Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.3 g/10 min | 2.3 g/10 min | Condition 230/2-8; ASTM D1238 |
Plaskolite Optix® CA-81 General Purpose Acrylic Resin Extrusion Grade Pellets. Highest Molecular weight. |
|||
Melt Flow | 2.3 g/10 min | 2.3 g/10 min | Condition 230/2-8; ASTM D1238 |
Plaskolite West Optix® CA-81 General Purpose Acrylic Resin Extrusion Grade Pellets. Highest Molecular weight. |
|||
Melt Flow | 2.3 g/10 min @Temperature 190 °C |
2.3 g/10 min @Temperature 374 °F |
|
North Wood Plastics HDPE with 40% Wood Fiber Data provided by North Wood Plastics, Inc. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® LA-0219-A LDPE Foam Resin Features: Good heat sealing latitudeModerate toughnessEasy processability Applications: Industrial packagingLinersBlends with LLDPEFoam ArticlesInformation provided by Nova Chemicals |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® LA-0224-A LDPE Foam Resin Excellent stiffness, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinFilm properties are typical of blown film.. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® LF-0219-A LDPE Blow Molding Resin Good heat sealing latitude, Easy processabilityApplications: Food contact, Squeeze bottles, Non-ESCRAdditives: Base resinInformation provided by NOVA Chemicals. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® LF-0219-D LDPE Film Resin Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Liners, industrial packaging, blends with LLDPE.Data provided by the manufacturer. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Yparex 8102 Polyolefin Adhesive Resin The Yparex range provides outstanding adhesion for all forms of polyethylene including cross-linked PE to: barrier plastics like EVOH and Polyamidemetals like aluminum, steel and copper.Yparex offer.. |
|||
Melt Flow | 2.3 g/10 min | 2.3 g/10 min | ExxonMobil Method |
ExxonMobil LD 503.LN Foams and Compounding Resin
(discontinued **) LD 503.LN is a low density homopolymer specially designed for maximum performance in foam applications.Information provided by ExxonMobil Chemical |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
M. Holland Company LD219 LDPE
(discontinued **) Features: Good Processability, Good ToughnessUses: Bottles, Industrial Applications, PackagingProcessing Method: Blow MoldingInformation provided by M. Holland. |
|||
Melt Flow | 2.3 g/10 min | 2.3 g/10 min | Exxon Method |
ExxonMobil Escorene® LD-760 High EVA Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 27.5% vinyl acetate copolymer designed for specialty compounding applications. Excellent filler acceptance produces highly loaded concentrates.Ap.. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Phillips 66 COPYLENE® CH023NX Polypropylene, Homopolymer, Thermoforming COPYLENE™ CH023NX has a high performance nucleation system designed to yield high clarity thermoformed articlesApplications: ThermoformingInformation provided by Phillips 66. |
|||
Melt Flow | 2.3 g/10 min | 2.3 g/10 min | ASTM D1238 |
Kolon DIAMAT® GP Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) LL0220KJ Linear Low Density Polyethylene LL0220KJ are linear low density polyethylene copolymers containing butane-1 as the comonomer.Applications: shipping sacks, carrier and garbage bags, consumer packaging, high clarity film, agricultu.. |
|||
Melt Flow | 2.3 g/10 min | 2.3 g/10 min | ASTM D1238 |
Lucky IH-830 Acrylic, Injection Grade Similar to grade EH-910, but with higher flow for injection molding. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent.. |
|||
Melt Flow | 2.3 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.3 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
LG Chemical 25SPR GPPS Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, Superior extrusion.. |
|||
Melt Flow | 2.3 g/10 min @Load 6.60 kg, Temperature 337 °C |
2.3 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM CRS5201 PEI (Asia Pacific) 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Melt Flow | 2.3 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.3 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® MP-0670 ABS, Metal Plating Grade Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 2.3 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.3 g/10 min @Load 11.0 lb, Temperature 392 °F |
|
Samsung Cheil Industries Starex® SD-0150GP High Impact Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Flow | 2.3 g/10 min @Load 5.00 kg, Temperature 190 °C |
2.3 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133/ASTM D1238 |
Silon Taborex TA 1108 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1108 HD is a crosslinkable compound according to the “SIOPLAS-SYSTEMâ€; made by a Silane grafted ethylene copolymer known as the graft and a Masterbatch containing the crosslinki.. |
|||
Melt Flow | 2.3 g/10 min @Load 2.20 kg |
2.3 g/10 min @Load 4.86 lb |
ASTM D1238 |
Sumitomo Chemical ESPOLEX® WT525 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Melt Flow | 2.3 g/10 min @Temperature 230 °C |
2.3 g/10 min @Temperature 446 °F |
I<sub>2</sub>; ASTM D1238 |
Formosa Plastics Formolene® 3302B Random Copolymer Polypropylene Random Copolymer for Extrusion and Thermoforming Applications Formolene® 3302B is a low melt flow random with excellent clarity, fast cycle time and easy mold release, designed for extrusion proces.. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LD 129.24 Cast Overwrap Film Resin Product Description: LD 129.24 is a medium density homopolymer film resin with good clarity and excellent stiffness. Film made from LD 129.24 can be used in overwrap applications and in push-through.. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LDPE LD 129.24 Low Density Polyethylene Resin Product Description: LD 129.24 is a medium density homopolymer film resin with good clarity and excellent stiffness. Film made from LD 129.24 can be used in overwrap applications and in push-through.. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LDPE LD 503.LP Low Density Polyethylene Resin Product Description: LD 503.LP is a LDPE homopolymer that is suitable for use in molding, extrusion, compounding and foam applications.Availability: Latin America, North America and South AmericaAdd.. |
|||
Melt Flow | 2.3 g/10 min | 2.3 g/10 min | ASTM D1238 |
Dow DOWLEX™ 2047G Linear Low Density Polyethylene For high performance stretch film applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Braskem Green PE SLH218 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene Description: SLH218 is a LLDPE Hexene copolymer produced by Braskem. It shows a good balance between optical properties, mechanical properties (Mainly stretchability), sealability and processability.. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Braskem LL 218 LLDPE Cast Film Extrusion Polyethylene Description: LL218 is a Linear Low Density Polyethylene, copolymer of butene-1, produced by Spherilene process. Developed for cast film extrusion. Films obtained with this product show a good proces.. |
|||
Melt Flow | 2.3 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.3 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Americas Styrenics STYRON® 404 High Impact Polystyrene Product CharacteristicsAdditive FreeTypical ApplicationsCompounding and masterbatchesInformation provided by AmericasStyrenics LLC. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Total LDPE 1022 FN 24 Low Density Polyethylene - Blown Film LDPE 1022 FN 24 is a low density polyethylene made by a high pressure process without antioxidant.LDPE 1022 FN 24 is suited to many applications in the field of consumer, industrial, food or hygiene.. |