Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 19.7 g/10 min | 19.7 g/10 min | Condition G |
Ineos Nova 3930 General Purpose Crystal Polystyrene
(discontinued **) High melt flow, Crystal clearApplications: Razor components, Personal care, Thin wall moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical and .. |
|||
Melt Flow | 19.7 g/10 min @Load 6.60 kg, Temperature 337 °C |
19.7 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM SF2250 PEI Blend (Asia Pacific) High flow Ultem for thin wall application |
|||
Melt Flow | 19.7 g/10 min @Load 6.60 kg, Temperature 337 °C |
19.7 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM SF2250 PEI Blend High flow Ultem for thin wall application |