Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 23.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
23.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
Melt Volume Rate (ml/10 min); ISO 1133 |
Chi Mei Wonderloy® PC-510 PC/ABS Alloy - Flame Retardant High Flow |
|||
Melt Flow | 23.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
23.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
Melt Volume Rate (ml/10 min); ISO 1133 |
Chi Mei Wonderloy® PC-540 PC/ABS Alloy - Flame Retardant High Heat |