Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 6.50 g/10 min | 6.50 g/10 min | Average value: 6.50 g/10 min Grade Count:3 |
Overview of materials for Polysulfone, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl.. |
|||
Melt Flow | 6.50 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.50 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |