Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 24.7 g/10 min @Load 2.16 kg, Temperature 250 °C |
24.7 g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
BASF Ultradur B 4500 PBT Ultradur B4500 is a general-purpose injection molding grade for high-precision, high-toughness, and dimensionally stable engineering parts. It conforms to FDA requirements of 21 CFR 177.1660. |
|||
Melt Flow | 24.7 g/10 min @Load 2.16 kg, Temperature 250 °C |
24.7 g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
BASF Ultradur B 4520 PBT Ultradur B4520 is a medium viscosity, rapidly freezing injection molding grade. |