Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 8.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products F43-01B 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Drip trayFunctional supportsA/C housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Melt Flow | 8.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products FT2500-630UV Thermoplastic Polyolefin, UV Stabilized, 500F Light Charcoal Applications: Air DamsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Melt Flow | 8.0 g/10 min | 8.0 g/10 min | ASTM D1238 |
Mytex Polymers AX1166 Polypropylene, Talc filled, Compounded Description: Talc filled compounded polypropylene produced for automotive interior applications using Mytex® Technology.Key Applications: InteriorInformation provided by Mytex Polymers |
|||
Melt Flow | 8.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
8.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers NPS 90-0827 Polystyrene Description: Injection Molding Grade, High ImpactInformation provided by Network Polymers Inc. |
|||
Melt Flow | 8.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
8.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 505RU PC Lexan* 505RU is a glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEEE/Ro.. |
|||
Melt Flow | 8.0 - 18 g/10 min @Load 2.16 kg, Temperature 250 °C |
8.0 - 18 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Polymer Resources TPSF-FRG10 Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced, Flame RetardantProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, .. |
|||
Melt Flow | 8.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
SABIC CC862 High Density Polyethylene for Injection Molding Product Description: SABIC HDPE CC862 is a high density polyethylene specially developed for still water bottle caps that meet organoleptic properties requirements. The material offers and ideal c.. |
|||
Melt Flow | 8.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
8.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
PTS Tristar® PC-08 8 MFI Extrusion Grade Polycarbonate Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Flow | 8.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
8.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Polimeri Europa Sinkral® D 232/M3 ABS Resin
(discontinued **) Special low gloss extrusion/ co-extrusion grade, with good flow. Designation: Thermoplastic ISO 2580-ABS 1, EGN, 105-08-09-15Applications: Sinkral D 232-M3 is widely used in the extrusion / co-extr.. |
|||
Melt Flow | 8.0 g/10 min @Load 2.16 kg, Temperature 330 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 626 °F |
|
Covestro Apec® DP 1-9379/5 Polycarbonate
(discontinued **) Key Features:Release agentUnfilledSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Ba.. |
|||
Melt Flow | 8.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
8.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D-1238 |
Chevron Phillips K-Resin® KR01BR SBC
(discontinued **) K-Resin® Styrene-Butadiene Copolymer (SBC)Applications:Molded boxes with integral hingesMedical devicesDisplaysToysMedia packagingFeatures:Good stiffnessGood toughnessGood warpage resistanceExcelle.. |
|||
Melt Flow | 8.0 - 13 g/10 min | 8.0 - 13 g/10 min | ASTM D1238 |
Kolon KOCETAL® K300LO Low Odor Acetal Resin Low odor of formaldehyde gas. Applications: Products for low odor. Information provided by API-Kolon. |
|||
Melt Flow | 8.0 g/10 min | 8.0 g/10 min | |
Global TPO-55D TPO Grade Data provided by Global Polymers Corporation. |
|||
Melt Flow | 8.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Lucobit Lucofin® 1415 Polyolefin TPO Granules, Signal White Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Melt Flow | 8.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
8.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
LG Chemical Lupoy 1302UV-08 Polycarbonate Resin Description: LUPOY PC 1302UV-08 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Melt Flow | 8.0 g/10 min | 8.0 g/10 min | ASTM D1238 |
Tipco Tipcolene® PPC FR V0 - UL94-V0 Flame Retardant Polypropylene Copolymer V-0 Flame Retardant PP CopolymerApplications: Electrical & AppliancesProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Melt Flow | 8.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Total HDPE 6480 High Density Polyethylene, Clarity Cast Film Resin Polyethylene: Clarity High Density Cast Film ResinCharacteristics:High stiffnessHigh clarityExcellent surface glossHigh tensile strengthGood barrier propertiesLow gel contentApplications:OverwrapFo.. |
|||
Melt Flow | 8.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman PAPERMATCH® T-4338/50 Specialty Masterbatch DescriptionPAPERMATCH® T-4338/50 is a specialty masterbatch formulated to impart paper-like properties to HDPE films. PAPERMATCH® T-4338/50 is a white, medium opacity grade designed to provide a .. |
|||
Melt Flow | 8.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
8.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Diamond Polymers Centrex® 825 Sheet Extrusion Grade Centrex 825 resin is a high-gloss, high-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it .. |
|||
Melt Flow | 8.0 g/10 min | 8.0 g/10 min | 200'C/5,000g; ASTM D-1238 |
Bapolan® 6450 Polystyrene Injection Molding Resin Bapolan 6450 is a high impact polystyrene resin designed for injection molding applications requiring fast cycle times, superior impact and gloss. It complies with US FDA21 CFR177.1640 and 94HB UL .. |
|||
Melt Flow | 8.0 g/10 min | 8.0 g/10 min | ASTM D1238 |
Buckeye Polymers BP RPP 2508 T Polypropylene, 25% Mineral Filled This Talc-filled product exhibits excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and mar resistance, and resis.. |
|||
Melt Flow | 8.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
BASF Novolen® 1184 L Polypropylene Nucleated grade with high processing stability containing antistatic for thermoformed parts.Data was collected by ISO methods and provided by BASF. |
|||
Melt Flow | 8.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
BASF Novolen® 2448 L Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Melt Flow | 8.0 - 12 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.0 - 12 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Aaron Industries AVPP C 200-2 Virgin Polypropylene Melt flow index may be specified. |
|||
Melt Flow | 8.0 g/10 min @Load 2.16 kg, Temperature 235 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Orgalloy® RS 6000CD Nylon 6 Alloy, Rigid Grade (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties.. |
|||
Melt Flow | 8.0 - 10 g/10 min | 8.0 - 10 g/10 min | |
Ashley Polymers Ashlene® R190B Acetal General purpose reprocessed copolymer, excellent toughness, strength, stiffness and lubricity. Black. Available in UV stabilized grades: R190-B2 (good weatherability); R190-H2B (maximum weatherab.. |
|||
Melt Flow | 8.0 - 10 g/10 min | 8.0 - 10 g/10 min | 230/3.8, nominal; ASTM D1238 |
Plastics Group Polifil® RP-ABS Acrylonitrile-Butadiene Styrene, High Flow Version Polifil® RP- Acrylonitrile-Butadiene Styrene is a styrenic resin with improved toughness and heat resistance versus HIPS grades. ABS exhibits high gloss, low shrinkage, and good dimensional stabili.. |
|||
Melt Flow | 8.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman PAPERMATCH® T-4228-50 Specialty Masterbatch DescriptionPAPERMATCH® T-4228/50 is a specialty masterbatch formulated to impart paper-like properties to HDPE films. PAPERMATCH® T-4228/50 is a white, medium opacity grade designed to provide a .. |