Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 9.00 - 14.0 g/10 min @Load 1.10 kg, Temperature 300 °C |
9.00 - 14.0 g/10 min @Load 2.43 lb, Temperature 572 °F |
ASTM D1238 |
Oxford Polymers PC 714-FR Series PC, Flame retardant Product Description: Amorphous, Polycarbonate injection molding grade, flame retardant Processing and Delivery Form: Pellets and Injection MoldingAdditives: Release Agents and UV stabilizersSpecial.. |
|||
Melt Flow | 9.00 - 18.0 g/10 min | 9.00 - 18.0 g/10 min | Average value: 13.7 g/10 min Grade Count:3 |
Overview of materials for Liquid Crystal Polymer (LCP), Unfilled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Unfilled". Each property range of values reported is minimum and maximum v.. |
|||
Melt Flow | 9.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
9.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 1097D Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 9.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
9.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Sinpolene TPP1040 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Talc Filler, 40% Filler by Weight Uses: Automotive Applications; Housings Forms: Pellets Processing Method: Injection .. |
|||
Melt Flow | 9.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
9.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Synres® PP G10 17 Polypropylene, Glass Reinforced Notes: The Specialty Compounding Division offers a proprietary line of glass reinforced polypropylene. Typical applications include automotive, building and construction, industrial as well as many .. |
|||
Melt Flow | 9.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
9.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Synres® PP G20 62 Polypropylene, Glass Reinforced Notes: The Specialty Compounding Division offers a proprietary line of glass reinforced polypropylene. Typical applications include automotive, building and construction, industrial as well as many .. |
|||
Melt Flow | 9.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
9.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-1155A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 9.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
9.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-1183A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 9.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
9.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-1273A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 9.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
9.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Uniprene® UN-2028A UMB Thermoplastic Elastomer Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Melt Flow | 9.00 g/10 min @Load 2.16 kg, Temperature 175 °C |
9.00 g/10 min @Load 4.76 lb, Temperature 347 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-2069B Thermoplastic Elastomer Uses: Caps; Food Packaging; Liners Pellets Processing Method: Extrusion; Injection Molding; Press Molding Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpmIn.. |
|||
Melt Flow | 9.00 g/10 min @Load 10.0 kg, Temperature 220 °C |
9.00 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Abstron KU602 ABS Heat Resistant High ImpactInformation provided by Bhansali |
|||
Melt Flow | 9.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
9.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Sinpolene CPP2040 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Calcium Carbonate Filler, 30% Filler by Weight Features: Copolymer Uses: Automotive Applications; Industrial Applicati.. |
|||
Melt Flow | 9.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
9.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Sinpolene FRF2074 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Features: Flame Retardant Uses: Appliance Components; Housings Forms: PelletsInformation Provided by Teknor Apex |
|||
Melt Flow | 9.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
9.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Sinpolene TPP1030 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Talc Filler, 30% Filler by Weight Uses: Automotive Applications; Housings Forms: Pellets Processing Method: Injection .. |
|||
Melt Flow | 9.00 - 22.0 g/10 min | 9.00 - 22.0 g/10 min | Average value: 16.4 g/10 min Grade Count:8 |
Overview of materials for Acetal Copolymer, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Melt Flow | 9.00 - 15.0 g/10 min | 9.00 - 15.0 g/10 min | Average value: 12.0 g/10 min Grade Count:4 |
Overview of materials for Polycarbonate, Glass Fiber & Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber & Bead Filled". Each property range of values reported is minimum and maximum.. |
|||
Melt Flow | 9.00 - 110 g/10 min | 9.00 - 110 g/10 min | Average value: 54.6 g/10 min Grade Count:7 |
Overview of materials for Polymethylpentene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polymethylpentene, Molded". Each property range of values reported is minimum and maximum values of appr.. |
|||
Melt Flow | 9.00 g/10 min @Load 10.0 kg, Temperature 220 °C |
9.00 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Abstron KU602 ABS Heat Resistant High ImpactInformation provided by Bhansali |