Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 40 g/10 min @Load 3.80 kg, Temperature 230 °C |
40 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite Optix® CA - 42 FDA General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Melt Flow | 40 g/10 min @Load 2.16 kg, Temperature 230 °C |
40 g/10 min @Load 4.76 lb, Temperature 446 °F |
STN EN ISO 1133 |
Plastcom SLOVASTER® B BT Polyethylene Terephthalate FeaturesPBT basic type for injection moulding. Melt is characterized by outstanding fluidity, which enables injection moulding of complicated and divided products also on multiple moulds. Anisotro.. |
|||
Melt Flow | 40 g/10 min @Load 2.16 kg, Temperature 190 °C |
40 g/10 min @Load 4.76 lb, Temperature 374 °F |
Procedure A Condition E; ASTM D1238 |
Network Polymers NPP 50-4052 Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc. |
|||
Melt Flow | 40 - 45 g/10 min @Load 2.16 kg, Temperature 230 °C |
40 - 45 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238/L |
NIZHNEKAMSKNEFTEKHIM PP 4341S Propylene and Ethylene Copolymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Melt Flow | 40 g/10 min @Load 1.20 kg, Temperature 300 °C |
40 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer (Asia Pacific) 40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized, available in transparent colors only |
|||
Melt Flow | 40 g/10 min @Load 0.325 kg, Temperature 270 °C |
40 g/10 min @Load 0.716 lb, Temperature 518 °F |
|
Plastcom SLOVASTER® B FRN 3 LS PBT, flame retarder, light stable FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of.. |
|||
Melt Flow | 40 g/10 min @Load 0.325 kg, Temperature 270 °C |
40 g/10 min @Load 0.716 lb, Temperature 518 °F |
|
Plastcom SLOVASTER® B FRN 3 PBT, flame retarder FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of.. |
|||
Melt Flow | 40 g/10 min @Load 2.16 kg, Temperature 190 °C |
40 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Eastman 18DOA Polyethylene
(discontinued **) Polyethylene 18DOA is a low density formulation suggested for the production of closures where a high melt index material is needed to meet shrinkage requirements and fast molding cycles. It molds .. |
|||
Melt Flow | 40 g/10 min @Load 1.20 kg, Temperature 300 °C |
40 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer (Europe-Africa-Middle East) 40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized, available in transparent colors only |
|||
Melt Flow | 40 g/10 min @Load 2.16 kg, Temperature 190 °C |
40 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® LM-4021-L LDPE Injection Molding Resin Features: Medium flow LDPE with a good balance of toughness, softness, dimensional stability and processability Applications: Injection molding of caps, closures and other specialty productsInformat.. |
|||
Melt Flow | 40 g/10 min @Load 10.0 kg, Temperature 380 °C |
40 g/10 min @Load 22.0 lb, Temperature 716 °F |
|
Lehmann & Voss LUVOCOM® 1105-7678 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Melt Flow | 40 g/10 min @Load 5.00 kg, Temperature 260 °C |
40 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
Kingfa LONOY 1300 PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine.. |
|||
Melt Flow | 40 g/10 min @Load 10.0 kg, Temperature 300 °C |
40 g/10 min @Load 22.0 lb, Temperature 572 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Durethan® DP BC 500 H2.0 901510 Nylon 6 PA 6, extrusion and blow molding grade, non-reinforced, elastomer-modified, high viscosity, good heat-ageing resistance |
|||
Melt Flow | 40 - 60 g/10 min @Load 2.16 kg, Temperature 150 °C |
40 - 60 g/10 min @Load 4.76 lb, Temperature 302 °F |
|
Taiwan Sheen Soon Sheenthane® AH-706L TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for hotmelt adhesiveHydrolysis resistance gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. U.. |
|||
Melt Flow | 40 g/10 min @Load 5.00 kg, Temperature 266 °C |
40 g/10 min @Load 11.0 lb, Temperature 511 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® 4022 PBT (Europe-Africa-Middle East) VALOX 4022 is a 20% high strength glass fibre reinforced PBT injection moulding resin, with improved mechanical properties. Applications : Spotlights, appliance housings and handles. |
|||
Melt Flow | 40 g/10 min @Load 5.00 kg, Temperature 250 °C |
