Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 27 g/10 min | 27 g/10 min | Condition 230/2-8; ASTM D1238 |
Plaskolite Optix® CA-41 General Purpose Acrylic Resin Injection Molding Grade Pellets only. Lowest Heat Resistance and maximum flow. |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 190 °C |
27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Eraclene® MS 80 U High Density Polyethylene - Injection Molding Eraclene MS 80 U is a gas phase high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application. This grade has a narrow molecular weight distribution and a hig.. |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 230 °C |
27 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Noble Polymers Regis™ 125098 Thermoplastic Olefin (TPO) Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi.. |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 190 °C |
27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Eraclene® MS 80 High Density Polyethylene - Injection Molding Eraclene MS 80 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MS 80 shows a good balance between processability and mechanical pro.. |
|||
Melt Flow | 27 g/10 min | 27 g/10 min | |
Custom Resins Duratel™ MF27 Acetal Copolymer
(discontinued **) Description: Duratel™ MF27 is a 27 melt flow, general purpose acetal copolymer. Information provided by Custom Resins. |
|||
Melt Flow | 27 g/10 min @Load 5.00 kg, Temperature 400 °C |
27 g/10 min @Load 11.0 lb, Temperature 752 °F |
ASTM D1238 |
Solvay Specialty Polymers Supradel® HTS-2401 High Temperature Sulfone Resin
(discontinued **) Supradel HTS-2401 is a high-temperature high-performance amorphous sulfone polymer designed for use in reinforced high temperature thermoplastic formulations. With its glass transition temperature o.. |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 230 °C |
27 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LyondellBasell Pro-fax PF531 Polypropylene Homopolymer, Radiation Resistant Primary Processing Method: Injection MoldingKey Features: high melt flow, radiation-resistant polypropylene homopolymer resin, excellent retention of physical properties and color after radiation st.. |
|||
Melt Flow | 27 g/10 min @Load 5.00 kg, Temperature 300 °C |
27 g/10 min @Load 11.0 lb, Temperature 572 °F |
|
Lehmann & Voss LUVOCOM® 50-1396 Polycarbonate, with carbon fiber, glass fiber and PTFE, electrically conducting Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Melt Flow | 27 - 31 g/10 min @Load 5.00 kg, Temperature 230 °C |
27 - 31 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
FKuR Kunststoff Biograde® C 6530 Biodegradable Plastic Compound BIOGRADE® are easy to process blends based on cellulose. BIOGRADE® is composed mainly of natural resources. Based on cellulose, a product of the paper industry BIOGRADE® has been especial.. |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 190 °C |
27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical LUCEL N127LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
Melt Flow | 27 g/10 min | 27 g/10 min | ASTM D1238 |
Kolon Kocetal® K700 General Purpose Grade Acetal Copolymer Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Melt Flow | 27 g/10 min | 27 g/10 min | ASTM D1238 |
Kolon KOCETAL® K700BK Colored Grade Acetal Resin Colored, low viscosity grade.Applications: Thin products, improved appearance.Information provided by API-Kolon. |
|||
Melt Flow | 27 g/10 min | 27 g/10 min | ASTM D1238 |
Kolon KOCETAL® VT702 Anti-Static Grade Acetal Resin Improved antistatic effects. Applications: Products for avoiding electric contamination. Information provided by API-Kolon. |
|||
Melt Flow | 27 g/10 min @Load 10.0 kg, Temperature 220 °C |
27 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Ineos ABS Lustran® ABS 450 Injection Molding Grade Lustran® ABS 450 has medium impact strength, high flow, and is injection molding grade. |
|||
Melt Flow | 27 g/10 min | 27 g/10 min | |
Intercontinental Polymers 554 PBT Polymer Type - Elastomer Polyester Pellets Applications: Engineering Resin - ModifiedInformation provided by Intercontinental Polymers. |
|||
Melt Flow | 27 g/10 min @Load 5.00 kg, Temperature 250 °C |
27 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® ENH4550 PBT 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Melt Flow | 27 g/10 min @Load 10.0 kg, Temperature 250 °C |
27 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® NH-1023P PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 27 g/10 min @Load 10.0 kg, Temperature 220 °C |
27 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® NH-1101 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 230 °C |
27 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Styron INSPIREâ„¢ T710-25 ES PolyPropylene Resin DA Thermoplastic Polyolefin Dow T710-25 ES Polypropylene Resin DAâ„¢ is a high impact TPO with enhanced flow, scratch and mar, and surface aesthetics for excellent molded-in-color appearance for automotive interior applicat.. |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 300 °C |
27 g/10 min @Load 4.76 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics LNP Thermocomp ZM3242 PPE+PS (Asia Pacific) Modified PPO* 30% mineral filled products, Non Halogenated Flame Retardant V-1 products.Supper low warpage series, HDT 110degCThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 230 °C |
27 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
SCG Chemicals EL-Proâ„¢ P740J Polypropylene Injection Molding Key Characteristics:Good flowabilityGood processabilityHigh stiffnessRecommended Applications:Automotive, motorcycle and electrical appliance parts that require good flowability such as automotive t.. |
|||
Melt Flow | 27 g/10 min @Load 1.20 kg, Temperature 300 °C |
27 g/10 min @Load 2.65 lb, Temperature 572 °F |
|
Covestro Makrolon® DP 1-1456 Polycarbonate, Impact Grade Impact modified injection molding grade, extremely easy flow and easy mold release, for thin walled applications with long flow lengths.Information provided by Bayer.As of 1 September 2015, Bayer Ma.. |
|||
Melt Flow | 27 g/10 min @Load 10.0 kg, Temperature 220 °C |
27 g/10 min @Load 22.0 lb, Temperature 428 °F |
Melt Volume Rate (ml/10 min); ISO 1133 |
Chi Mei Polylac® PA-758R ABS - Transparent Transparent, Chemical Resistant |
|||
Melt Flow | 27 g/10 min | 27 g/10 min | ASTM D1238 |
Aclo Accucomp Polyacetal (POM) ACE093L Low Viscosity |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 190 °C |
27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Azoty Tarnow™ TARNOFORM 500 POM Easy flowing grade for injection molding of thin-walled parts or in case of long flow path.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 250 °C |
27 g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
BASF Ultradur B 4300 G6 LS High Speed BK15045 30% Glass Filled PBT |
|||
Melt Flow | 27 g/10 min | 27 g/10 min | ISO 1133 |
Addiplast Addilene J 683 Polypropylene Copolymer Copper ResistantInformation provided by Addiplast. |
|||
Melt Flow | 27 g/10 min | 27 g/10 min | Condition 230/2-8; ASTM D1238 |
Plaskolite West Optix® CA-41 General Purpose Acrylic Resin Injection Molding Grade Pellets only. Lowest Heat Resistance and maximum flow. |
|||
Melt Flow | 27 g/10 min @Load 2.16 kg, Temperature 190 °C |
27 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
PTS POM-270 Acetal Copolymer Information provided by PTS LLC. |