Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 24 g/10 min @Load 2.16 kg, Temperature 230 °C |
24 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products FT2202-732UV Thermoplastic Polyolefin, UV Stabilized, YGYA Black Applications: Box top railTail gate linerExterior trimInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Melt Flow | 24 g/10 min | 24 g/10 min | LAB 012 |
Mytex Polymers AS33K(W)-02 Polypropylene, Talc filled, Compounded Description: Talc filled compounded polypropylene produced for automotive interior applications using Mytex® Technology.Key Applications: General purpose interiorInformation provided by Mytex Polym.. |
|||
Melt Flow | 24 g/10 min @Load 2.16 kg, Temperature 230 °C |
24 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
PolyMirae Moplen HP640R Injection Molding Grade Polypropylene Moplen HP640R is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP640R is a homopolymer particularly suitable for injection molding.. |
|||
Melt Flow | 24 g/10 min @Load 2.16 kg, Temperature 230 °C |
24 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 B |
Mytex Polymers AS319L-01US Thermoplastic Polyolefin, 19% Talc Filled AS319L-01US is a compounded thermoplastic polyolefin (TPO) designed for exterior automotive applications requiring cold temperature impact, processability and paintability. Available in natural or .. |
|||
Melt Flow | 24 g/10 min @Load 5.00 kg, Temperature 260 °C |
24 g/10 min @Load 11.0 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycoloy® C1000HF PC+ABS (Europe-Africa-Middle East) CYCOLOY C1000HF is a general purpose PC+ABS blend specially developed for thin wall applications requiring a high flow with a good balance of properties. It is suitable for applications in the autom.. |
|||
Melt Flow | 24 g/10 min @Load 5.00 kg, Temperature 190 °C |
24 g/10 min @Load 11.0 lb, Temperature 374 °F |
|
Total Finaprene® 602 Styrene-Butadiene TPE Copolymer Compound, Formulated to 61 Shore A
(discontinued **) Styrene-Butadiene CopolymerDescription: Finaprene® 602 is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its broad molecular weight distribution, Finaprene® 60.. |
|||
Melt Flow | 24 g/10 min @Load 2.16 kg, Temperature 190 °C |
24 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
M. Holland Company LD500 LDPE
(discontinued **) Features: High Clarity, High Flow, Narrow Molecular Wt. Dist., Good Processability, Warp ResistantUses: Drink LidsApprovals: FDA 21 CFR 177.1520(c) 2.2 and ASTM D 1248, I, Class A, Cat. 1Processing .. |
|||
Melt Flow | 24 g/10 min @Load 2.16 kg, Temperature 190 °C |
24 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
M. Holland Company LD505 LDPE
(discontinued **) Additives: 0.050 % Slip Features: High Flow, Medium GlossUses: Household Goods, ToysProcessing Method: Injection MoldingInformation provided by M. Holland. |
|||
Melt Flow | 24 g/10 min | 24 g/10 min | Condition I; ASTM D1238 |
Plaskolite Optix® PL-200 Acrylic Resin
(discontinued **) Injection molding grade pellets.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Melt Flow | 24 g/10 min @Load 2.16 kg, Temperature 190 °C |
24 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical LUTENE MB9205 LDPE Injection Molding Grade Description: The physical and structural characteristics of LUTENE MB9205 give it excellent flow properties and good productivity, clarity and surface gloss.Main Application: Lids of all sizes, hous.. |
|||
Melt Flow | 24 g/10 min @Load 2.16 kg, Temperature 230 °C |
24 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
IRPC Polimaxx Polene 3370RM Polypropylene Random Copolymer CHARACTERISTICS: GOOD EXTRUDABILITY, GOOD ADHESIVE, GOOD CLARITY, LOW NECK IN/ODOR HIGH SPEED APPLICATIONS: EXTRUSION COATING FOR COATED OPP FILM |
|||
Melt Flow | 24 g/10 min @Load 5.00 kg, Temperature 200 °C |
24 g/10 min @Load 11.0 lb, Temperature 392 °F |
|
Kraton® D1113 P (SIS) Linear Block Copolymer Description: Kraton D1113 P is a clear, linear block copolymer based on styrene and isoprene with a polystyrene content of 16%. It is supplied from North America in the physical form identified: Kra.. |
|||
Melt Flow | 24 - 28 g/10 min @Load 2.16 kg, Temperature 230 °C |
24 - 28 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Samyang Triel® 5301SP Thermoplastics Polyetherester Elastomer, Double Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5301SP is intended for double extrusion.Information provided by Samyang. |
|||
Melt Flow | 24 g/10 min @Load 6.60 kg, Temperature 337 °C |
24 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM ATX200 PEI+PCE High flow Polyetherimide blend. ECO Conforming, UL94 V0 Listing. |
