Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 16 g/10 min @Load 2.16 kg, Temperature 230 °C |
16 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products HP521-186 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 7701 Graphite Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Melt Flow | 16 g/10 min @Load 5.00 kg, Temperature 260 °C |
16 g/10 min @Load 11.0 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycoloy® C2100 PC+ABS (Europe-Africa-Middle East) CYCOLOY C2100 is a flame retardant blend, specifically developed to meet the stringent requirements of mains current carrying applications. CYCOLOY C2100 combinesThis data was supplied by SABIC-IP f.. |
|||
Melt Flow | 16 g/10 min @Load 2.16 kg, Temperature 260 °C |
16 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS Non-chlorinated and non-brominated flame retardant PC+ABS offering balanced flow and impact properties for various applications. |
|||
Melt Flow | 16 g/10 min @Load 2.16 kg, Temperature 210 °C |
16 g/10 min @Load 4.76 lb, Temperature 410 °F |
|
Noltex Soarnol® H4815 Ethylene Vinyl Alcohol Copolymer Special designed the highest ethylene content grade. Ethylene content 48 mol%.Information provided by Soarus, LLC. In the United States SOARNOL is produced by Noltex, L.L.C., an affiliate of Nippo.. |
|||
Melt Flow | 16 g/10 min @Load 5.00 kg, Temperature 260 °C |
16 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® CP8930 PC+ABS (Asia Pacific) High heat, PC/ABS for automotive electro plating applications, excellent balance in flow/impact |
|||
Melt Flow | 16 g/10 min @Temperature 275 °C |
16 g/10 min @Temperature 527 °F |
DSC |
Kolon NOPLA® KE531 PEN-PET Copolyester NOPLA® is an advanced PEN-PET copolyester which can be used for bottle, sheet & injection molding applicationsUV protection & prolonged outdoor durability, enhanced gas barrier, outstanding impac.. |
|||
Melt Flow | 16 g/10 min @Load 10.0 kg, Temperature 220 °C |
16 g/10 min @Load 22.0 lb, Temperature 428 °F |
Estimated using room temperature density |
Ineos ABS Lustran® H607AS Contains antistatic additives,Property data per ISO test methods. |
|||
Melt Flow | 16 g/10 min @Load 2.16 kg, Temperature 230 °C |
16 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Multibase Multi-Flex® A 6221 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Thermal Stability, GoodOzone ResistantGeneral PurposeForms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsAutomotive Under the HoodInfo.. |
|||
Melt Flow | 16 g/10 min @Load 10.0 kg, Temperature 250 °C |
16 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL WCA875 PPE-TPE (Europe-Africa-Middle East) Non-halogenated flame retardant Flexible Noryl extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Excellent flame retardant performance with balanced t.. |
|||
Melt Flow | 16 g/10 min @Load 6.60 kg, Temperature 337 °C |
16 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 1110 PEI Enhanced flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
Melt Flow | 16 g/10 min @Load 10.0 kg, Temperature 250 °C |
16 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® SR-7300 ABS/PET, Unreinforced Material with superior chemical resistance that can be used in the interior/exterior material of household appliances that require heat resistanceInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 16 g/10 min @Load 10.0 kg, Temperature 220 °C |
16 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® TX-0510 TRABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 16 g/10 min @Load 10.0 kg, Temperature 220 °C |
16 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® TX-0510 TRABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 16 g/10 min @Load 2.16 kg, Temperature 235 °C |
16 g/10 min @Load 4.76 lb, Temperature 455 °F |
ASTM D1238 |
Samyang Tribit® 1503 Polybutylene Terephthalate Characteristics:High flow & processabilityApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll information provid.. |
|||
Melt Flow | 16 g/10 min @Load 5.00 kg, Temperature 260 °C |
16 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS (Asia Pacific) PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed. |
|||
Melt Flow | 16 - 24 g/10 min @Load 2.16 kg, Temperature 230 °C |
16 - 24 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 1498-01 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1498-01 is a high flow, medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. Schulman... |
|||
Melt Flow | 16 g/10 min @Load 2.16 kg, Temperature 190 °C |
16 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Red 5670 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 5670 is a red color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® 56.. |
|||
Melt Flow | 16 - 24 g/10 min @Load 2.16 kg, Temperature 230 °C |
16 - 24 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 1498-01 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1498-01 is a high flow, medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. Schulman... |
|||
Melt Flow | 16 g/10 min | 16 g/10 min | |
Zylog Hipolyene® 6251 Y M2 Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Melt Flow | 16 g/10 min @Load 2.16 kg, Temperature 190 °C |
16 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
ELASTO UK Dryflex® 8010-102 Flame Retardant TPE for Extrusion, Pebble Gray Vitaprene® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Vitaprene® compounds permit sophisticated component design and.. |
|||
Melt Flow | 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
16 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Diamond Polymers PC-1500F Clear, Natural Polycarbonate Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 16 g/10 min @Load 10.0 kg, Temperature 240 °C |
16 g/10 min @Load 22.0 lb, Temperature 464 °F |
ISO 1133 |
Cossa Polimeri ESTABLEND PA 1616 GF ABS / Nylon 6 Blend, 8% Glass Filled ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.8% glass fiber reinforcedHigh impact strength, high chemical resistance, excellent heat resistance, good dimensional stabil.. |
|||
Melt Flow | 16 g/10 min | 16 g/10 min | ASTM D1238 |
Aclo Accutech Polypropylene Copolymer CP0437T30L1 Talc Reinforced |
|||
Melt Flow | 16 g/10 min @Load 10.0 kg, Temperature 220 °C |
16 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D-1238 |
Bhansali Engineering Abstron IMGS20 Glass Reinforced Grade Glass Reinforced ABS & SAN Resins for product specific requirement of very high rigidity and temperatureInformation provided by Bhansali |
|||
Melt Flow | 16 - 20 g/10 min | 16 - 20 g/10 min | 230/2.16; May be specified; ASTM D1238 |
Plastics Group Polifil® RMT-20V 20% Talc-Reinforced Polypropylene, High Impact, UV Stabilized Polifil® RMT-V series compounds are high impact, UV stabilized polypropylenes reinforced with asbestos-free talc. In addition to high impact strength, they possess a high flex modulus and the abili.. |
|||
Melt Flow | 16 - 24 g/10 min @Temperature 230 °C |
16 - 24 g/10 min @Temperature 446 °F |
Condition L; ASTM D1238 |
A. Schulman POLYFORT™ PP 1498HU UV Stabilized, Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1498HU is a high flow UV stabilized medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. .. |