Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 4.0 g/10 min @Load 0.325 kg, Temperature 275 °C |
4.0 g/10 min @Load 0.716 lb, Temperature 527 °F |
STN EN ISO 1133 |
Plastcom PLASTAMID® 6 BT B 27 PA6 Basic type PA 6 for compounding, for general use. Grade can contain PA 66 up to 5% and TiO2 content up to 0.25 %. Use: automotive, engineering, electrical and consumer-goods industryInformation Prov.. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
STN EN ISO 1133 |
Plastcom SLOVAMID® 6 GF 30 FRG 2 PA6 reinforced with glass fiber, flame retarded PA 6 for injection molding, reinforced with 30 % glass fiber, flame retarded with halogen free flame retardant. Main features: flammability in accordance with UL 94 5 at 3.2 mm. Application for the .. |
|||
Melt Flow | 4.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
4.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® EX58F ABS (Europe-Africa-Middle East) High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant. |
|||
Melt Flow | 4.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
cm³/10 min |
Polimeri Europa EDISTIR RK0414 High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,088-03-04-23 UL94 V-0, polybromobiphenylether (PBBE) free, flame retarded high impact polystyrene with excellent light .. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 330 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 626 °F |
ASTM D1238 |
Covestro Apec® DP9-9371 High-Heat Polycarbonate, General Purpose
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
M. Holland Company CP200 Polypropylene Impact Copolymer Impact copolymerMedium impact resistanceLow temperature impact resistanceApplications: Appliance componentsConsumer ApplicationsHousehold goodsInformation provided by M. Holland |
|||
Melt Flow | 4.0 g/10 min | 4.0 g/10 min | ASTM D1238 |
Hyosung Topilene J440 PP J440 Injection Impact CopolymerApplications:CrateContainerBatter caseCharacteristics:High ImpactInformation provided by Hyosung Corporation |
|||
Melt Flow | 4.0 g/10 min | 4.0 g/10 min | ASTM D1238 |
Hyosung Topilene R401 PP R401 Extrusion Random CopolymerApplications:Extrusion blow moldingStationary sheetCharacteristics:TransparencyStiffnessInformation provided by Hyosung Corporation |
|||
Melt Flow | 4.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
4.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical RS657L ABS, Chemical Resistance to Cyclopentane, Low Specific Gravity Feature: Extrusion Molding, Chemical Resistance to Cyclopentane, Thin ThicknessApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Ineos T50-400 HDPE T50-400 is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and end-use p.. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
IRPC Polimaxx Polene 1111NX GA6 Polypropylene Compound CHARACTERISTICS: POLYPROPYLENE HOMOPOLYMER WITH 30% GLASS FIBRE REINFORCED HIGH IMPACT STRENGTH, HIGH MECHANICAL STRENGTH, HIGH STIFFNESS LOW SHRINKAGEAPPLICATIONS: INJECTION MOLDING FOR AUTOPARTS, .. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Multibase Multi-Flex® A 9702 MR TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg |
4.0 g/10 min @Load 4.76 lb |
ISO 1133 |
SIDPEC EGYPTENE® HD 3840 EA MDPE Wire and Cable Grade Applications:Suitable for the production of silane cross-linkable compoundsLow voltage power cable insulationInjection molded technical parts and closureInformation provided by Interchim s.r.l., off.. |
|||
Melt Flow | 4.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
4.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM Data |
Styron CALIBRE™ 300 4 Polycarbonate, General Purpose CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren.. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
SCG Chemicals EL-Leneâ„¢ M3204 Butene (C4) Rotational Molding Resin Natural base resin available in pellet / powder formKey Characteristics:Low warpageGood processingGood impact resistanceTypical Applications:Low temperature service parts, straight-wall or flat-surf.. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Borealis Borecene™ RM7402 Linear Polyethylene for Rotational Molding Borecene RM7402 is a third generation linear medium density natural polyethylene for rotational molding. The narrow molecular weight distribution imparted through metallocene catalyst technology pro.. |
|||
Melt Flow | 4.0 - 9.0 g/10 min | 4.0 - 9.0 g/10 min | 190/2.16; May be specified; ASTM D1238 |
Plastics Group Polifil® RP-HDPE High Density Polyethylene Polifil® RP-High Density Polyethylene is a moderate stiffness material that retains excellent toughness. HDPE exhibits outstanding chemical resistance and environmental stress crack resistance. Inj.. |
|||
Melt Flow | 4.0 - 8.0 g/10 min | 4.0 - 8.0 g/10 min | ASTM D1238 |
A. Schulman POLYFLAM™ RCP 770C/CW DescriptionPolyflam® RCP 770C/CW is a flame-retardant concentrate based in low-density polyethylene that features excellent dispersion and processing stability up to 550°F.ApplicationRCP 770 C/CW.. |
|||
Melt Flow | 4.0 g/10 min | 4.0 g/10 min | ASTM D1238 |
Dow ATTANE™ 4404G, 2mil Ultra Low Density Ethylene/Octene Copolymer ATTANE™ 4201G provides improved cling in one-sided cling applications, and has improved toughness and optical properties. It complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a.Information provided by.. |
|||
Melt Flow | 4.0 g/10 min | 4.0 g/10 min | ASTM D1238 |
Aclo Accutech Polypropylene Homopolymer HP0334G30CL Glass Reinforced Coupled |
|||
Melt Flow | 4.0 - 37 g/10 min | 4.0 - 37 g/10 min | ASTM D1238 |
Buckeye Polymers BP FLEX A6410 BLK Thermoplastic Elastomer SEBS Product Information: BP Flex Thermoplastic Elastomers are based on SEBS polymers (Styrene-ethylene/butylene-styrene) providing increased oxidation and weather resistance, higher service temperatures.. |
|||
Melt Flow | 4.0 g/10 min | 4.0 g/10 min | ASTM D1238 |
Asahi Kasei Thermylene® P6-20FG-0693 20% Glass Fiber Reinforced, Heat and UV Stabilized Information provided by Asahi Thermofil |
|||
Melt Flow | 4.0 - 17.5 g/10 min @Load 3.80 kg, Temperature 232 °C |
4.0 - 17.5 g/10 min @Load 8.38 lb, Temperature 450 °F |
ASTM D1238 |
Arkema Group KYNAR FLEX® 2950-05 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toug.. |
|||
Melt Flow | 4.0 g/10 min | 4.0 g/10 min | ASTM D1238 |
Asahi Kasei Thermylene® P7-40FG-0874 40% Glass Fiber Reinforced, Impact Modified Information provided by Asahi Thermofil |
|||
Melt Flow | 4.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
|
BASF Polystyrol® 2710 Impact Grade Polystyrene (Europe) Special high-impact grade for refrigerators and the packaging sector. Particularly resistant to stress cracking.Data was collected by ISO methods and provided by BASF. |
|||
Melt Flow | 4.0 - 12 g/10 min | 4.0 - 12 g/10 min | 200/5; May be specified; ASTM D1238 |
Plastics Group Polifil® RP-HIPS High Impact Polystyrene Polifil® RP-High Impact Polystyrene (HIPS) combines the good stiffness properties of polystyrene, with enhanced impact properties gained by the addition of impact modifiers, usually butadiene rubbe.. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products G20P100-406 20% Glass Fiber Reinforced Polypropylene, UV Stabilized, (Ford ZUEA) Midnight Black Applications: Arm rest insertVacuum canisterStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |