Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 49.3 g/10 min @Load 5.00 kg, Temperature 275 °C |
49.3 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
BASF Ultramid® A3EG7 35% Glass Filled PA66 (Conditioned) Ultramid A3EG6 is a 35% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
Melt Flow | 49.3 g/10 min @Load 5.00 kg, Temperature 275 °C |
49.3 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
BASF Ultramid® A3EG7 35% Glass Filled PA66 (Dry) Ultramid A3EG6 is a 35% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |