Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 45 g/10 min @Load 2.16 kg, Temperature 230 °C |
45 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
SABIC PP 412MK49 Polypropylene Impact Copolymer for Injection Molding Product Description: PP 412MK49 is specially developed for producing injection molded articles. This grade contains an antistatic & nucleating agents. It has medium flow properties, good impact r.. |
|||
Melt Flow | 45 g/10 min | 45 g/10 min | I<sub>21</sub>; ASTM D238 |
Petromont 8001 High Density Polyethylene Resin Pétromont HDPE 8001 is a high density, homopolymer polyethylene resin produced using the UNIPOL® Process. This high strength resin is intended for extrusion on cast line, where excellent processab.. |
|||
Melt Flow | 45 g/10 min @Load 2.16 kg, Temperature 230 °C |
45 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
SABIC PP 6711K Polypropylene Copolymer for Injection Molding Product Description: PP 6711K is a controlled rheology grade with narrow molecular weight distribution intended specifically for producing injection molded articles with high clarity, good flow pro.. |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 190 °C |
45 g/10 min @Load 11.0 lb, Temperature 374 °F |
|
Total Finaprene® 411x Styrene-Butadiene TPE Copolymer Compounded to 59 Shore A
(discontinued **) Styrene-Butadiene CopolymerDescription: Finaprene® 411x is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its high molecular weight, Finaprene® 411x provides e.. |
|||
Melt Flow | 45 g/10 min | 45 g/10 min | melt index; ASTM D1238 |
Asahi Kasei Tenac®-C 8554 Acetal Copolymer, High Flow
(discontinued **) Superhigh-flow grade, with properties necessary for VCR reels.Applications: VCR reels.This product is not a part of the standard product line dated 2003. |
|||
Melt Flow | 45 g/10 min | 45 g/10 min | ASTM D1238 |
LyondellBasell Alathon® ETP H4745 High Density Polyethylene ApplicationsALATHON H 4745 is a new, multi-purpose, high-flow resin featuring enhanced cold temperature impact performance, enhanced processability and thermal stability for fast cycling and exhibit.. |
|||
Melt Flow | 45 g/10 min @Load 10.0 kg, Temperature 380 °C |
45 g/10 min @Load 22.0 lb, Temperature 716 °F |
|
Lehmann & Voss LUVOCOM® 1502-7866/GN4 PPSU, unreinforced Applications: Automotive industry, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceHigh chemical res.. |
|||
Melt Flow | 45 g/10 min | 45 g/10 min | ASTM D1238 |
Hyosung Topilene J842 PP J842 Injection Impact CopolymerApplications: Very large articles:Washing M/C partsIndustrial applianceCharacteristics:High flowabilityHigh stiffnessInformation provided by Hyosung Corporation |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 260 °C |
45 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
Kingfa LONOY 1200 PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine.. |
|||
Melt Flow | 45 g/10 min | 45 g/10 min | ASTM D1238 |
KEP Kepital® F40 Standard Grade/Low Viscosity Acetal Homopolymer injection molding: electrical parts, machine/mechanical parts, industrial parts, automotive applications, electronic data processing.Kepital® is a registered trademark of Korea Engineering Plasti.. |
|||
Melt Flow | 45 g/10 min @Load 2.16 kg, Temperature 250 °C |
45 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
LG Chemical Lupox® GP1000H PBT Description: Injection Molding, PBT, High Flow, High ImpactApplication: Automotive (Connector)CAS No. 155123-66-3 and 24968-12-5Information provided by LG Chemical |
|||
Melt Flow | 45 g/10 min @Load 2.16 kg, Temperature 230 °C |
45 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
IRPC Polimaxx Polene 2340TC Polypropylene Block Copolymer CHARACTERISTICS: EXCELLENT FLOWABILITY, HIGH STIFFNESS, MEDIUM IMPACT, HEAT STABILITYAPPLICATIONS: INJECTION MOLDING FOR THIN WALL CONTAINERS : DRINKING CUPS, NOODLE CUPS |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 200 °C |
45 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Kraton® D1162 P (SIS) Linear Triblock Copolymer Description: Kraton D1162 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 43%. It is supplied from North America in the physical form identified: .. |
|||
Melt Flow | 45 g/10 min @Load 10.0 kg, Temperature 380 °C |
45 g/10 min @Load 22.0 lb, Temperature 716 °F |
|
Lehmann & Voss LUVOCOM® 1502-7865/BK2 PPSU, unreinforced Applications: Automotive industry, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceHigh chemical res.. |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 266 °C |
45 g/10 min @Load 11.0 lb, Temperature 511 °F |
ASTM D 1238 |
SABIC Innovative Plastics Valox® CS860 PBT+PET (Asia Pacific) 30% glass reinforced PBT+PET blend. Color stable, FR. Housewares, appliances; iron skirt, oven trim/panels.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 265 °C |