40 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® IQ4860HR PBT Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |
|||
Melt Flow | 40 g/10 min | 40 g/10 min | ASTM D1238 |
Samyang Trilen® 9550AC Polypropylene, General Purpose Mechanical strength and thermal resistance are excellent.9550AC is a general purpose grade.Applications: ConnectorsInformation provided by Samyang. |
|||
Melt Flow | 40 g/10 min @Load 10.00 kg |
40 g/10 min @Load 22.05 lb |
ASTM D1238 |
Sumitomo Chemical ESPOLEX® 3675 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Melt Flow | 40 g/10 min @Load 5.00 kg, Temperature 224 °C |
40 g/10 min @Load 11.0 lb, Temperature 435 °F |
ASTM D1238 |
Lubrizol Pellethane® 2363-65D Thermoplastic Polyurethane Elastomer Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Melt Flow | 40 g/10 min @Load 2.16 kg, Temperature 230 °C |
40 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Lubrizol Stat-Rite® X-5111 Static Control Polypropylene Stat-Rite® X-5111 is a static dissipative Polypropylene alloy. Stat-Rite® X-5111 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ES.. |
|||
Melt Flow | 40 g/10 min @Load 2.16 kg, Temperature 190 °C |
40 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Westlake EM184AA Low Density Polyethylene WESTLAKE low-density polyethylene EM184 is a low density injection-molding formulation suggested for the production of closures where a high melt index is needed to meet shrinkage requirements and f.. |
|||
Melt Flow | 40 g/10 min @Load 10.0 kg, Temperature 220 °C |
40 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D 1238 |
Cossa Polimeri ESTADIENE 1640 AS Acrylonitrile Butadiene Styrene General purpose ABSGood impact resistance, high melt flow rate, high gloss, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Melt Flow | 40 g/10 min @Load 2.16 kg, Temperature 190 °C |
40 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LD 637.LI Molding, Extrusion and Compounding Resin Product Description: LD 637.LI is a high melt index LDPE homopolymer intended for injection molding or compounding applications requiring high flow. It is ideal for tamper-evident, tear-to-open clos.. |
|||
Melt Flow | 40 g/10 min @Load 2.16 kg |
40 g/10 min @Load 4.76 lb |
Melt flow ratio I10/I2 is 8.5. |
Dow DOWLEX™ IP-40 High Density Polyethylene DOWLEX® IP-40 resin is an improved processing high density resin designed to offer excellent processability and impact resistance required for food container applications. This resin is designed by.. |
|||
Melt Flow | 40 g/10 min @Load 2.16 kg |
40 g/10 min @Load 4.76 lb |
Melt flow ratio I10/I2 is 8.5. |
Dow DOWLEX™ IP-41 High Density Polyethylene DOWLEX® IP-41 resin is an improved processing high density polyethylene resin designed to offer excellent processability and rigidity required for food containers, overcaps, and other general purpo.. |
|||
Melt Flow | 40 g/10 min @Load 2.16 kg, Temperature 230 °C |
40 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238L |
Braskem RP 141 Injection Molding Polypropylene Description: RP 141 is a high melt flow rate random copolymer designed for injection molding. This product offers outstanding transparency, very good stiffness/impact strength balance and excellent .. |
|||
Melt Flow | 40 g/10 min @Load 5.00 kg, Temperature 235 °C |
40 g/10 min @Load 11.0 lb, Temperature 455 °F |
3 min.; ASTM D1238 |
ALM PA 250 Nylon 12 SLS Prototyping Polymer Highly Recyclable Nylon 12 Laser Sintering Material.Engineered for excellent mechanical properties, part definition and surface finish. Stabilized against thermal degradation resulting in little or.. |
|||
Melt Flow | 40 g/10 min @Load 5.00 kg, Temperature 275 °C |
40 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
BASF Ultramid® A34 01 PA66 (Dry) Ultramid A34 01 is an intermediate visosity, PA66 grade. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation "X Polyamide", 1.6.1998 or .. |
|||
Melt Flow | 40 g/10 min @Load 2.16 kg, Temperature 230 °C |
40 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM-D1238 |
Braskem RP 145 RACO Random Polypropylene Copolymer RP 145 is a high melt flow rate random copolymer designed for use in thin-walled injection molding parts. This product offers good transparency, very good stiffness/impact strength balance, excellen.. |