Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 500 g/10 min | 500 g/10 min | modified; ASTM D1238, ISO 1133 |
DuPont Elvax® 4310 Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 4310 is an ethylene-vinyl acetate / acid terpolymer resin for use in industrial applications.Applications:Elvax® 4310 resins can be used for the following applications: adhesives, .. |
|||
Melt Flow | 500 g/10 min | 500 g/10 min | Exxon Method |
ExxonMobil Escorene® LD-737 EVA Copolymer for Specialty Applications
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 19.5% vinyl acetate copolymer.Applications: Compound viscosity modifier; High flow applications. |
|||
Melt Flow | 500 g/10 min @Load 5.00 kg, Temperature 316 °C |
500 g/10 min @Load 11.0 lb, Temperature 600 °F |
ASTM D1283 |
Chevron Phillips Ryton® PR27 Polyphenylene Sulfide Resin
(discontinued **) Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R.. |
|||
Melt Flow | 500 g/10 min @Load 2.16 kg, Temperature 190 °C |
500 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont Elvax® 410 Ethylene Vinyl Acetate DuPont™ Elvax® 410 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications:Elvax® 410 resins can be used for the following applications: adhesives, sealants.. |
|||
Melt Flow | 500 g/10 min @Load 2.16 kg, Temperature 190 °C |
500 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escorene® UL 7510 Adhesive Application Resin Escorene Ultra UL 7510 is a very high flow, 18.7% vinyl acetate copolymer that has very good compatibility with hydrocarbon tackifiers and most waxes. It is suitable for making hot melt adhesives, s.. |
|||
Melt Flow | 500 g/10 min @Load 2.16 kg, Temperature 190 °C |
500 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escorene™ UL 7511 Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra UL 7511 is a very high flow, 18.5% VA copolymer that has very good compatibility with hydrocarbon tackifiers and most waxes. It is suitable for making hot melt ad.. |