Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.4 g/10 min @Load 5.00 kg, Temperature 230 °C |
2.4 g/10 min @Load 11.0 lb, Temperature 446 °F |
|
Polimeri Europa Dutral® PM 8273 Ethylene - Propylene Masterbatch Dutral® PM 8273 is a masterbatch based on Ethylene - Propylene elastomer produced by suspension polymerization using a Ziegler-Natta Catalyst. A non-staining antioxidant is added during the produc.. |
|||
Melt Flow | 2.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers NPS 90-0304 Super High Impact Polystyrene Description: Injection Molding GradeInformation provided by Network Polymers Inc. |
|||
Melt Flow | 2.4 g/10 min @Temperature 190 °C |
2.4 g/10 min @Temperature 374 °F |
|
North Wood Plastics Polypropylene with 40% Wood Fiber, Molding Grade Data provided by North Wood Plastics, Inc. |
|||
Melt Flow | 2.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DSM Yparex® 8403 R Polyolefin Adhesive Resin (European Grade)
(discontinued **) The Yparex range provides outstanding adhesion for all forms of polyethylene including cross-linked PE to: barrier plastics like EVOH and Polyamidemetals like aluminum, steel and copper.Yparex offer.. |
|||
Melt Flow | 2.4 g/10 min @Load 2.16 kg, Temperature 400 °C |
2.4 g/10 min @Load 4.76 lb, Temperature 752 °F |
ASTM D1238 |
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK)
(Unverified Data**) Ketaspire KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and exte.. |
|||
Melt Flow | 2.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers NPS 90-0304 F Super High Impact Polystyrene Description: Injection Molding GradeInformation provided by Network Polymers Inc. |
|||
Melt Flow | 2.4 - 3.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.4 - 3.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
FKuR Kunststoff Terralene® LL 1303 Biobased Polyethylene With the brand name Terralene® FKuR offers biobased polyethylene compounds made using Braskem's Green PE. When compared to conventional polyethylene (PE), the main difference is that the ethanol.. |
|||
Melt Flow | 2.4 - 3.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.4 - 3.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem LB 0316 LLDP IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba.. |
|||
Melt Flow | 2.4 g/10 min @Load 6.60 kg, Temperature 295 °C |
2.4 g/10 min @Load 14.6 lb, Temperature 563 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 9075 PEI High flow Polyetherimide blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Melt Flow | 2.4 g/10 min @Load 6.60 kg, Temperature 295 °C |
2.4 g/10 min @Load 14.6 lb, Temperature 563 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 9075 PEI (Asia Pacific) High flow Polyetherimide blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Melt Flow | 2.4 g/10 min @Load 6.60 kg, Temperature 295 °C |
2.4 g/10 min @Load 14.6 lb, Temperature 563 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM LTX300A PEI Copolymer High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors. |
|||
Melt Flow | 2.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
|
Samsung Cheil Industries Starex® MP-0160RD Metal Plating Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Flow | 2.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D 1238 |
Styrolution PS 5310 HIPS Excellent ESCRGood ToughnessMatte easily decorated finishInformation provided by Styrolution |
|||
Melt Flow | 2.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
|
Samsung Cheil Industries Starex® MP-0160RD Metal Plating Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Flow | 2.4 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.4 g/10 min @Load 8.38 lb, Temperature 446 °F |
ISO 1133 |
Styron Magnumâ„¢ 375 HP Acrylonitrile Butadiene Styrene (ABS) High Heat, Low Gloss ABS.Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Melt Flow | 2.4 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.4 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM Data |
Styron Magnum™ 555 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Melt Flow | 2.4 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.4 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM Data |
Styron Magnum™ 585 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Melt Flow | 2.4 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.4 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM Data |
Styron Pulse® 759 ABS + Polycarbonate, 15% Glass Reinforced PULSE® 759 Engineering resin is a 15% glass reinforced resin designed to provide excellent processability, high heat resistance, and practical toughness. PULSE 759 Engineering resin has been used.. |
|||
Melt Flow | 2.4 g/10 min @Load 6.60 kg, Temperature 295 °C |
2.4 g/10 min @Load 14.6 lb, Temperature 563 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM LTX300A PEI Copolymer (Asia Pacific) High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors. |
|||
Melt Flow | 2.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133H |
Total PSC 1160/1160N Crystal Polystyrene 1160 is a high resistance, high molecular weight crystal polystyrene mainly for the extrusion industry. Most notable for the production of bi-oriented polystyrene (BOPS). It is particularly useful.. |
|||
Melt Flow | 2.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LDPE LD 123.LN Low Density Polyethylene Resin Product Description: LD 123.LN blown film grade offers an excellent balance of optical and strength properties for general purpose clear film applications.Availability: Latin America, North America .. |
|||
Melt Flow | 2.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® 111DP NC010 Acetal (POM)
(Unverified Data**) Nucleated High Viscosity Acetal Homopolymer Delrin 111DP is a new high viscosity acetal homopolymer with enhanced crystallization and excellent creep and fatigue resistance. It has improved thermal .. |
|||
Melt Flow | 2.4 g/10 min | 2.4 g/10 min | Condition E; ASTM D 1238 |
CPT C-Flex® R70-116 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Melt Flow | 2.4 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.4 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
BASF Novolen® 1100 H Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Melt Flow | 2.4 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.4 g/10 min @Load 8.38 lb, Temperature 446 °F |
|
Arkema Group Altuglas® GR 7E LIL Acrylic ALTUGLAS GR 7E LIL is an injection molding grade with excellent balance between mechanical, thermal and optical properties.Key features : easy processing and demolding improved chemical resistance .. |
|||
Melt Flow | 2.4 g/10 min @Load 5.00 kg, Temperature 230 °C |
2.4 g/10 min @Load 11.0 lb, Temperature 446 °F |
|
Arkema Group Kynar® 9000 HDC N 123 PVDF
(discontinued **) Designation ISO 12086-PVDF-E,GG1,Q.5E5.J.A.I.D, CF,Kynar PVDF are fluorinated thermoplastic homopolymers.Outstanding characteristics of Kynar: chemical resistance, imperviousness to UV, high barrier.. |
|||
Melt Flow | 2.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238G |
Total Lacqrene® 1160(AS) Crystal Polystyrene
(discontinued **) LACQRENE® 1160 is a high resistance, high molecular weight crystal polystyrene mainly for the extrusion industry. It is particularly useful in the production of thick sheet by direct gassing, wher.. |
|||
Melt Flow | 2.4 g/10 min @Load 5.00 kg, Temperature 190 °C |
2.4 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Polyplastic Armlen® PE MF 70-2FR Magnesium Hydroxide Filled Polyethylene 70% Magnesium HydroxideFor extrusion of fire resistant aluminum composite panels.Information provided by PolyPlastic Group. |
|||
Melt Flow | 2.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® FG150 NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has low die deposit and low porosity. It has been developed for consideration in applications and parts for th.. |
|||
Melt Flow | 2.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DSM Yparex® 8403 RS Polyolefin Adhesive Resin (European Grade)
(discontinued **) The Yparex range provides outstanding adhesion for all forms of polyethylene including cross-linked PE to: barrier plastics like EVOH and Polyamidemetals like aluminum, steel and copper.Yparex offer.. |