45 g/10 min @Load 11.0 lb, Temperature 509 °F |
ASTM D1238 |
Samyang Tripet® 2550GN30 Polyethylene Terephthalate, 30% Glass Fiber Reinforced, Flame Retardant TRIPET® has excellent heat resistance, good surface, chemical resistance and high electrical performance.Applications:Coil BobbinConnectorMotor HousingLamp HousingRelay BaseIron bodyAll informati.. |
|||
Melt Flow | 45 g/10 min @Load 2.16 kg, Temperature 230 °C |
45 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis BH345MO Polypropylene Copolymer BH345MO is a heterophasic copolymer. This grade is characterized by optimum combination of very high stiffness, good flow properties and good impact strength. and is designed for high speed injectio.. |
|||
Melt Flow | 45 g/10 min @Load 2.16 kg, Temperature 230 °C |
45 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
ExxonMobil SFT325 Polypropylene Homopolymer Product Description: A premium homopolymer resin designed to provide soft cotton-like feel and robust spinning to nonwovens applications where fluid barrier is desired.Availability: North America F.. |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 275 °C |
45 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
Azoty Tarnow™ Tarnamid® T-27 MX6 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grade, reinforced with 10% hybrid mineral-glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning, good su.. |
|||
Melt Flow | 45 g/10 min @Load 2.16 kg, Temperature 190 °C |
45 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Beijing Ranger Chem BLUESTAR® BS450 Acetal Copolymer Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Melt Flow | 45 g/10 min @Load 10.0 kg, Temperature 220 °C |
45 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D-1238 |
Bhansali Engineering Abstron IM-17 A EP ABS Electro Plating Applications Electroplating & Hot Stamping GradesInformation provided by Bhansali |
|||
Melt Flow | 45 g/10 min @Load 2.16 kg, Temperature 230 °C |
45 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238L |
Braskem CP 144 Coating Polypropylene Information provided by Braskem |
|||
Melt Flow | 45 g/10 min @Load 2.16 kg, Temperature 230 °C |
45 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238L |
Braskem CP 145 Injection Molding Polypropylene Applications: Household; thin-walled parts; easy mould filling. Information provided by Braskem |
|||
Melt Flow | 45 g/10 min @Load 2.16 kg, Temperature 230 °C |
45 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238L |
Braskem H 117 Injection Molding Polypropylene Description: H 117 is a ultra-high melt flow rate homopolymer. This product is suitable to high productivity on thin-walled parts. H 117 features an excellent stiffness, thermal resistance, low warp.. |
|||
Melt Flow | 45 g/10 min @Load 2.16 kg, Temperature 190 °C |
45 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem IJ33D LLDPE Injection Molding Polyethylene Copolymer IJ33D is a linear low-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers high fluidity, excellent flexibi.. |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 275 °C |
45 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
Azoty Tarnow™ Tarnamid® T-27 MF30 Polyamide 6 - Mineral Reinforced 30% Mineral filled, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High mechani.. |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 275 °C |
45 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
Azoty Tarnow™ Tarnamid® T-29 MCS Polyamide 6 - Colored Colored medium-high viscosity grade for injection molding.Tarnamid® has the following main properties:High mechanical strength, rigidity and hardnessHigh impact strengthHigh vibration damping capac.. |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 316 °C |
45 g/10 min @Load 11.0 lb, Temperature 601 °F |
Procedure B; ASTM D1283 |
Chevron Phillips Ryton® PR09 Polyphenylene Sulfide Resin
(discontinued **) Off White Polyphenylene Sulfide ResinRyton® PR09 is a finely divided powder. Ryton® PPS exhibits excellent thermal stability and chemical resistance and is suitable for a variety of applications .. |
|||
Melt Flow | 45 g/10 min | 45 g/10 min | (MVR) [cm³/10min]; ISO 1133 |
EMS-Grivory Grivory® F 50 nat 6368 PA6 Product description: Grilon F 50 natural 6368 is a modified, very high viscous Polyamide 6 for extrusion processes: Very high melt strengthGood chemical resistanceGood gas-barrierGood mechanical pro.. |
|||
Melt Flow | 45 g/10 min @Load 10.0 kg, Temperature 220 °C |
45 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D-1238 |
Bhansali Engineering Abstron IM-17A ABS Injection Molding Grade Medium Impact, High Gloss, High FlowInformation provided by Bhansali |