Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 7.0 g/10 min | 7.0 g/10 min | (Condition L) ASTM D-1238-94a |
Multibase Multi-Flex® TPO D-6208 Data provided by Multibase. |
|||
Melt Flow | 7.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
7.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
Procedure A; ASTM D1238 |
PolyOne Maxxam™ PPC-20T Nat Polypropylene Copolymer (PP Copolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HFD1034 PC Copolymer 7 MFR LEXAN HFD Copolymer UV-stabilized, available in transparent colors only |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® LUX2614G PC (Asia Pacific) Lexan LUX2614G (EXRL0944) is a diffusive, high viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develop.. |
|||
Melt Flow | 7.0 g/10 min @Load 2.16 kg, Temperature 260 °C |
7.0 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer (Asia Pacific) Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3.. |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 101 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated, 7.0 MFR, for thicker sections without sinks. |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 953 PC Opaque colors, high viscosity, superior flame retardance. UV-stabilized. |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 955 PC Lexan* 955 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in various opaque color.. |
|||
Melt Flow | 7.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
7.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Nucrel® 30707HS Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating
(discontinued **) 7 wt% Acrylic Acid.Nucrel® 30707HS is an ethylene-acrylic acid copolymer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusio.. |
|||
Melt Flow | 7.0 g/10 min | 7.0 g/10 min | ASTM D1238 |
Hyosung Topilene C600H PP C600H Film Grade Butane Random CopolymerApplications: Sealable CPP/OPPCharacteristics:Very low sealSlip propertyTransparencyInformation provided by Hyosung Corporation |
|||
Melt Flow | 7.0 g/10 min | 7.0 g/10 min | ASTM D1238 |
Hyosung Topilene C600Y PP C600Y Butene Random CopolymerApplications: FilmCharacteristics:Excellent transparency & glossLow sealing temperatureHigh hot-tack strengthGood stiffnessInformation provided by Hyosung Corporation |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
LG Chemical Lupoy 1301V-7 Polycarbonate Resin Description: LUPOY PC 1301V-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.. |
|||
Melt Flow | 7.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
7.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Lucobit Lucofin® 1400MN Powder Ethylene Butyl Acrylate Lucofin 1400MN Powder is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400MN Powder is softer and more flexible ethane et.. |
|||
Melt Flow | 7.0 g/10 min @Load 5.00 kg, Temperature 260 °C |
7.0 g/10 min @Load 11.0 lb, Temperature 500 °F |
|
Ineos ABS Triax® 1120 ABS + Polyamide Blend (DAM) Key Features:UnfilledPlatableHigh impact or high impact modifiedSuitable processing methods:Injection moldingFilm extrusionBlow molding |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics PC0700 PC (Europe-Africa-Middle East) PC0700 resin is a low flow (MFR = 7 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. It.. |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics PC0703R PC (Asia Pacific) PC0703R resin is a low flow (MFR = 7 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the extrusion market. |
|||
Melt Flow | 7.0 g/10 min @Load 6.60 kg, Temperature 337 °C |
7.0 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D 1238 |
SABIC Innovative Plastics Ultem 2100N PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 7.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
7.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® WR-9140 General Purpose ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Flow | 7.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
7.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
PlastxWorld CEVIAN® SER91 ABS General purpose and flame retarded ABS with excellent moldability and no plate-out.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Informat.. |
|||
Melt Flow | 7.0 g/10 min | 7.0 g/10 min | |
Toyobo GLAMIDE® TY-502NZ 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Melt Flow | 7.0 g/10 min | 7.0 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ FXP 1943 CaC03 and Glass Fiber Hybrid Copolymer Polypropylene DescriptionPolyfort® FXP 1943 is a 20% CAC03 and glass fiber hybrid copolymer polypropylene product. Information provided by A. Schulman. |
|||
Melt Flow | 7.0 g/10 min | 7.0 g/10 min | ASTM D1238 |
ExxonMobil Escorene™ UL 00728CC Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00728CC is a copolymer of ethylene and vinyl acetate.Processing Conditions: Processing temperatures above 220°C (428°F) may cause resin degradation.Availability: Africa & M.. |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Entec Hylex® P1007L1 HB Polycarbonate Available in North America Agency Ratings: FDA 21 CFR 177.1580 RoHS Compliant Form: Pellets Information provided by Entec |
|||
Melt Flow | 7.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
7.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Diamond Polymers NPP25-0616 Black Impact Modified Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 7.0 g/10 min | 7.0 g/10 min | ASTM D1238 |
Aclo Accutech Polypropylene Homopolymer HP0334C20L Calcium Reinforced |
|||
Melt Flow | 7.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
7.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D-1238 |
Bhansali Engineering Abstron SE-32 ABS Sheet Extrusion Grade Super high and Very High Impact Sheeting grades for Automobile & Luggage ApplicationsInformation provided by Bhansali |
|||
Melt Flow | 7.0 - 10 g/10 min @Load 12.5 kg |
7.0 - 10 g/10 min @Load 27.6 lb |
|
Solvay Specialty Polymers Hylar® MP20 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Melt Flow | 7.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
7.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Unipetrol PP MONSTEN® GB 107 Polypropylene Homopolymer Made for injection molding. Basic stabilization. Homopolymer.Information provided by Unipetrol RPA |
|||
Melt Flow | 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 953A PC Clear, tints and opaque colors, high viscosity, flame retardant with exceptional surface. UV-stabilized. |
|||
Melt Flow | 7.0 g/10 min | 7.0 g/10 min | ASTM D1238 |
Tipco Tipcolene® HR 7222 - 25% Talc/Mineral Reinforced, Impact Modified Polypropylene Copolymer Compound 25% Mineral Reinforced, Impact Modified PP Copolymer BlendApplications: Automotive InteriorsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |