Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 48 g/10 min @Load 2.16 kg, Temperature 230 °C |
48 g/10 min @Load 4.76 lb, Temperature 446 °F |
Procedure A Condition L; ASTM D1238 |
Network Polymers NPP 25-5001 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Melt Flow | 48 g/10 min @Pressure 0.655 MPa |
48 g/10 min @Pressure 95.0 psi |
Severs Efflux; Geon® ALTC 23 (with provided formulation); Internal Method |
PolyOne Geon™ 130 Series 138 Polyvinyl Chloride Copolymer (PVC Copolymer) Geon® 138 is a vinyl ester copolymer dispersion resin, exhibiting fast fusion at low processing temperatures, resulting in energy savings and the ability to work with heat sensitive substrates. The.. |
|||
Melt Flow | 48 g/10 min @Load 10.0 kg, Temperature 220 °C |
48 g/10 min @Load 22.0 lb, Temperature 428 °F |
|
Ineos ABS NOVODUR® L3FR ABS, Injection Grade
(discontinued **) Injection molding grade, flame retardant, very easy flow. Contains no polyhalogenated diphenyls or diphenyl ethers.Applications: Television and computer housings.Information provided by the manufact.. |
|||
Melt Flow | 48 g/10 min @Load 10.0 kg, Temperature 220 °C |
48 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical HI153 ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Melt Flow | 48 g/10 min @Load 5.00 kg, Temperature 260 °C |
48 g/10 min @Load 11.0 lb, Temperature 500 °F |
Calculated from MVR using melt density; ISO 1133 |
Lanxess Pocan® B 7425 000000 PBT, 20% Glass Spheres PBT, 20% glass spheres, injection molding, low tendency to warp, improved surface finish |
|||
Melt Flow | 48 g/10 min @Load 10.0 kg, Temperature 220 °C |
48 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical AF308 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
Melt Flow | 48 g/10 min @Load 10.0 kg, Temperature 220 °C |
48 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® NE-1010 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 48 g/10 min @Load 10.0 kg, Temperature 220 °C |
48 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® NE-1010 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 48 g/10 min @Load 2.16 kg, Temperature 250 °C |
48 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Samyang Tribit® 1550GN30 PBT Alloy, Reinforced Flame Retardancy Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1550GN30 is a reinforced, flame retardant (.. |
|||
Melt Flow | 48 g/10 min @Load 2.16 kg, Temperature 250 °C |
48 g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
DuPont Performance Polymers Crastin® 6131 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Low Viscosity Polybutylene Terephthalate Crastin 6131 NC010 is an unreinforced low viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by.. |
|||
Melt Flow | 48 g/10 min | 48 g/10 min | ISO 1133 |
Domo 2348TC Polypropylene Copolymer Information provided by Domo. |
|||
Melt Flow | 48 g/10 min | 48 g/10 min | ISO 1133 |
Domo 2600TC Polypropylene Copolymer Information provided by Domo. |
|||
Melt Flow | 48 g/10 min @Load 2.16 kg, Temperature 190 °C |
48 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Azoty Tarnow™ TARNOFORM 700 POM Easy flowing grade for injection molding of thin-walled parts or in case of long flow path.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Melt Flow | 48 g/10 min @Load 10.0 kg, Temperature 220 °C |
48 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D-1238 |
Bhansali Engineering Abstron SHF-50+M ABS Injection Molding Grade High Flow High Gloss, Fancy ApplicationsInformation provided by Bhansali |
|||
Melt Flow | 48 g/10 min @Load 2.16 kg, Temperature 190 °C |
48 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem IF33 LLDPE Injection Molding Polyethylene Copolymer IF33 is a linear low-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers high fluidity, good flexibility, .. |
|||
Melt Flow | 48 g/10 min @Load 2.16 kg, Temperature 190 °C |
48 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem IN34 LLDPE Injection Molding Polyethylene Copolymer IN34 is a linear low-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers high fluidity, excellent flexibil.. |
|||
Melt Flow | 48 g/10 min @Load 10.0 kg, Temperature 220 °C |
48 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D-1238 |
Bhansali Engineering Abstron SHF-50+M ABS Injection Molding Grade High Flow High Gloss, Fancy ApplicationsInformation provided by Bhansali |
|||
Melt Flow | 48 g/10 min @Load 2.16 kg, Temperature 190 °C |
48 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Chevron Phillips LX8124 HDPE Injection Molding Resin
(discontinued **) Resin Type: linear copolymer; ASTM D4976 Classification: PE 231, A 52600Characteristics: excellent flow, moderate impact strength, good stiffness, moderate ESCR, excellent shrinkage resistanceApplic.. |