Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 7.8 g/10 min | 7.8 g/10 min | (Condition L) ASTM D-1238 |
Multibase Multi-Flex® TPE D 6208 BLK Ash is 2%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Melt Flow | 7.8 - 12.8 g/10 min @Load 1.20 kg, Temperature 250 °C |
7.8 - 12.8 g/10 min @Load 2.65 lb, Temperature 482 °F |
|
Kazanorgsintez PC-075A Polycarbonate Production Method: Obtained by means of polycondensation method. Application: Intended for manufacture of optical products by method of die-casting (including CD, DVD, and other discs), as well .. |
|||
Melt Flow | 7.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
7.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 2100R PEI 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Melt Flow | 7.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
7.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 2100R PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Melt Flow | 7.8 g/10 min @Load 10.0 kg, Temperature 220 °C |
7.8 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® GR-4010 ABS, 10% Glass Filled Material with 10% GF reinforcement with high stiffness that can be used in refrigerator vegetable boxesInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 7.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
7.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Silon Taboradd 23-08350 Processing Aid Masterbatch Masterbatch with a highly effective processing aid for polyethylene, especially PE-X and PE-HD.Information provided by Silon |
|||
Melt Flow | 7.8 g/10 min @Load 10.0 kg, Temperature 220 °C |
7.8 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® GR-4010 ABS, 10% Glass Filled Material with 10% GF reinforcement with high stiffness that can be used in refrigerator vegetable boxesInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 7.8 g/10 min @Load 5.00 kg, Temperature 300 °C |
7.8 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL GTX GTX673 PPE+PA Conductive Noryl GTX* resin designed for profile extrusion. This grade can be electrostatic or powder coat painted without the need for a primer. In addition, its high heat capability allows it to .. |
|||
Melt Flow | 7.8 g/10 min @Load 5.00 kg, Temperature 300 °C |
7.8 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be.. |
|||
Melt Flow | 7.8 g/10 min @Load 5.00 kg, Temperature 300 °C |
7.8 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA (Asia Pacific) Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be.. |
|||
Melt Flow | 7.8 g/10 min @Load 5.00 kg, Temperature 300 °C |
7.8 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA (Europe-Africa-Middle East) Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be.. |
|||
Melt Flow | 7.8 g/10 min @Load 2.16 kg, Temperature 330 °C |
7.8 g/10 min @Load 4.76 lb, Temperature 626 °F |
ISO 1133 |
Covestro Apec® 2095 Polycarbonate Easy flowingeasy to demoldsoftening temperature (VST/B 120)=203 °CPreprocessingMax. Water content |
|||
Melt Flow | 7.8 g/10 min @Load 2.16 kg, Temperature 330 °C |
7.8 g/10 min @Load 4.76 lb, Temperature 626 °F |
ISO 1133 |
Covestro Apec® 2097 Polycarbonate Easy flowingeasy to demoldUV-stabilizedsoftening temperature (VST/B 120)=202 °CPreprocessingMax. Water content |