Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 26 g/10 min @Load 3.80 kg, Temperature 230 °C |
26 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite Optix® CP - 41 UVA General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Melt Flow | 26 g/10 min @Load 3.80 kg, Temperature 230 °C |
26 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite West Optix® CA - 41 FDA General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Melt Flow | 26 g/10 min @Load 3.80 kg, Temperature 230 °C |
26 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite West Optix® CP - 41 UVA General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Melt Flow | 26 g/10 min | 26 g/10 min | ASTM D1238 |
Mytex Polymers AS88L-01 Polypropylene, Compounded, Elastomer Description: AS88L-01 is a compounded, elastomer modified polypropylene with good impact and excellent material flow properties. This product is designed for painted and mold-in-color applications .. |
|||
Melt Flow | 26 g/10 min @Load 2.16 kg, Temperature 190 °C |
26 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Flexirene® MS 20 U Linear Low Density Polyethylene Flexirene MS 20 U is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MS 20 U are characterized by optimum low tempe.. |
|||
Melt Flow | 26 g/10 min @Load 2.16 kg, Temperature 190 °C |
26 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Flexirene® MS 26 A Linear Low Density Polyethylene Flexirene MS 26 A is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MS 26 A are characterized by optimum low tempe.. |
|||
Melt Flow | 26 g/10 min @Load 2.16 kg, Temperature 260 °C |
26 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® C6840 PC+ABS (Asia Pacific) Cycoloy* C6840 resin is an injection moldable, flame retardant PC/ABS blend. It contains non-chlorinated & non-brominated flame retardant systems intended to meet governmental regulations and variou.. |
|||
Melt Flow | 26 g/10 min @Load 5.00 kg, Temperature 260 °C |
26 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS (Asia Pacific) PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Melt Flow | 26 g/10 min @Load 2.16 kg, Temperature 250 °C |
26 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
PTS PBT-101G0 PBT Resin Typical Applications: Appliance partsInformation provided by PTS LLC. |
|||
Melt Flow | 26 g/10 min @Load 1.20 kg, Temperature 300 °C |
26 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® BFL2000U PC (Asia Pacific) Lexan* BFL2000U Polycarbonat (PC) resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating. Lexan* BFL2000U is designed for hig.. |
|||
Melt Flow | 26 g/10 min | 26 g/10 min | ASTM D1238 |
Formosa Plastics Formolene® LH5326 Injection Molding HDPE
(discontinued **) CopolymerApplications: Housewares, bowls, food containers, toysFormolene LH5326 is a high density polyethylene for injection molding applications.Meets all requirements of the U.S. Food and Drug Adm.. |
|||
Melt Flow | 26 g/10 min @Load 2.16 kg, Temperature 260 °C |
26 g/10 min @Load 4.76 lb, Temperature 500 °F |
Calculated from MVR using melt density; ISO 1133 |
Lanxess Pocan® B 3225 901510 PBT, 20% Glass Fiber PBT, 20% glass fibers, injection molding |
|||
Melt Flow | 26 g/10 min @Load 2.16 kg, Temperature 230 °C |
26 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Multibase Multi-Flex® D 5308 HF Black TPO Thermoplastic Polyolefin Elastomer Forms: PelletsInformation provided by Multibase |
|||
Melt Flow | 26 g/10 min @Load 1.20 kg, Temperature 250 °C |
26 g/10 min @Load 2.65 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® IQ3001 PBT (Europe-Africa-Middle East) Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications. |
|||
Melt Flow | 26 g/10 min @Load 10.0 kg, Temperature 220 °C |
26 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® NH-1014S PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 26 g/10 min @Load 10.0 kg, Temperature 220 °C |
26 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® WR-9120 J ASA, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 26 g/10 min @Load 2.16 kg, Temperature 230 °C |
26 g/10 min @Load 4.76 lb, Temperature 446 °F |
from MVR; ISO 1033 |
Sax Polymers SAXALEN PPH319FX21 Polypropylene Homopolymer SAXALEN PPH319FX21 is a unfilled Polypropylene - Homopolymer intended for injection molding. It has flame retardant properties and suitable to produce thin-walled parts.Information provided by SAX P.. |
|||
Melt Flow | 26 g/10 min @Load 2.16 kg, Temperature 250 °C |
26 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® HX420HP PBT (Europe-Africa-Middle East) Medium Flow, 30% Glass filled, Polybutylene Terephthalate (PBT) resin. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Melt Flow | 26 g/10 min @Load 5.00 kg, Temperature 266 °C |
26 g/10 min @Load 11.0 lb, Temperature 511 °F |
ASTM D1238 |
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC (Asia Pacific) Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability. |
|||
Melt Flow | 26 g/10 min @Load 2.16 kg, Temperature 325 °C |
26 g/10 min @Load 4.76 lb, Temperature 617 °F |
DAM; cm³/10min; ISO 1133 |
DuPont Performance Polymers Zytel® HTN FR52G30BL NC010 Polyphthalamide (PPA)
(Unverified Data**) 30% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G30BL NC010 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel.. |
|||
Melt Flow | 26 g/10 min @Load 2.16 kg, Temperature 230 °C |
26 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM Data |
Dow Prevail® 3050 ABS + Polyurethane PREVAIL® 3050 thermoplastic resin offers designers and manufacturers a combination of flexibility and low temperature toughness not previously available in an engineering thermoplastic and is used .. |
|||
Melt Flow | 26 - 34 g/10 min @Load 2.16 kg, Temperature 230 °C |
26 - 34 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
AKG Polymers Vision PP PPC SK3005 Polypropylene Copolymer Compound Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin.. |
|||
Melt Flow | 26 - 34 g/10 min @Load 2.16 kg, Temperature 230 °C |
26 - 34 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
AKG Polymers Vision PP PPH BL3004 Polypropylene Homopolymer Compound Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin.. |
|||
Melt Flow | 26 g/10 min @Load 2.16 kg, Temperature 230 °C |
26 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
BASF Novolen® 1101 P Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Melt Flow | 26 g/10 min @Load 2.16 kg, Temperature 230 °C |
26 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM-D1238 |
Braskem CP 202XP HECO Polypropylene Heterophasic Copolymer CP 202XP is a high melt flow rate heterophasic copolymer designed to achieve parts with high stiffness and impact strength resistance, low warpage, and excellent surface appearance. Its applications.. |
|||
Melt Flow | 26 g/10 min @Load 10.0 kg, Temperature 220 °C |
26 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D-1238 |
Bhansali Engineering Abstron SE-22 FR Flame Retardant ABS Grade Information provided by Bhansali |
|||
Melt Flow | 26 g/10 min @Load 5.00 kg, Temperature 235 °C |
26 g/10 min @Load 11.0 lb, Temperature 455 °F |
3 min.; ASTM D1238 |
ALM PA 860 White Nylon 11 SLS Prototyping Polymer Unfilled White PA 11 that is formulated for easy processing across all LS platforms. Tightly controlled particle distribution creates a smooth surface finish and excellent feature detail. Parts prod.. |
|||
Melt Flow | 26 g/10 min @Load 2.16 kg, Temperature 260 °C |
26 g/10 min @Load 4.76 lb, Temperature 500 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Pocan® B 3225 Z 000000 PBT, 20% Glass Fiber
(discontinued **) PBT, 20% glass fibers, injection molding, impact modified |