupilon® S2000UR 9.5 MFI, UV Stabilized Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Melt Flow | 9.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
9.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
LyondellBasell Adflexâ„¢ KS311P Polyolefin Description: Adflexâ„¢ KS-311P thermoplastic olefin resin is a barefoot formulation (no slip, no antiblock) designed for cast film extrusion applications. It is based on proprietary Basell proces.. |
|||
Melt Flow | 9.5 g/10 min @Load 6.60 kg, Temperature 337 °C |
9.5 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 4001 PEI PTFE filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
Melt Flow | 9.5 g/10 min @Load 6.60 kg, Temperature 337 °C |
9.5 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 4001 PEI (Asia Pacific) PTFE filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
Melt Flow | 9.5 g/10 min @Load 5.00 kg, Temperature 266 °C |
9.5 g/10 min @Load 11.0 lb, Temperature 511 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® V2105U PBT Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |
|||
Melt Flow | 9.5 g/10 min @Load 2.16 kg, Temperature 250 °C |
9.5 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® AR-6508 PBT/PET, Glass Filled Good WeatherabilityInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 9.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
9.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Styrolution PS 495F HIPS Styrolution PS 495F is a high flow, high impact polystyrene with a good heat resistance and a high stiffness.High flow HIPSGood heat resistance with high stiffnessSuitable for gas-assisted injection.. |
|||
Melt Flow | 9.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
9.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Styrolution PS 495N HIPS Styrolution PS 495N is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss.High flowGood balance of toughness and heat resistanceUL 94 HBInfor.. |
|||
Melt Flow | 9.5 g/10 min @Load 5.00 kg, Temperature 280 °C |
9.5 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL EXNL0357 PPE+PS |
|||
Melt Flow | 9.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Westlake EF608 Low Density Polyethylene Westlake EF608 is a high melt index LDPE resin suggested for thin gauge garment films and other films requiring excellent drawdown. The high melt index makes this material a good choice in compound.. |
|||
Melt Flow | 9.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
|
Covestro Makrolon® 2803 Polycarbonate, Injection Grade Medium flowing injection molding grade with UV stabilizer.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name .. |
|||
Melt Flow | 9.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
|
Covestro Makrolon® 2805 Polycarbonate, Injection Grade Medium flowing injection molding grade with easy mold release, Makrolon grade 2858 for food contact applications.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separ.. |
|||
Melt Flow | 9.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
|
Covestro Makrolon® 6465 Polycarbonate, Injection Grade Medium viscosity, flame retardant injection molding with easy mold burning behavior.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and offici.. |
|||
Melt Flow | 9.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
|
Covestro Makrolon® 6557 Polycarbonate, Injection Grade Medium viscosity, flame retardant injection molding grade with easy mold release, UV-stabilized.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer A.. |
|||
Melt Flow | 9.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LDPE LD 516.LN Low Density Polyethylene Resin Product Description: LD 516.LN is a medium MI, low density polyethylene resin designed for use in color concentrates and masterbatches where its flow properties ensure improved processability and un.. |
|||
Melt Flow | 9.5 - 11.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.5 - 11.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Arkema Group Orevac® 9307 Y Film EVA-MAH Terpolymer EVA Terpolymers based Main Applications: Extrusion coating Skin packaging adhesive Thermo-adhesive filmsInformation provided by Arkema Group |
|||
Melt Flow | 9.5 g/10 min @Load 2.16 kg, Temperature 275 °C |
9.5 g/10 min @Load 4.76 lb, Temperature 527 °F |
|
Arkema Group Orgalloy® RS 66M25 Nylon 66 Alloy, 25% Mineral Filled (Conditioned) RS 66 series, rigid polyamide 66 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional propertie.. |
|||
Melt Flow | 9.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Azoty Tarnow™ TARNOFORM 500 GF6 POM 30% glass fiber reinforced, high flow injection molding grade, suitable for applications where high strength and stiffness is required, combined with higher flowability during molding.Information pr.. |
|||
Melt Flow | 9.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
9.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Americas Styrenics STYRON A-TECH® 1400AS High Impact Polystyrene Product CharacteristicsHigh FlowGood ImpactFood Contact CompliantTypical ApplicationsTelevision housingsPrinter HousingsConsumer goodsInformation provided by AmericasStyrenics LLC. |