Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 42.9 g/10 min @Load 2.16 kg, Temperature 250 °C |
42.9 g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
BASF Ultradur® B 4560 PBT Description: Medium viscosity injection molding grade for industrial parts in the automotive field, for example for head lamp bezel. Suitable for direct metalizing.Information provided by BASF |