Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.1 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.1 g/10 min @Load 4.76 lb, Temperature 374 °F |
Procedure A; ASTM D1238 |
PolyOne Maxxam™ SY 89-21-1 Polypropylene, Unspecified (PP, Unspecified) Maxxam ™ SY 89-21-1 is a polypropylene copolymer compound with a pre-dispersed blowing agent for up to 50% expansion. The compound offers consistent cell structure, dielectric properties, and stren.. |
|||
Melt Flow | 2.1 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.1 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Riblene® FL 34 Low Density Polyethylene - Blown Film Extrusion Riblene FL 34 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FL 34 is characterized by a good balance between processabilit.. |
|||
Melt Flow | 2.1 g/10 min @Load 1.00 kg, Temperature 235 °C |
2.1 g/10 min @Load 2.20 lb, Temperature 455 °F |
Procedure A Condition Q; ASTM D1238 |
Network Polymers Softflex® 0826 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Melt Flow | 2.1 g/10 min | 2.1 g/10 min | ISO 1133 |
Total Lacqtene® FD 0270 LDPE, blown film, compounding, injection molding
(discontinued **) Low density radical polyethylene made by high pressure process. Temperature profile (°C) for injection molding: 200 to 260Information provided provided by Total Petrochemicals.Total Petrochemicals .. |
|||
Melt Flow | 2.1 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.1 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® LA-0218-AF LDPE Foam Resin
(discontinued **) Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Specifically designed for foam process, Blends with LLDPEAdditives: Base resinFilm properties are typical of blown fi.. |
|||
Melt Flow | 2.1 g/10 min | 2.1 g/10 min | Exxon Method |
ExxonMobil Escorene® LD-725 High EVA Film and Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An 18% vinyl acetate copolymer designed for specialty film and compounding applications. Outstanding sealability and low modulus are key attributes.. |
|||
Melt Flow | 2.1 g/10 min | 2.1 g/10 min | Exxon Method |
ExxonMobil Escorene® LD-612 EVA Injection Molding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.8% vinyl acetate copolymer resin designed for molding and extrusion applications requiring low temperatures, flexibility and toughness. This re.. |
|||
Melt Flow | 2.1 g/10 min | 2.1 g/10 min | ASTM D1238G |
Hannam Chemical Hanalac 740 ABS, Super High Impact Grade Superior impact strength, even at low temperature. Applications: helmets, shoe heels, bobbins, roller skates, bags, pipes, radiator grills, auto parts, appliance wheels. |
|||
Melt Flow | 2.1 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.1 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex ELEXAR® EL 8623 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Melt Flow | 2.1 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.1 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Styron MAGNUMâ„¢ 375 HH Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection moldingApplications: Automotive interior trim applications requiring low volatile organic compounds (VOC)Information provided by.. |
|||
Melt Flow | 2.1 g/10 min @Load 5.00 kg, Temperature 280 °C |
2.1 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
Melt Flow | 2.1 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.1 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Daploy™ WB130HMS High Melt Strength Polypropylene for Foam Extrusion Daploy WB130HMS resin is a propylene-based, structurally isomeric polymer, which combines significantly increased melt strength with largely drawability of the polymer melt. Thus, the material is g.. |
|||
Melt Flow | 2.1 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.1 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Daploy™ WB140HMS Polypropylene Daploy™ WB140HMS is a structurally isomeric modified propylene homopolymer. Applications: door liners, parcel shelves, microwaveable food packaging, cushioning and protective packaging, lightweigh.. |
|||
Melt Flow | 2.1 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.1 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Borealis FA6220 Low Density Polyethylene FA6220 is a Low Density Polyethylene for Film Extrusion. Includes Antioxidant. This grade is developed for the production of thin blown films. Applications: shrink film, pouches, general packagin.. |
|||
Melt Flow | 2.1 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.1 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Appeel® LSR11D542 Lidding Sealant Resin Appeel® LSR11D542 is a modified ethylene vinyl acetate copolymer resin designed to function as a peelable sealing layer for lidding and pouch applications. It provides a peelable seal and a "whiten.. |
|||
Melt Flow | 2.1 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.1 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Bynel® 30E671 Adhesive Resin Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melt Flow | 2.1 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.1 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Westlake EMAC® SP2255 17% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2255 is a 17% EMA copolymer containing slip and antiblock. This resin is designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat s.. |
|||
Melt Flow | 2.1 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.1 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Westlake EMAC® SP2260 24% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2260 is a 24% EMA copolymer designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperatures are required. SP2260 provide.. |
|||
Melt Flow | 2.1 g/10 min | 2.1 g/10 min | Condition E; ASTM D 1238 |
CPT C-Flex® R70-082 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Melt Flow | 2.1 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.1 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont™ Bynel® 30E753 Anhydride Modified Ethylene Vinyl Acetate BYNEL® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melt Flow | 2.1 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.1 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LD 124.MS General Purpose Clarity Film Resin Product Description: LD 124.MS blown film resin offers an excellent balance of optical and strength properties for general purpose clear film applications. Availability: Latin America, North America.. |
|||
Melt Flow | 2.1 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.1 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LD 143.26 High Clarity Packaging Film Resin Product Description: LD 143.26 is a homopolymer packaging film resin with excellent clarity and good stiffness. It is suitable for processing in either blown or cast film equipment. In blown film eq.. |
|||
Melt Flow | 2.1 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.1 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® 100ST BK602 Acetal (POM)
(Unverified Data**) Super Toughened High Viscosity Acetal Homopolymer Delrin 100ST BK602 is a super tough high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed part.. |
|||
Melt Flow | 2.1 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.1 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers ABS TR-5000 Transparent Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 2.1 g/10 min @Load 2.16 kg, Temperature 235 °C |
2.1 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® AESN G9 T6L Nylon 12, Graphite Filled (Dry) Designation ISO 1874-PA12,EHLS,22-010,CD10Rigid grade with graphite fillers for extrusion. Available color: steel gray. Reinforced light and heat stabilizing agents.Very low friction coefficient. No.. |
|||
Melt Flow | 2.1 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.1 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238L |
Braskem H 605 Thermoforming Polypropylene Applications: Flat and corrugated sheets with high transparency; thermoformed packing with high transparency. Information provided by Braskem |
|||
Melt Flow | 2.1 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.1 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem LL4800N PEBDL Cast Film Extrusion Polyethylene Copolymer LL4800N is a linear low-density polyethylene, copolymer of octene-1, produced by the solution process. It was developed for cast film extrusion. Films obtained with this product show a good processi.. |
|||
Melt Flow | 2.1 g/10 min | 2.1 g/10 min | Exxon Method |
ExxonMobil Escorene® UL-7560 EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An 18% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |
|||
Melt Flow | 2.1 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.1 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238L |
Braskem H 606 Thermoforming Polypropylene Description: H 606 is low melt flow rate homopolymer with general purpose additive package. This resin is designed for extrusion and thermoforming. H 606 presents excellent processability and high o.. |