|||
Melt Flow | 24 g/10 min @Load 2.16 kg, Temperature 230 °C |
24 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
SK Chemicals SKYPEL P137DW Productivity Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Melt Flow | 24 g/10 min @Load 2.16 kg, Temperature 230 °C |
24 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polyram Metal Cap PPC372B73 Polypropylene, 73% Mineral Filled 73% mineral filled, heavy density polypropylene for molding metallized parts and galvanized coversInformation provided by Polyram Ram On Ind. |
|||
Melt Flow | 24 g/10 min @Load 2.16 kg, Temperature 190 °C |
24 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ White LL8350 AP Concentrate Based In LLDPE DescriptionPOLYBATCH® LL8350 AP is an advanced performance white color concentrate containing 50% TiO2 in LLDPE. This product has been specifically engineered to provide improved resistance to phe.. |
|||
Melt Flow | 24 g/10 min @Load 5.00 kg, Temperature 260 °C |
24 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Covestro Bayblend® T50 XF Polycarbonate + ABS Injection molding gradeVicat/B 120 = 115 °Cexcellent flowgood low temperature impact strengthPreprocessingMax. Water content |
|||
Melt Flow | 24 g/10 min @Load 2.16 kg, Temperature 190 °C |
24 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Diamond Polymers NPP10-2523 Low Density Polyethylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 24 g/10 min @Load 2.16 kg, Temperature 230 °C |
24 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Diamond Polymers NPP30-2400 GF20 20% Glass Filled Homopolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 24 g/10 min | 24 g/10 min | ISO 1133 |
Domo 1101S Polypropylene Homopolymer Information provided by Domo. |
|||
Melt Flow | 24 g/10 min @Load 2.16 kg, Temperature 190 °C |
24 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
E-Polymers EFLEX® M400 PP Homopolymer M-series: E-FLEX M series resins are a maleic anhydride grafted (MAH) polymer concentrate designed as synthetic rubber and polyolefin manufactured by E-Polymers. It offers excellent adhesion to nyl.. |
|||
Melt Flow | 24 g/10 min @Load 2.16 kg, Temperature 230 °C |
24 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Carmel Olefins CAPILENE® T 12 EV Polypropylene Homopolymer CAPILENE® T 12 EV is a polypropylene homopolymer with narrow molecular weight distribution, controlled rheology, intended for fiber applications. It is characterized by easy processing, very good m.. |
|||
Melt Flow | 24 g/10 min | 24 g/10 min | Melt Flow Ratio (I10/I2) is 7.3; ASTM D1238 |
Huntsman Rexell® L2101 Injection Molding LLDPE
(discontinued **) Linear-low very low density copolymer, injection molding, FDA compliant.Features: High flow, flexible with excellent environmental stress crack (ESCR), and warpage resistance.Applications: Fitments,.. |
|||
Melt Flow | 24 g/10 min @Load 2.16 kg, Temperature 190 °C |
24 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Radici Heraform® R 3000 Acetal Copolymer Very easy flowing grade for injection molding of thin-walled parts or in case of long flow path.Information provided by Radici group. |
|||
Melt Flow | 24 g/10 min @Load 2.16 kg, Temperature 230 °C |
24 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
ExxonMobil Exxtral™ H1020H Performance Polyolefin Product Description: A specialty thermoplastic olefin resin with good flow, cold temperature impact resistance, low CLTE, medium shrinkage and excellent paintability for automotive exterior applicat.. |
|||
Melt Flow | 24 g/10 min @Load 10.0 kg, Temperature 220 °C |
24 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® NH-1015 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 24 g/10 min @Load 10.0 kg, Temperature 220 °C |
24 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® NH-3208GL PC, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 24 g/10 min @Load 2.16 kg, Temperature 230 °C |
24 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Styron INSPIRE™ TF7000 ES Natural Performance Polymer INSPIRE* TF7000 ES Natural Performance Polymer DA™ is a very high stiffness (2400 MPa) TPO designed for instrument panel upper and lower components, as well as other interior trim applications wher.. |
|||
Melt Flow | 24 g/10 min | 24 g/10 min | ASTM D1238 |
Huntsman PE2053 Injection Molding Polyethylene
(discontinued **) Homopolymer, Drug Master File listed product, and FDA compliant.Features: High flow characteristics, good gloss, and processability.Applications: Injection molding: large moldings including housewar.. |