Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 26.86 g/10 min @Load 5.00 kg, Temperature 275 °C |
26.86 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
BASF Ultramid® A3HG6 Balance 30% Glass Filled PA 66/610 (Conditioned) Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. .. |