Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 39.26 g/10 min @Load 5.00 kg, Temperature 380 °C |
39.26 g/10 min @Load 11.0 lb, Temperature 716 °F |
|
Lehmann & Voss LUVOCOM® 1105-7594/BL PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |