Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 8.5 g/10 min | 8.5 g/10 min | ASTM D1238 |
Multibase Multi-Pro® 1510 CNU White Polypropylene Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Melt Flow | 8.5 g/10 min @Load 5.00 kg, Temperature 260 °C |
8.5 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Melt Flow | 8.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
8.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® 194 PC Nonhalogenated. 8.5 MFR. High impact. Thick wall sections. Opaques only. FDA food contact compliant in limited colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 8.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
8.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® OQ4620 PC Optical grade with UV cut-off up to 400 nm, greater optical purity than standard grades. For needs of sunglass and sunvisor markets.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 8.5 g/10 min @Load 5.00 kg, Temperature 260 °C |
8.5 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® C1150E PC+ABS (Asia Pacific) High impact, extrusion grade polycarbonate/ABS alloy. |
|||
Melt Flow | 8.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
8.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM Data |
Americas Styrenics Styron® 482 High Impact Polystyrene
(discontinued **) STYRON® 482 high impact polystyrene resin is a high flow resin typically used in toys. When used unmodified for the manufacture of food contact articles STYRON 482 complies with the US Food, Drug a.. |
|||
Melt Flow | 8.5 g/10 min @Load 5.00 kg, Temperature 190 °C |
8.5 g/10 min @Load 11.0 lb, Temperature 374 °F |
|
Total Finaprene® 602 Styrene-Butadiene TPE Copolymer, Uncompounded
(discontinued **) Styrene-Butadiene CopolymerDescription: Finaprene® 602 is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its broad molecular weight distribution, Finaprene® 60.. |
|||
Melt Flow | 8.5 g/10 min @Load 2.16 kg, Temperature 260 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
Ravago Manufacturing Americas Hybrid S470H Acrylonitrile Butadiene Styrene + PC Alloy Available in North America Flame Retardant RoHS Compliant UL File Number: E157012 Form: Pellets Processing Method: Injection Molding Information provided by Ravago |
|||
Melt Flow | 8.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Phillips 66 COPYLENE® CH085S Polypropylene, Homopolymer, Cast Film, Slip COPYLENE™ CH085S is a controlled rheology polypropylene homopolymer resin containing slip additive. COPYLENE™ CH085S is used in injection molding and cast film extrusion applications. Applications.. |
|||
Melt Flow | 8.5 - 11 g/10 min | 8.5 - 11 g/10 min | ASTM D1238 |
Kolon KOCETAL® GF705 G/F Reinforced Acetal Resin Glass fiber reinforced, improved stiffnessApplications: Products for high stiffness, improved fatigue properties. Information provided by API-Kolon. |
|||
Melt Flow | 8.5 g/10 min @Load 5.00 kg, Temperature 260 °C |
8.5 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Ineos ABS Triax® KU2-3154 ABS + Polyamide Blend (Conditioned), Injection Molding Grade Triax® KU2-3154 is mineral reinforced, easy-flowing, injection molding grade, and comes in pellets. It has reduced moisture absorption and very low warpage. |
|||
Melt Flow | 8.5 g/10 min | 8.5 g/10 min | ASTM D1238 |
KKPC Kuhmo MIB IT Blow Molding HIPS Key features: Vacuum Molding. Common Uses: Stirred type yot container.HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between impact-resis.. |
|||
Melt Flow | 8.5 g/10 min @Load 5.00 kg, Temperature 280 °C |
8.5 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL SE1X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V1, UL746C F1. Dielectric strength. Suitable for E/E market indoor/outdoor applications. |
|||
Melt Flow | 8.5 g/10 min @Load 5.00 kg, Temperature 300 °C |
8.5 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Melt Flow | 8.5 g/10 min @Load 5.00 kg, Temperature 300 °C |
8.5 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS (Europe-Africa-Middle East) Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Melt Flow | 8.5 g/10 min @Load 5.00 kg, Temperature 280 °C |
8.5 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL GTX GTX987 PPE+PA66 (Europe-Africa-Middle East) Conductive GTX, CTE 7 |
|||
Melt Flow | 8.5 g/10 min | 8.5 g/10 min | ISO 1133 |
Wico Plast Wicolon 807 Polycarbonate, U.V. Stabilized ApplicationsInjection moldingCharacteristics:U.V. stabilizedAll information provided by Wico Plast, Warenhandelsges. mbH |
|||
Melt Flow | 8.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
8.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM Data |
Dow AIM® 4810 High Impact Styrenic Resin AIM® 4810 advanced styrenic resin is designed to offer the processability of high impact polystyrene and the gloss and practical toughness of high gloss ABS. It can be processed at lower temperatur.. |
|||
Melt Flow | 8.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
8.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM Data |
Dow Tyril® 990 SAN TYRIL® 990 SAN copolymer grade provides colorless glass-like clarity and excellent overall optical properties. It provides a profile of very good strength with stiffness, chemical resistance, heat .. |
|||
Melt Flow | 8.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Chi Mei Kibiton® PB-5502 Styrene-Butadiene Copolymer Hot melt adhesive |
|||
Melt Flow | 8.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Barlog Plastics KEBAFORM C 3090(K) POM Copolymer, 27% glass fiber reinforced POM-GF27Information provided by BARLOG plastics GmbH. |
|||
Melt Flow | 8.5 g/10 min @Load 2.16 kg, Temperature 220 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 428 °F |
ISO 1133 |
DuPont Performance Polymers Hytrel® 4068FG TPC-ET
(Unverified Data**) Hytrel® 4068FG is a high performance thermoplastic polyester elastomer with food compliance specificity.Information provided by DuPont Performance Polymers |